533.1R-20: Guide for Design and Construction Responsibilities for Architectural Precast Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 533.1R-20: Guide for Design and Construction Responsibilities for Architectural Precast Concrete

Author(s): ACI Committee 533

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 12

Keywords: architect; architectural precast concrete; construction manager; general contractor; owner; precaster; specialty structural engineer; structural engineer of record

DOI:

Date: 5/4/2020

Abstract:
Architectural precast concrete is a subcategory of concrete construction that involves the same basic entities as other concrete construction, but is cast in a plant and has a more decorative appeal by using color, texture, distinguished surface finishes, or all of these. This document outlines the responsibilities for various parties of the design/construction team for architectural precast concrete projects and does not necessarily apply to concrete or precast concrete in general.