Reactive Phases in Alkali Carbonate Reaction Reference Aggregate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reactive Phases in Alkali Carbonate Reaction Reference Aggregate

Author(s): Mengesha Beyene, Jose Munoz, Richard Meininger, and Anant Shastry

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 281-292

Keywords: acid-insoluble residues (AIR); alkali-carbonate reaction (ACR); alkali-silica reaction (ASR); ASR gel; cryptocrystalline quartz; dolomitic limestone; microcrystalline quartz; scanning electron microscopyenergy- dispersive spectroscopy; quantitative image

DOI: 10.14359/51726997

Date: 11/1/2020

Abstract:
The reference Pittsburg Ontario alkali carbonate-reactive (ACR) aggregate source was characterized using a holistic approach to identify and quantify mineral phases, particularly reactive forms of silica and expansive types of clays in the aggregate which may have a role in the controversial ACR mechanism and resulting expansion and cracking of concrete. This research was performed using state-of-the-art analytical techniques and methods that included polarized light microscopy (PLM), quantitative image analysis (QIA) of backscattered electron (BSE) scanning electron microscope (SEM) images, acid-insoluble residue (AIR) tests, X-ray diffraction (XRD), X-ray fluorescence (XRF), and a chemical ratio method of identifying alkali-reactive carbonate rocks. Three types of silica phases were identified through PLM examination: upper silt-sized quartz grains both in the virgin aggregate and acid insoluble residue (AIR); cryptocrystalline silica dispersed and hidden in the fine-grained rock matrix and identified only in the AIR; and cryptocrystalline-to-microcrystalline silica occupying interstitial spaces of dolomitic limestone particles which lacked clay in their matrix. PLM findings were confirmed through QIA of the AIR. Particle size distribution of silica phases through QIA showed that silica phases in sizes of 0.5 to 2 μm (0.00002 to 0.00008 in.) occur in high abundance. QIA of AIR identified illite as the major clay mineral in the aggregate. While this clay type is not known to be expansive, microcrystalline to cryptocrystalline silica phases are potentially alkali-silica reactive (ASR) in concrete as opposed to ACR.

Related References:

1. Tang, M., and Deng, M., “Progress on the Studies of Alkali-Carbonate Reaction. In: Proceedings 12th International Conference on Alkali-Aggregate Reaction in Concrete,” Beijing, China, 2004, pp. 51-59.

2. Hadley, D. W., 1964, “Alkali Reactivity of Dolomitic Carbonate Rocks,” Symposium on Alkali-Carbonate Rock Reaction, Highway Research, Record No. 45, pp. 1-19.

3. Ozol, M. A., “Alkali Carbonate Rock Reaction,” Significance of Tests and Properties of Concrete and Concrete-Making Materials, ASTM STP 169C, West Conshohocken, Pennsylvania, 1994, pp. 372-387.

4. Swenson, E. G., “A Reactive Aggregate Undetected by ASTM Test,” ASTM Bulletin, American Society for Testing and Materials, No. 226, 1957, pp. 48-51.

5. Tang, M. S.; Liu, Z.; and Han, S. F., “Mechanism of Alkali-Carbonate Reaction,” Proceedings of the 7th International Conference on Alkali-Aggregate Reaction in Concrete, Ottawa, ON, Canada, 1986, pp. 275-279.

6. Gillott, J. E., “Mechanism and Kinetics of Expansion in the Alkali-Carbonate Rock Reaction,” Canadian Journal of Earth Sciences, V. 1, No. 2, 10 1964, pp. 121-145. doi: 10.1139/e64-007

7. Swenson, E. G., and Gillott, J. E., “Alkali-Carbonate Rock Reaction,” Highway Research Record, V. 45, 1964, pp. 21-40.

