Analysis of a Fire Damaged and FRP Laminate Strengthened Reinforced Concrete Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of a Fire Damaged and FRP Laminate Strengthened Reinforced Concrete Bridge

Author(s): Santosh Timilsina, Nur Yazdani, Eyosias Beneberu, and Abel Mulenga

Publication: Symposium Paper

Volume: 340

Issue:

Appears on pages(s): 179-196

Keywords: bridge tests, distribution factors, evaluation, fiber-reinforced polymer (FRP) strengthening, finite element analysis, fire damaged bridge, load testing

DOI: 10.14359/51725812

Date: 4/1/2020

Abstract:
Fire is a possible hazard on highway bridges which causes significant economic damage, and it is also one of the least investigated of all hazards. There is a lack of knowledge on the long term performance and structural integrity of fire damaged and fiber reinforced polymer (FRP) laminate retrofitted bridges. One such rare in-service bridge was selected for this study. The fire damaged cast-in-place non-prestressed girders were previously repaired with mortar and strengthened with FRP wrapping. The girders were instrumented with strain gages and displacement transducers, and a non-destructive live load test was carried out to evaluate the structural response. The results from the load testing were used to compare two identical girder spans with and without CFRP strengthening. A full-scale non-linear finite element model of the overall bridge superstructure was created, and the test results used to calibrate the model. The carbon (CFRP) strengthened girder exhibited similar stiffness compared to the undamaged girder as evidenced by almost equivalent mid-span deflection. The girder moment capacity decreased significantly due to fire damage, and the CFRP strengthening plus mortar repair was successful in restoring the moment capacity. The finite element model provided good correlation with load test results.

Related References:

1. Aidoo, J., Harries, K. A., & Petrou, M. F. (2006). “Full-scale experimental investigation of repair of reinforced concrete interstate bridge using CFRP materials.” Journal of Bridge Engineering, 11(3), 350-358.

2. Akinci, N. O., Liu, J., and Bowman, M. D. (2008). “Parapet strength and contribution to live-load response for superload passages.” J. Bridge Eng., 13(1), 55–63. 3. Alnahhal, W. I., Chiewanichakorn, M., Aref, A. J., & Alampalli, S. (2006). “Temporal thermal behavior and damage simulations of FRP deck.” Journal of Bridge Engineering, 11(4), 452-464.

4. Alos-Moya, J., Paya-Zaforteza, I., Garlock, M. E., Loma-Ossorio, E., Schiffner, D., & Hospitaler, A. (2014). “Analysis of a bridge failure due to fire using computational fluid dynamics and finite element models.” Engineering Structures, 68, 96-110.

5. American Association of State Highway and Transportation Officials. (2011a). “Manual for Bridge Evaluation, 2nd Edition.” C3, Washington, DC.

6. American Association of State Highway and Transportation Officials. (2011b). AASHTO LRFD Bridge Design Specifications, Customary U.S. Units, 7th Edition, Farmington Hills, MI.

7. ASCE. (2017). “2017 report card for America’s infrastructure.’’ ASCE.

8. ASTM C39/C39M (2014a). “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” Annual Book of ASTM Standards, ASTM International, Vol. 04. 02, West Conshohocken, PA

9. ASTM D3039/D3039M (2014b). “Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials,” Annual Book of ASTM Standards, ASTM International, Vol. 04. 02, West Conshohocken, PA

10. Bakht, B., & Jaeger, L. G. (1990). “Bridge testing—A surprise every time.” Journal of Structural Engineering, 116(5), 1370-1383.

11. Barr, P. J., Eberhard, M. O., & Stanton, J. F. (2001). “Live-load distribution factors in prestressed concrete girder bridges.” Journal of Bridge Engineering, 6(5), 298-306.

12. Chajes, M. J., Mertz, D. R., & Commander, B. (1997). “Experimental load rating of a posted bridge.” Journal of Bridge Engineering, 2(1), 1-10.

13. Chung, W., & Sotelino, E. D. (2006). “Three-dimensional finite element modeling of composite girder bridges.” Engineering Structures, 28(1), 63-71.

14. Eom, J., & Nowak, A. S. (2001). “Live load distribution for steel girder bridges.” Journal of Bridge Engineering, 6(6), 489-497.

15. El Shahawy, M., and Garcia, A. M. (1989). "Structural research and testing in Florida." Structural Res. Rep. No. SRR-01-89, Fla. Dept. of Transp., Tallahassee, Fla

16. Evarts, B. (2018) “Fire loss in the United States during 2017.” National Fire Protection Association, Quincy, MA.

17. Fu, G., Sardis, P., and Tang, 1. (1992). "Proof testing of highway bridges." Res. Rep. 153, Engineering. Res. and Development Bureau, N.Y. State Dept. of Transp., Albany, N.Y.

18. Gong, X. and Agrawal, A. (2014). "Numerical simulation of fire damage to a long-span truss bridge." J. Bridge Eng., Volume 20, Issue 10, Pages.

