Experimental Studies to Investigate Efficacies of Slag as Fine Aggregate Substitute

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Studies to Investigate Efficacies of Slag as Fine Aggregate Substitute

Author(s): T. Hemalatha, Arjun S, and B. S. Sindu

Publication: Materials Journal

Volume: 117

Issue: 5

Appears on pages(s): 241-250

Keywords: M-sand; ordinary portland cement; portland pozzolana cement; river sand; slag aggregate

DOI: 10.14359/51725981

Date: 9/1/2020

Abstract:
This study investigates the feasibility of using induction furnace slag as a substitute for river sand/manufactured sand (M-sand) in the production of concrete. The properties of concrete made with slag fine aggregate is compared with concrete made of river sand and M-sand. Experimental studies have been carried out on concretes made of three types of aggregates and two types of cement (ordinary portland cement [OPC] and portland pozzolana cement [PPC]). Mechanical and durability property tests performed according to standards showed that the characteristics obtained for the concrete made with slag aggregate is comparable with that of the concrete made with river sand and M-sand. This study suggests the 100% replacement of conventional fine aggregate with slag fine aggregate for the production of concrete without compromising the strength and durability characteristics. Further, the study demonstrates that with the suitable measures, the high water absorption of slag aggregate can be compensated.

Related References:

1. USGS, “Cement, Statistics and Information,” U.S. Geological Survey, Reston, VA, 2013.

2. USGS, “Sand and Gravel (Construction) Statistics,” Historical Statistics for Mineral and Material Commodities in the United States, T. D. Kelly and G. R. Matos, eds., U.S. Geological Survey Data Series 140, 2013.

3. Baykal, G., and Doven, A. G., “Utilization of Fly Ash by Pelletization Process; Theory, Application Areas and Research Results,” Resources, Conservation and Recycling, V. 30, No. 1, 2000, pp. 59-77. doi: 10.1016/S0921-3449(00)00042-2

4. Liao, Y. C., and Huang, C. Y., “Effects of Heat Treatment on the Physical Properties of Lightweight Aggregate from Water Reservoir Sediment,” Ceramics International, V. 37, No. 8, 2011, pp. 3723-3730. doi: 10.1016/j.ceramint.2011.04.122

5. Source. www.mineralproducts.org.

6. Khanzadi, M., and Behnood, A., “Mechanical Properties of High-Strength Concrete Incorporating Copper Slag as Coarse Aggregate,” Construction and Building Materials, V. 23, No. 6, 2009, pp. 2183-2188. doi: 10.1016/j.conbuildmat.2008.12.005

7. Ayano, T.; Kuramoto, O.; and Sakata, K., “Concrete with Copper Slag Fine Aggregate,” Zairyo/Journal of the Society of Materials Science, V.4 9, No. 10, 2000, pp. 1097-1102.

8. Ferreira, V. J.; Vilaplana, A. S.; García-Armingol, T.; Aranda-Usón, A.; Lausín-González, C.; López-Sabirón, A. M.; and Ferreira, G., “Evaluation of the Steel Slag Incorporation as Coarse Aggregate for Road Construction: Technical Requirements and Environmental Impact Assessment,” Journal of Cleaner Production, V. 130, 2016, pp. 175-186. doi: 10.1016/j.jclepro.2015.08.094

9. Aggarwal, Y., and Siddique, R., “Microstructure and Properties of Concrete Using Bottom Ash and Waste Foundry Sand as Partial Replacement of Fine Aggregates,” Construction and Building Materials, V. 54, 2014, pp. 210-223. doi: 10.1016/j.conbuildmat.2013.12.051

10. Pathak, N., and Siddique, R., “Effects of Elevated Temperatures on Properties of Self-Compacting-Concrete Containing Fly Ash and Spent Foundry Sand,” Construction and Building Materials, V. 34, 2012, pp. 512-521. doi: 10.1016/j.conbuildmat.2012.02.026

11. EIA, Energy Information Association. https://www.eia.gov.

12. Sun, J.; Feng, J.; and Chen, Z., “Effect of Ferronickel Slag as Fine Aggregate on Properties of Concrete,” Construction and Building Materials, V. 206, 2019, pp. 201-209. doi: 10.1016/j.conbuildmat.2019.01.187

13. Chunlin, L.; Kunpeng, Z.; and Depeng, C., “Possibility of Concrete Prepared with Steel Slag as Fine and Coarse Aggregates: A Preliminary Study,” Procedia Engineering, V. 24, 2011, pp. 412-416. doi: 10.1016/j.proeng.2011.11.2667