8. Gillott, J. E., and Swenson, E. G., “Mechanism of Alkali-Carbonate Rock Reaction,” Quarterly Journal of Engineering Geology, V. 2, No. 1, 1969, pp. 7-23. doi: 10.1144/GSL.QJEG.1969.002.01.02

9. Tang, M., and Lu Y., “Rapid Method for Determining the Alkali-Reactivity of Carbonate Rock,” Concrete Alkali-Aggregate Reactions, Noyes Publications, Park Ridge, NJ, 1986, pp. 286-287.

10. Tong, L., “Alkali-Carbonate Rock Reaction” thesis, Nanjing Institute of Chemica Technology, Nanjing China, 1994, 219 pp.

11. Tang, M., and Deng, M., “Progress on the Studies of Alkali-Carbonate Reaction” Proc. 12th Int. Conf. AAR, Beijing, China, 2008, pp 51-59.

12. López-Buendía, A. M.; Climent, V.; Urquiola, M. M.; and Bastida, J., Influence of Dolomite Stability on Alkali–carbonate Reaction. In: Broekma ns, M.A.T.M. & Wigum, B.J. (eds) Proceedings 13th International Alkali–Aggregate Reactions Conference, Trondheim, Norway, 2008.

13. Katayama, T., “How to Identify Carbonate Rock Reactions in Concrete,” Materials Characterization, V. 53, No. 2-4, 2004, pp. 85-104. doi: 10.1016/j.matchar.2004.07.002

14. Katayama, T., “Modern Petrography of Carbonate Aggregates in Concrete-Diagnosis of So-Called Alkali-carbonate Reaction and Alkali-Silica Reaction, 8th CANMET/ACI International Conference on Recent Advances in Concrete Technology, SP-235, American Concrete Institute, Farmington Hills, MI, 2006, pp. 423-444.

15. Katayama, T., and Sommer, H., “Further Investigation of the Mechanisms of So-Called Alkali-Carbonate Reaction based on Modern Petrographic Techniques,” In M.A.T.M, 2008.

16. Katayama, T., “The So-Called Alkali-Carbonate Reaction (ACR)—its Mineralogical and Geochemical Details, with Special Reference to ASR,” Cement and Concrete Research, V. 40, No. 4, 2010, pp. 643-675. doi: 10.1016/j.cemconres.2009.09.020

17. Grattan-Bellew, P. E.; Mitchell, L. D.; Margeson, J.; and Deng, M., “Is Alkali-Carbonate Reaction just a Variant of Alkali-Silica Reaction, ACR=ASR?,” Cement and Concrete Research, V. 40, No. 4, 2009, pp. 556-562. doi: 10.1016/j.cemconres.2009.09.002

18. Fecteau, P.; Fournier, B.; Choquette, M.; and Duchesne, J., “Contribution of the Understanding of the So-Called Alkali-Carbonate Reaction,” 14th International Conference on Alkali-Aggregate Reaction, Austin, TX, 2012.

19. Dubberke, and W., Marks, V., “The Relationship of Ferroan Dolomite Aggregate to Rapid Concrete Deterioration,” Iowa Department of Transportation, Ames, IA, 1987, 31 pp.

20. Rogers, C. A.; Grattan-Bellew, P. E.; Hooton, R. D.; Ryell, J.; and Thomas, M. D. A., “Alkali-Aggregate Reactions in Ontario,” Canadian Journal of Civil Engineering, V. 27, No. 2, 2000, pp. 246-260. doi: 10.1139/l99-073

21. Hadley, D. W., “Alkali Reactivity of Carbonate Rocks - Expansion and Dedolomitization,” Proceedings of the Annual Meeting - Highway Research Board, V. 40, 1961, pp. 462-474.

22. Sherwood, W. C., and Newlon, H. H Jr., “Studies on the Mechanisms of Alkali-Carbonate Reaction: Part-Chemical Reactions,” Highway Research Record, 1964, p. 45.

23. Mather, K.; Buck, A. D.; and Luke, W. I., “Alkali-Silica and Alkali-Carbonate Reactivity of Some Aggregates from South Dakota, Kansas, and Missouri,” Symposium on Alkali- Carbonate Rock Reactions, Highway Research Board, No. 45, 1964, pp. 72-109.

