Load Test of a Precast Concrete Tub Stadium Riser and Bond Testing of #20 Bar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load Test of a Precast Concrete Tub Stadium Riser and Bond Testing of #20 Bar

Author(s): Jeremiah Fasl

Publication: Web Session

Volume: ws_F19_Fasl.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/24/2019

Abstract:
During installation of precast concrete tub risers at a collegiate stadium in the United States, cracking was observed shortly after installation. Because the precast concrete risers were cracking within a cantilevering portion of the stadium, the Engineer-of-Record was concerned with the safety and durability of the risers and requested that one of the risers be load tested in accordance with the requirements of ACI 318-11. As such, a riser was instrumented with multiple string potentiometers to measure the deflection response as the riser was loaded with water (using industrial sized totes) to the total test load magnitude. This presentation will discuss the condition of the risers, as well as the methodology and results of the load test.