Title: Study on Permeability of Cracked Concrete

Author(s): Antonio Princigallo

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 151-164

Keywords: cracks; durability; mechanical properties; permeability; self-healing

DOI: 10.14359/51725997

Date: 11/1/2020

Abstract:
The present study concerns a testing methodology to investigate the permeability of cracked concrete based on oxygen permeability testing. The methodology was applied to study self-healing; thus, concrete specimens were preliminarily subjected to mechanical compression and successively exposed to water. The aim was to assess any change in the conditions of the oxygen flow respect to the corresponding plain specimens. Different concrete types were used—that is, ordinary concrete and high-performance concrete. It was found that both the oxygen permeability as well as the type of oxygen flow were affected by the presence of cracks even partially filled in with hydration products. In particular, the intrinsic permeability was determined. In addition, it was possible to assess the relative proportions of viscous and inertial flows. On those bases, the critical velocity was identified as a parameter to permit a consistent comparison between different specimens under similar flow types.

Related References:

1. Lv, Z., and Chen, D., “Overview of Recent Work on Self-Healing in Cementitious Materials,” Materiales de Construcción, V. 64, No. 316, 2014, p. e034. doi: 10.3989/mc.2014.05313

2. Muhammad, N. Z.; Shafaghat, A.; Keyvanfar, A.; Abd. Majid, M. Z.; Ghoshal, S. K.; Mohammadyan Yasouj, S. E.; Ganiyu, A. A.; Kouchaksaraei, M. S.; Kamyab, H.; Taheri, M. M.; Shirdar, M. R.; and McCaffer, R., “Tests and Methods of Evaluating the Self-Healing Efficiency of Concrete: A Review,” Construction and Building Materials, V. 112, 2016, pp. 1123-1132. doi: 10.1016/j.conbuildmat.2016.03.017

3. Wu, M.; Johannesson, B.; and Geiker, M., “A Review: Self-Healing in Cementitious Materials and Engineered Cementitious Composite as a Self-Healing Material,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 571-583. doi: 10.1016/j.conbuildmat.2011.08.086

4. Huang, H.; Ye, G.; and Damidot, D., “Effect of Blast Furnace Slag on Self-Healing of Microcracks in Cementitious Materials,” Cement and Concrete Research, V. 60, 2014, pp. 68-82. doi: 10.1016/j.cemconres.2014.03.010

5. Yang, Y.; Yang, E.-H.; and Li, V. C., “Autogenous Healing of Engineered Cementitious Composites at Early Age,” Cement and Concrete Research, V. 41, No. 2, 2011, pp. 176-183. doi: 10.1016/j.cemconres.2010.11.002

6. Hilloulin, B.; Hilloulin, D.; Grondin, F.; Loukili, A.; and De Belie, N., “Mechanical Regains due to Self-Healing in Cementitious Materials: Experimental Measurements and Micro-Mechanical Model,” Cement and Concrete Research, V. 80, 2016, pp. 21-32. doi: 10.1016/j.cemconres.2015.11.005

7. Sisomphon, K.; Copuroglu, O.; and Koenders, E. A. B., “Effect of Exposure Conditions on Self Healing Behavior of Strain Hardening Cementitious Composites Incorporating Various Cementitious Materials,” Construction and Building Materials, V. 42, 2013, pp. 217-224. doi: 10.1016/j.conbuildmat.2013.01.012

8. Aldea, C.-M.; Song, W.-J.; Popovics, J. S.; and Shah, S. P., “Extent of Healing of Cracked Normal Strength Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 12, No. 1, 2000, pp. 92-96. doi: 10.1061/(ASCE)0899-1561(2000)12:1(92)

9. Zhu, Y.; Zhang, Z. C.; Yao, Y.; Guan, X. M.; and Yang, Y. Z., “Analysis of Crack Microstructure, Self-Healing Products, and Degree of Self-Healing in Engineered Cementitious Composites,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 6, 2016, p. 04016017. doi: 10.1061/(ASCE)MT.1943-5533.0001533

10. Wiktor, V., and Jonkers, H. M., “Quantification of Crack-Healing in Novel Bacteria-Based Self-Healing Concrete,” Cement and Concrete Composites, V. 33, No. 7, 2011, pp. 763-770. doi: 10.1016/j.cemconcomp.2011.03.012

