Concrete Q&A: Epoxy-Coated Reinforcement and Cryogenic Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A: Epoxy-Coated Reinforcement and Cryogenic Temperatures

Author(s):

Publication: Concrete International

Volume: 42

Issue: 5

Appears on pages(s): 68

Keywords:

DOI: 10.14359/51725800

Date: 5/1/2020

Abstract:
I’m designing a foundation to support a liquefied natural gas (LNG) tank in a marine environment, and I want to use epoxy-coated reinforcement (ECR). In case of a major spill, the pier will be exposed to LNG at cryogenic temperatures. However, per Section 4.7.1 of ACI 376-11,1 deformed reinforcement at service temperatures equal or greater than 0°F (–18°C) must be uncoated. How can I meet the code and protect the reinforcement?

Related References:

1. ACI Committee 376, “Code Requirements for Design and Construction of Concrete Structures for the Containment of Refrigerated Liquefied Gases (ACI 376-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 149 pp.

2. ASTM A706/A706M-16, “Standard Specification for Deformed and Plain Low-Alloy Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016, 7 pp.

3. CAN/CSA G30.18-M92 (R2007), “Billet-Steel Bars for Concrete Reinforcement,” CSA Group, Canada, 1992. (withdrawn, superseded by G30.18-09)

4. “Technical Data Sheet from Arbed,” Krybar, Jan. 1981.

5. “Production and Properties of Low Carbon 25Mn 5Cr 1Ni Austenitic Steel,” Nippon Research Report, Nippon Steel Corporation, 1980, pp. 1-19.

6. “Technical Document No. 221-037,” Nippon Kokan Corporation, Ltd., 1980.

7. Dodge, E., “How Dangerous Is LNG?,” Dec. 22, 2014. Breaking Energy website: https://breakingenergy.com/2014/12/22/how-dangerous-is-lng/. Accessed Mar. 27, 2020.