Title:
Spatial Variation of Concrete Strength in Safety Evaluation of Existing Structures
Author(s):
Ming Liu
Publication:
Symposium Paper
Volume:
340
Issue:
Appears on pages(s):
197-209
Keywords:
spatial variation; concrete strength; safety evaluation; existing structures; statistical
DOI:
10.14359/51725813
Date:
4/1/2020
Abstract:
The root causes of uncertainties in new concrete structures have been evidenced to be substantially different from those in safety evaluation of existing structures. Therefore, the design methodology in ACI 318 shall be re-calibrated to better reflect the effects of these significant differences, particularly for the spatial variation of concrete strength in existing structures. The degree of uncertainties that whether the testing data can reliably represent the concrete strength at the critical locations of interesting has been identified to play a vital role in developing an effective structural safety evaluation methodology. This paper presents a novel statistical procedure, where the semi-variogram modeling is used to establish the spatial variation of concrete strength so that the degree of uncertainty mentioned above can be quantified as a function of the spacing intervals of the testing points. Kriging is used to estimate the expected concrete strength with the desired confidence levels for the locations between the measurement locations to ensure the critical locations are covered. The actual concrete coring data were analyzed to illustrate how to estimate the spatial variation. The proposed methodology can also be applied to any testing data that can characterize the stochastic properties of concrete strength in existing structures.
Related References:
ACI 214.4R, 2010, “Guide for obtaining cores and interpreting compressive strength results”, Farmington Hills: American Concrete Institute (ACI).
ACI 318, 2014, “Building code requirements for structural concrete and commentary”, Farmington Hills: American Concrete Institute (ACI).
ACI 348, 2016, Tech Note 1: What is the inherent probability of exceedance of the equivalent design concrete compressive strength based on ACI 318, 214.4R, and 562?, Farmington Hills: American Concrete Institute (ACI) (under TAC review)
ACI 562, 2016, “Code requirements for evaluation, repair, and rehabilitation of concrete buildings and commentary”, Farmington Hills: American Concrete Institute (ACI).
CSA Group, 2014, “Canadian highway bridge design code”, Canadian Standards Association Huang, H. and Liu, M. 2018. Risk-based performance evaluation for concrete bridge deck repair. Proceeding of the Ninth International Conference on Bridge Maintenance, Safety and Management (IABMAS 2018)
McCuen, R.H. , Aggour, M.S. and Ayyub, B.M. 1988. Spacing for accuracy in ultrasonic testing of bridge timber piles, Journal of Structural Engineering, American Society of Civil Engineers, 114(12), 2652-2668
Micic, T.V. Chryssanthopoulos, M.K. and Baker, M.J. 1995. Reliability analysis of highway bridge deck assessment, Structural Safety 17, 135-150
Nowak, A.S. and Szerszen, M.M. 2003. Calibration of design code for buildings (ACI 318): Part 1 – statistical models for resistance, ACI Structural Journal, 100(3), 377-382
Shinozuka, M. 1972. Probabilistic modeling of concrete structure, Journal of the Engineering Mechanics Division, Proceeding of the American Society of Civil Engineers, 98(EM6), 1433-1451
Szerszen, M.M. & Nowak, A.S. 2003. Calibration of design code for buildings (ACI 318): Part 2 – reliability analysis and resistance factors, ACI Structural Journal, 100(3), 383-391