11. Schlangen, E., and Sangadji, S., “Addressing Infrastructure Durability and Sustainability by Self Healing Mechanisms—Recent Advances in Self Healing Concrete and Asphalt,” Procedia Engineering, V. 54, 2013, pp. 39-57. doi: 10.1016/j.proeng.2013.03.005

12. Giannaros, P.; Kanellopoulos, A.; and Al-Tabbaa, A., “Damage Recovery in Self-Healing Concrete,” HealCON-Conference, Nov. 28-29, 2016, Delft, the Netherlands.

13. Claisse, P., and Dean, C., “Compressive Strength of Concrete after Early Loading,” Proceedings of the Institution of Civil Engineers, V. 166, No. 3, pp. 152-157. doi: 10.1680/coma.11.0005710.1680/coma.11.00057

14. ter Heide, N., and Schlangen, E., “Selfhealing of Early Age Cracks in Concrete,” Proceedings of the First International Conference on Self Healing Materials, Apr. 18-20, 2007, Noordwijk aan Zee, the Netherlands.

15. TC-122-MLC. “Micro-Cracking and Lifetime Performance of Concrete, State of the Art Report – Part 2: Mechanical Micro-Cracking of Concrete,” Materials and Structures, V. 29, Mar, 1996, pp. 67-78.

16. EN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures - Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004.

17. Chen, W., and Skoczylas, F., “Gas Permeability of Macro-Cracked Concrete: Effect of Temperature and Water Saturation,” Fracture Mechanics of Concrete and Concrete Structures—Assessment, Durability, Monitoring and Retrofitting of Concrete Structures, Korea Concrete Institute, Seoul, South Korea, 2010.

18. Hearn, N., “Effect of Shrinkage and Load-Induced Cracking on Water Permeability of Concrete,” ACI Materials Journal, V. 96, No. 2, Mar.-Apr. 1999, pp. 234-241.

19. Picandet, V.; Khelidj, A.; and Bellegou, H., “Crack Effects on Gas and Water Permeability of Concretes,” Cement and Concrete Research, V. 39, No. 6, 2009, pp. 537-547. doi: 10.1016/j.cemconres.2009.03.009

20. Van Mullem, T.; Gruyaert, E.; Debbaut, B.; Caspeele, R.; and De Belie, N., “Novel Active Crack Width Control Technique to Reduce the Variation on Water Permeability Results for Self-Healing Concrete,” Construction and Building Materials, V. 203, 2019, pp. 541-551. doi: 10.1016/j.conbuildmat.2019.01.105

21. Andrade, J. S. Jr.; Costa, U. M. S.; Almeida, M. P.; Makse, H. A.; and Stanley, H. E., “Inertial Effects on Fluid Flow through Disordered Porous Media,” Physical Review Letters, V. 82, No. 26, 1999, pp. 5249-5252. doi: 10.1103/PhysRevLett.82.5249

22. EN 197-1:2011, “Cement - Part 1: Composition, Specifications and Conformity Criteria for Common Cements,” European Committee for Standardization, Brussels, Belgium, 2011.

23. EN 206:2013+A1:2016, “Concrete - Specification, Performance, Production and Conformity,” European Committee for Standardization, Brussels, Belgium, 2013.

24. UNI 11164:2005, “Calcestruzzo - Determinazione della Permeabilità all'Ossigeno,” UNI Ente Italiano di Normazione, Milan, Italy.

25. Zeng, Z., and Grigg, R., “A Criterion for Non-Darcy Flow in Porous Media,” Transport in Porous Media, V. 63, No. 1, 2006, pp. 57-69. doi: 10.1007/s11242-005-2720-3

26. Lucas, Y.; Panfilov, M.; and Buès, M., “High Velocity Flow through Fractured and Porous Media: The Role of Flow Non-Periodicity,” European Journal of Mechanics - B/Fluids, V. 26, No. 2, 2007, pp. 295-303. doi: 10.1016/j.euromechflu.2006.04.005


ALSO AVAILABLE IN:

Electronic Materials Journal