Evaluation of CO2 Uptake of Fly-Ash-Blended High-Strength Concrete Due to Carbonation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of CO2 Uptake of Fly-Ash-Blended High-Strength Concrete Due to Carbonation

Author(s): Xiao-Yong Wang

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 231-241

Keywords: carbonation model; CO2 uptake; fly ash; high-strength concrete

DOI: 10.14359/51725982

Date: 11/1/2020

Abstract:
Carbonation of concrete can cause the uptake of CO2 and alleviate the CO2 emissions burden of the concrete industry. This study shows a procedure for evaluating the CO2 uptake of fly ash (FA)-blended high-strength concrete, considering both the service and recycling stages. First, a blended cement hydration model is proposed to evaluate the contents of carbonizable substances, porosity, and CO2 diffusivity. In the service stage, a one-dimensional carbonation model is proposed for evaluating carbonation depth. In the recycling stage, an unreacted core model is proposed for evaluating the carbonation process of spherical crushed concrete. Second, CO2 uptake models are proposed for the service and recycling stages, considering concrete materials, structural elements, and environmental exposure. The total CO2 uptake ratio is determined as the sum of CO2 uptake in the service and recycling stages. The calculation results show that, as the FA replacement ratio increases from 0 to 40%, the CO2 uptake ratio in the service stage increases from 2.78 to 4.72%, and the total CO2 uptake ratio increases from 18.9 to 20.8%. As the surface to volume ratio of the structural element increases, or the size of particles of crushed concrete decreases, the rate of CO2 uptake increases but the total CO2 uptake ratio does not change.

Related References:

1. Chen, T.; Gao, X.; and Qin, L., “Mathematical Modeling of Accelerated Carbonation Curing Of Portland Cement Paste At Early Age,” Cement and Concrete Research, V. 120, 2019, pp. 187-197. doi: 10.1016/j.cemconres.2019.03.025

2. Papadakis, V. G.; Fardis, M. N.; and Vayenas, C. G., “Hydration and Carbonation of Pozzolanic Cements,” ACI Materials Journal, V. 89, No. 2, Mar.-Apr. 1992, pp. 119-130.

3. Papadakis, V. G., “Effect of Supplementary Cementing Materials on Concrete Resistance Against Carbonation And Chloride Ingress,” Cement and Concrete Research, V. 30, No. 2, 2000, pp. 291-299. doi: 10.1016/S0008-8846(99)00249-5

4. Wang, X.-Y., and Luan, Y., “Modeling of Hydration, Strength Development, and Optimum Combinations of Cement-Slag-Limestone Ternary Concrete,” International Journal of Concrete Structures and Materials, V. 12. 2018.

5. Lagerblad, B., “Carbon Dioxide Uptake During Concrete Life Cycle– State of the Art,” Swedish Cement and Concrete Research Institute, Stockholm, Sweden, 2005, pp. 1-47.

6. Souto-Martinez, A.; Delesky, E. A.; Foster, K. E. O.; and Srubar, W. V. III, “A Mathematical Model for Predicting the Carbon Sequestration Potential of Ordinary Portland Cement (Opc) Concrete,” Construction and Building Materials, V. 147, 2017, pp. 417-427. doi: 10.1016/j.conbuildmat.2017.04.133

7. Lee, S.; Park, W.; and Lee, H., “Life Cycle CO2 Assessment Method for Concrete Using CO2 Balance and Suggestion to Decrease Lcco2 of Concrete in South-Korean Apartment,” Energy and Building, V. 58, 2013, pp. 93-102. doi: 10.1016/j.enbuild.2012.11.034

8. Possan, E.; Felix, E. F.; and Thomaz, W. A., “Co2 Uptake by Carbonation of Concrete During Life Cycle of Building Structures,” Journal of Building Pathology and Rehabilitation, V. 1, No. 1, 2016, p. 7. doi: 10.1007/s41024-016-0010-9

9. Kim, T., and Chae, C. U., “Evaluation Analysis of the CO2 Emission and Absorption Life Cycle for Precast Concrete in Korea,” Sustainability, V. 8, No. 7, 2016, pp. 663-676. doi: 10.3390/su8070663

10. Yang, K.-H.; Seo, E.-A.; and Tae, S.-H., “Carbonation and CO2 Uptake of Concrete,” Environmental Impact Assessment Review, V. 46, 2014, pp. 43-52. doi: 10.1016/j.eiar.2014.01.004