19. Gustaferro, A. H., & Martin, L. D. (1989). “Design for fire resistance of precast prestressed concrete (p. 85). Chicago”. Prestressed Concrete Institute.

20. Hag-Elsafi, O., Alampalli, S., & Kunin, J. (2001). “Application of FRP laminates for strengthening of a reinforced-concrete T-beam bridge structure.” Composite structures, 52(3-4), 453-466.

21. Hamedi, M., Eshragh, S., Franz, M., & Sekula, P. M. (2018). “Analyzing Impact of I-85 Bridge Collapse on Regional Travel in Atlanta (No. 18-04563)”.

22. Klaiber, F. W., T. J. Wipf, C. M. Streeter, “Testing of Old Reinforced Concrete Bridges”, Iowa Department of Transportation Project HR-390, Iowa State University, December, 1997.

23. Lichtenstein, A. G. (1995). “Bridge rating through nondestructive load testing.” National Cooperative Highway Research Program Project, 12-28.

24. Mabsout, M. E., Tarhini, K. M., Frederick, G. R., & Tayar, C. (1997). “Finite-element analysis of steel girder highway bridges.” Journal of Bridge Engineering, 2(3), 83-87.

25. Markey, I. (1991). “Load testing of Swiss bridges.” Steel Construction Today, 5(1), 15-20.

26. Mayo, R., Nanni, A., Gold, W., & Barker, M. (1999, November). “Strengthening of bridge G270 with externallybonded CFRP reinforcement.” In SP-188, American Concrete Institute, Proc., 4th International Symposium on FRP for Reinforcement of Concrete Structures (FRPRCS4), Baltimore, MD, Nov (pp. 429-440).

27. McGrattan, K., Klein, B., Hostikka, S., & Floyd, J. (2010). “Fire dynamics simulator (version 5), user’s guide.” NIST special publication, 1019(5), 1-186.

28. Moses, E, Lebet, J. P., and Bez, R. (1994). “Applications of field testing to bridge evaluation.” Journal of Structural Engineering, ASCE, 120(6), 1745-1762. 29. Nigro, E., Manfredi, G., Cosenza, E., & Zappoli, M. (2006, June). “Effects of high temperature on the performances of RC bridge decks strengthened with externally bonded FRP reinforcement.” In Proceedings of 2nd International fib Conference, Naples, Italy (pp. 5-8).

30. Pallempati, H., Beneberu, E., Yazdani, N., & Patel, S. (2016). “Condition assessment of fiber-reinforced polymer strengthening of concrete bridge components.” Journal of Performance of Constructed Facilities, 30(6), 04016052.

31. Purkiss, J., A. (2007). “Fire safety engineering design of structures.” Butterworth-Heinemann, Elsevier, Oxford, UK, 2007.

32. Reed, C. E., Peterman, R. J., & Rasheed, H. A. (2005). “Evaluating FRP repair method for cracked prestressed concrete bridge members subjected to repeated loadings (Phase 1)” (No. K-TRAN: KSU-01-2).

33. Schiebel, S., Parretti, R., Nanni, A., & Huck, M. (2002). “Strengthening and load testing of three bridges in Boone County, Missouri.” Practice periodical on structural design and construction, 7(4), 156-163.

34. Schulz, J. L. (1993). “In search of better load ratings.” Civil Engineering, 63(9), 62.

35. Shanafelt, G. O., & Horn, W. B. (1985). “Guidelines for Evaluation and Repair of Prestressed Concrete Bridge Members.” NCHRP Report, (280).

36. SIMULIA (2016). “ABAQUS standard user’s manual. Version 6.14, vol. I–III.” Pawtucket (America): Hibbitt, Karlsson & Sorensen, Inc.

37. Stallings, J. M., Tedesco, J. W., El-Mihilmy, M., & McCauley, M. (2000). “Field performance of FRP bridge repairs.” Journal of Bridge Engineering, 5(2), 107-113.

38. Timilsina, S. (2019), “In-service performance evaluation of fire and impact damaged bridges with CFRP laminate strengthening.” (Ph.D. Dissertation), The University of Texas at Arlington, Arlington, TX.

39. TxDOT (2014). “Item 421.” Texas Department of Transportation.

40. Wright, W., Lattimer, B., Woodworth, M., Nahid, M., and Sotelino, E. (2013), NCHRP 12-85. “Highway bridge fire hazard assessment”, Transportation Research Board, Blacksburg, VA.

41. Yost, J. R., Schulz, J. L., & Commander, B. C. (2005). “Using NDT data for finite element model calibration and load rating of bridges.” In Structures Congress 2005: Metropolis and Beyond (pp. 1-9).

42. Yousif, Z., & Hindi, R. (2007). “AASHTO-LRFD live load distribution for beam-and-slab bridges: Limitations and applicability.” Journal of Bridge Engineering, 12(6), 765-773.

43. Zhang, Z., & Aktan, A. E. (1997). “Different levels of modeling for the purpose of bridge evaluation.” Applied Acoustics, 50(3), 189-204.