Evaluation of adhesion strength in concrete with crack induced due to steel corrosion by nondestructive testing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of adhesion strength in concrete with crack induced due to steel corrosion by nondestructive testing

Author(s): Yuto Nakagawa

Publication: TCA

Volume: Vol. 7 No. 1 (2019): Vol. 7 No. 1: January - June

Issue:

Appears on pages(s): 7-14

Keywords: Half-cell Potential, Ultrasonic Testing, Steel Corrosion, Internal Crack, Adhesion Stress

DOI:

Date: 11/18/2018

Abstract:
Currently, it is regarded as a problem that aged structures are rapidly increasing in maintenance of RC members. Therefore, it is desirable to integrate rational inspection and repair for aged RC members in maintenance. In other words, it is ideal to first conduct a standard investigation for a wide area in a short time and then to examine the degree of deterioration in detail at a limited range. Therefore, it is necessary to consider the corrosion of the steel bar which serves as the nucleus in the maintenance control against chloride attack, and the adhesion characteristics between the steel bar and the concrete decreased thereby. However, a quantitative and systematical estimation method has not been established for the steel corrosion in RC members. Therefore, in this study, specimens having several degrees of steel corrosion were prepared within the range where no cracks appeared on the surface. A combination of nondestructive testing was conducted to estimate the adhesion strength between steel bars and concrete. The degree of steel corrosion was estimated first by the half-cell potential, then internal cracks due to steel corrosion in concrete were visually investigated by ultrasonic tomography method. As a result of this experiment, it was possible to identify the corroded area was specified with the half-cell potential. Moreover, as corrosion progressed, it became clear that the ultrasonic velocity around the steel bar decreased, and the adhesion strength between the steel bar and the concrete decreased. Therefore, this study could develop a maintenance method combining the half-cell potential and the ultrasonic tomography method.