11. Kwon, S.-J., “Effect of Mineral Admixture on CO2 Emissions and Absorption in Relation to Service Life and Varying CO2 Concentrations,” International Journal of Sustainable Building Technology and Urban Development, V. 7, No. 3-4, 2016, pp. 165-173. doi: 10.1080/2093761X.2016.1237393

12. Engelsen, C. J., and Justnes, H., “CO2 Binding by Concrete,” SINTEF Building and Infrastructure, Oslo, Norway, 2014.

13. Levenspiel, O., Chemical Reaction Engineering, Wiley, New York, 1999.

14. Castellote, M., and Andrade, C., “Modelling the Carbonation of Cementitious Matrixes by Means of the Unreacted-Core Model, UR-CORE,” Cement and Concrete Research, V. 38, No. 12, 2008, pp. 1374-1384. doi: 10.1016/j.cemconres.2008.07.004

15. Thomas, M., Supplementary Cementing Materials in Concrete, CRC press, Boca Raton, FL, 2013.

16. Ashraf, W., “Carbonation of Cement-Based Materials: Challenges and Opportunities,” Construction and Building Materials, V. 120, 2016, pp. 558-570. doi: 10.1016/j.conbuildmat.2016.05.080

17. Liu, J.; Qiu, Q.; Chen, X.; Wang, X.; Xing, F.; Han, N.; and He, Y., “Degradation of Fly Ash Concrete Under the Coupled Effect of Carbonation and Chloride Aerosol Ingress,” Corrosion Science, V. 112, 2016, pp. 364-372. doi: 10.1016/j.corsci.2016.08.004

18. Šavija, B., and Lukovic´, M., “Carbonation of Cement Paste: Understanding, Challenges, and Opportunities,” Construction and Building Materials, V. 117, 2016, pp. 285-301. doi: 10.1016/j.conbuildmat.2016.04.138

19. Wang, X.-Y., “Impact of Climate Change on Proportional Design of Fly Ash Blended Low Co2 Concrete,” ACI Materials Journal, V. 116, No. 3, May 2019, pp. 141-153. doi: 10.14359/51714465

20. Wang, X.-Y., “Analysis of Hydration and Strength Optimization of Cement-Fly Ash-Limestone Ternary Blended Concrete,” Construction and Building Materials, V. 166, 2018, pp. 130-140. doi: 10.1016/j.conbuildmat.2018.01.058

21. Papadakis, V.; Vayenas, C. G.; and Fardis, M. N., “Experimental Investigation and Mathematical Modeling of the Concrete Carbonation Problem,” Chemical Engineering Science, V. 46, No. 5-6, 1991, pp. 1333-1338. doi: 10.1016/0009-2509(91)85060-B

22. Lam, L.; Wong, Y. L.; and Poon, C. S., “Degree of Hydration and Gel/Space Ratio of High-Volume Fly Ash/Cement Systems,” Cement and Concrete Research, V. 30, No. 5, 2000, pp. 747-756. doi: 10.1016/S0008-8846(00)00213-1

23. Shen, Q.; Pan, G.; and Bao, B., “A Method for Calculating the Carbonation Degree of Calcium–Silicate–Hydrate,” Advances in Cement Research, V. 30, No. 9, 2018, pp. 427-436. doi: 10.1680/jadcr.16.00086

24. Jiang, L.; Lin, B.; and Cai, Y., “A Model for Predicting Carbonation of High-Volume Fly Ash Concrete,” Cement and Concrete Research, V. 30, No. 5, 2000, pp. 699-702. doi: 10.1016/S0008-8846(00)00227-1

25. Fang, X.; Xuan, D.; and Poon, C. S., “Empirical Modelling of CO2 Uptake by Recycled Concrete Aggregates under Accelerated Carbonation Conditions,” Materials and Structures, V. 50, No. 4, 2017, p. 200 doi: 10.1617/s11527-017-1066-y

26. Rezagholilou, A.; Papadakis, V. G.; and Nikraz, H., “Rate of Carbonation in Cement Modified Base Course Material,” Construction and Building Materials, V. 150, 2017, pp. 646-652. doi: 10.1016/j.conbuildmat.2017.05.226

27. Zhou, Y.; Pan, L.; Tang, Q.; Zhang, Y.; Yang, N.; and Lu, C., “Evaluation of Carbonation Effects on Cement-Solidified Contaminated Soil Used in Road Subgrade,” Advances in Materials Science and Engineering, V. 2018, 2018, p. 5271324.


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Edit Module Settings to define Page Content Reviewer