24. Melanesi, C. A.; Marfil, S. A.; Batic, O. R.; and Maiza, P. J., “The Alkali-Carbonate Reaction and Its Reaction Products – An Example with Argentinean Dolomite Rocks,” Cement and Concrete Research, V. 26, No. 10, 1996, pp. 1579-1591. doi: 10.1016/0008-8846(96)00140-8

25. Axon, E. O., and Lind, J., “Alkali-Reactive Carbonate Rocks in Indiana – An Academic or a Practical Problem.” HRB Bulletin No. 45, 1964, pp. 114-125.

26. Beyene, M. A.; Snyder, A.; Lee, R. J.; and Blaszkiewicz, M., “Alkali-Silica Reaction (ASR) as a Root Cause of Distress in a Concrete Made from Alkali Carbonate Reaction (ACR) Potentially Susceptible Aggregates,” Cement and Concrete Research, V. 51, 2013, pp. 85-95. doi: 10.1016/j.cemconres.2013.04.014

27. Pansu, M., and Gautheyrou, J., Handbook of Soil Analysis: Mineralogical, Organic and Inorganic Methods, 2007, Springer Science & Business Media, Berlin, Germany

28. Poppe, L. J.; Paskevich, V. F.; Hathaway, J. C.; and Blackwood, D. S., “A Laboratory Manual for X-Ray Powder Diffraction,” U.S. Geological Survey Open-File Report, V. 1, No. 041, 2001, pp. 1-88.

29. Stutzman, P.; Feng, P.; and Bullard, J. W., “Phase Analysis of Portland Cement by Combined Quantitative X-Ray Powder Diffraction and Scanning Electron Microscopy,” Journal of Research, V. 121, 2016, pp. 47-107. doi: (NIST JRES)10.6028/jres.121.004

30. Chancey, R. T.; Stutzman, P.; Juenger, M. C.; and Fowler, D. W., “Comprehensive Phase Characterization of Crystalline and Amorphous Phases of a Class F Fly Ash,” Cement and Concrete Research, V. 40, No. 1, 2010, pp. 146-156. doi: 10.1016/j.cemconres.2009.08.029

31. Biehl, L., and Landgrebe, D., “MultiSpec—A Tool for Multispectral–hyperspectral Image Data Analysis,” Computers & Geosciences, V. 28, No. 10, 2002, pp. 1153-1159. doi: 10.1016/S0098-3004(02)00033-X

32. Stutzman, P., Lespinasse, G., and Leigh, S. (2008), Compositional Analysis and Certification of NIST Reference Material Clinker 2686a. NIST Technical Note, 1602.

33. Snyder, K. A., and Stutzman, P. E., “Hydrated Phases in Blended Cement Systems and Synthetic Saltstone Grouts,” 2013, National Institute of Standards and Technology, Gaithersburg, MD

34. Bullard, J. W., “An Application for Quantitative Analysis of Cement and Clinker Microstructure Images,” National Institute of Standards and Technology, (2015), Technology Note 1876, U.S. Department of Commerce.

35. Katayama, T.; Jensen, V.; and Rogers, C. A., The Enigma of the ‘So-called’ Alkali–Carbonate Reaction, Proceedings of the Institution of Civil Engineers—Construction Materials, V. 169, No. 4, 2016, pp. 223–232.

36. Sims, I., “Editorial,” Construction Materials, V. 169, 2016, pp. 179-181. doi: 10.1680/jcoma.2016.169.4.179

37. Beyene, M., and Meininger, R. C., “Alkali Reactive Carbonate Rocks: Is it Alkali Silica Reaction (ASR) or Alkali Carbonate Reaction (ACR)?” Sixth International Conference on Durability of Concrete Structures, Paper Number ICC26, July 18-20, University of Leeds, Leeds, UK.


ALSO AVAILABLE IN:

Electronic Materials Journal