14. Guo, Y.; Xie, J.; Zheng, W.; and Li, J., “Effects of Steel Slag as Fine Aggregate on Static and Impact Behaviours of Concrete,” Construction and Building Materials, V. 192, 2018, pp. 194-201. doi: 10.1016/j.conbuildmat.2018.10.129

15. Yüksel, İ.; Bilir, T.; and Özkan, Ö., “Durability of Concrete Incorporating Non-Ground Blast Furnace Slag and Bottom Ash as Fine Aggregate,” Building and Environment, V. 42, No. 7, 2007, pp. 2651-2659. doi: 10.1016/j.buildenv.2006.07.003

16. Singh, G., and Siddique, R., “Strength Properties and Micro-Structural Analysis of Self-Compacting Concrete Made with Iron Slag as Partial Replacement of Fine Aggregates,” Construction and Building Materials, V. 127, 2016, pp. 144-152. doi: 10.1016/j.conbuildmat.2016.09.154

17. Monosi, S.; Ruello, M. L.; and Sani, D., “Electric Arc Furnace Slag as Natural Aggregate Replacement in Concrete Production,” Cement and Concrete Composites, V. 66, 2016, pp. 66-72. doi: 10.1016/j.cemconcomp.2015.10.004

18. Manso, J. M.; Polanco, J. A.; Losanez, M.; and Gonzalez, J. J., “Durability of Concrete Made with EAF Slag as Aggregate,” Cement and Concrete Composites, V. 28, No. 6, 2006, pp. 528-534. doi: 10.1016/j.cemconcomp.2006.02.008

19. Dash, M. K., and Patro, S. K., “Performance Assessment of Ferrochrome Slag as Partial Replacement of Fine Aggregate in Concrete,” European Journal of Environmental and Civil Engineering, V. 21, 2018, pp. 1-20. doi: 10.1080/19648189.2018.1539674

20. Saha, A. K., and Sarker, P. K., “Durability Characteristics of Concrete Using Ferronickel Slag Fine Aggregate and Fly Ash,” Magazine of Concrete Research, V. 70, No. 17, 2018, pp. 865-874. doi: 10.1680/jmacr.17.00260

21. IS 2386-1, “Methods of Test for Aggregates for Concrete, Part I: Particle Size and Shape,” Indian Standard, New Delhi, India.

22. IS 2386-3, “Methods of Test for Aggregates for Concrete, Part 3: Specific Gravity, Density, Voids, Absorption and Bulking,” Indian Standard, New Delhi, India.

23. ASTM C1585-13, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes,” ASTM International, West Conshohocken, PA, 2013, doi: https://doi.org/10.1520/C1585-13.10.1520/C1585-13

24. Lam, M. N.; Le, D. H.; and Jaritngam, S., “Compressive Strength and Durability Properties of Roller-Compacted Concrete Pavement Containing Electric Arc Furnace Slag Aggregate and Fly Ash,” Construction and Building Materials, V. 191, 2018, pp. 912-922. doi: 10.1016/j.conbuildmat.2018.10.080

25. IS 456-2000, “Indian Standard Plain and Reinforced Concrete Code of Practice,” Bureau of Indian Standards, New Delhi, 2000.

26. ASTM C1202-19, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2019. doi: https://doi.org/10.1520/C1202-19.10.1520/C1202-19

27. DIN 1048 (Part-5), “German Standard for Determination of Permeability of Concrete,” German Institute for Standardization, Berlin, Germany.

28. Dias, W. P., “Reduction of Concrete Sorptivity with Age through Carbonation,” Cement and Concrete Research, V. 30, No. 8, 2000, pp. 1255-1261. doi: 10.1016/S0008-8846(00)00311-2

29. Martys, N. S., and Ferraris, C. F., “Capillary Transport in Mortars and Concrete,” Cement and Concrete Research, V. 27, No. 5, 1997, pp. 747-760. doi: 10.1016/S0008-8846(97)00052-5

30. Chen, L.; Zheng, K.; Xia, T.; and Long, G., “Mechanical Property, Sorptivity and Microstructure of Steam-Cured Concrete Incorporated with the Combination of Metakaolin-Limestone,” Case Studies in Construction Materials., V. 11, 2019, p. e00267 doi: 10.1016/j.cscm.2019.e00267

31. Chen, J. J.; Kwan, A. K.; and Jiang, Y., “Adding Limestone Fines as Cement Paste Replacement to Reduce Water Permeability and Sorptivity of Concrete,” Construction and Building Materials, V. 56, 2014, pp. 87-93. doi: 10.1016/j.conbuildmat.2014.01.066

32. Cement Concrete & Aggregates Australia, “Chloride Resistance of Concrete,” Report, June 2009, www.ccaa.com.au. (last accessed October 8, 2020)


ALSO AVAILABLE IN:

Electronic Materials Journal