Experimental Testing of Tension-Loaded Deformed Anchors in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Testing of Tension-Loaded Deformed Anchors in Concrete

Author(s): Rachel Chicchi, Amit H. Varma, Jungil Seo, Thomas Bradt, and Ethan McCarty

Publication: Structural Journal

Volume: 117

Issue: 5

Appears on pages(s): 133-146

Keywords: breakout failure; deformed reinforcing bar anchors; deformed wire anchors; group anchor assemblies; tension-loaded

DOI: 10.14359/51724670

Date: 9/1/2020

Abstract:
Embed plates anchored with welded deformed reinforcing bars or heavy-gauge deformed wire are commonly used for attachments in nuclear facilities. These connections may experience significant tension and/or shear. The required embedment of the welded bars is typically determined based on development length concepts, with the assumption that the nominal tensile capacity of the connection can be taken as the tension yield strength of the bars. This paper presents results of large-scale experimental investigations conducted to evaluate the tensile capacity of such embed plates. Single anchor pullout test results are also presented to categorize bond behavior for deformed reinforcing bar anchors (DRAs) and deformed wire anchors (DWAs). Preliminary results indicate that adoption of the design paradigm given in the Code for the concrete-governed strength of bonded anchors can provide a reasonable approximation for DRAs but requires additional calibration and study for application to DWAs owing to their diminished bond capacity.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 620 pp.

2. ACI Committee 349, “Code Requirements for Nuclear Safety Related Concrete Structures (ACI 349-13),” American Concrete Institute, Farmington Hills, MI, 2013, 196 pp.

3. Fuchs, W.; Eligehausen, R.; and Breen, J. E., “Concrete Capacity Design (CCD) Approach for Fastening to Concrete,” ACI Structural Journal, V. 92, No. 1, Jan.-Feb. 1995, pp. 787-802.

4. Eligehausen, R., and Balogh, T., “Behavior of Fasteners Loaded in Tension in Cracked Reinforced Concrete,” ACI Structural Journal, V. 92, No. 3, May-June 1995, pp. 365-379.

5. Eligehausen, R.; Cook, R. A.; and Appl, J., “Behavior and Design of Adhesive Bonded Anchors,” ACI Structural Journal, V. 103, No. 6, Nov.-Dec. 2006, pp. 822-831.

6. Silva, J., and Eligehausen, R., “Design of Reinforcing Bar Anchorages for Tension Loading,” Joint ACI-fib Session on Bond in Concrete, The ACI Concrete Convention and Exposition, Detroit, MI, Mar. 26-30, 2017.


ALSO AVAILABLE IN:

Electronic Structural Journal