Reliability Analysis of Carbon Fiber-Reinforced Polymer Shear-Strengthened Reinforced Concrete Beams Subjected to Deterioration

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reliability Analysis of Carbon Fiber-Reinforced Polymer Shear-Strengthened Reinforced Concrete Beams Subjected to Deterioration

Author(s): Amirmasoud Taki, Afshin Firouzi, and Saeed Mohammadzadeh

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 25-38

Keywords: carbon fiber-reinforced polymer (CFRP); deterioration models; Monte Carlo simulation (MCS); reinforced concrete (RC); shear failure; time-dependent reliability analysis

DOI: 10.14359/51724663

Date: 7/1/2020

Abstract:
A time-dependent reliability analysis of reinforced concrete (RC) beams shear-strengthened with carbon fiber-reinforced polymer (CFRP) sheets is conducted. Environmental effects are considered as two state degradation function representing retention in strength of CFRP and three state chloride ion attack on steel reinforcement. Modeling these deterioration mechanisms, a time-variant reliability analysis of fiber-reinforced polymer (FRP)-strengthened beams with respect to possible shear failures, including delamination of FRP sheets and ultimate shear failure, are conducted during their lifetime. In the proposed methodology, these shear failure limit states are formulated based on the ACI 440.2R provisions; then, an event-based Monte Carlo simulation (MCS) is employed to calculate lifetime reliability indexes. The merit of the proposed reliability analysis framework is that by explicitly considering the environmental deterioration mechanisms in different harshness classifications, one can more precisely predict the lifetime risk of failure. It is found that by using the proposed analysis framework, the probability of the survival of the beam conditional on FRP delamination can be calculated. Furthermore, this study reveals the impact of the level of load-carrying capacity of delaminated FRPs—namely, α factor—on the ultimate reliability of beams. It is concluded that there is a significant difference of the safety of beams with the variable levels of α, which highlights the need for further investigation of the real behavior of these strengthened beams to classify into serviceability or ultimate limit state.

Related References:

ACI Committee 440, 2017, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 114 pp.

Alsayed, S. H., and Siddiqui, N. A., 2013, “Reliability of Shear-Deficient RC Beams Strengthened with CFRP-Sheets,” Construction and Building Materials, V. 42, pp. 238-247. doi: 10.1016/j.conbuildmat.2013.01.024

Amidi, S., and Wang, J., 2016, “Subcritical Debonding of FRP-to-Concrete Bonded Interface under Synergistic Effect of Load, Moisture, and Temperature,” Mechanics of Materials, V. 92, pp. 80-93. doi: 10.1016/j.mechmat.2015.09.001

Atadero, R. A., and Karbhari, V. M., 2008, “Calibration of Resistance Factors for Reliability-Based Design of Externally-Bonded FRP Composites,” Composites. Part B, Engineering, V. 39, No. 4, pp. 665-679. doi: 10.1016/j.compositesb.2007.06.004

Baji, H.; Ronagh, H. R.; and Li, C. Q., 2016a, “Probabilistic Assessment of FRP-Confined Reinforced Concrete Columns,” Composite Structures, V. 153, pp. 851-865. doi: 10.1016/j.compstruct.2016.07.003

Baji, H.; Ronagh, H. R.; and Li, C. Q., 2016b, “Probabilistic Design Models for Ultimate Strength and Strain of FRP-Confined Concrete,” Journal of Composites for Construction, ASCE, V. 20, No. 6, p. 04016051 doi: 10.1061/(ASCE)CC.1943-5614.0000704

Baji, H.; Yang, W.; and Li, C. Q., 2017, “An Optimum Strengthening Strategy for Corrosion-Affected Reinforced Concrete Structures,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec., pp. 1591-1602. doi: 10.14359/51700834

Belarbi, A.; Bae, S.; Ayoub, A.; Kuchma, D.; Mirmiran, A.; and Okeil, A., 2011, “Design of FRP Systems for Strengthening Concrete Girders in Shear,” NCHRP Report No. 678, Transportation Research Board, Washington, DC.

Bousselham, A., and Chaallal, O., 2013, “Experimental Investigations on the Influence of Size on the Performance of RC T-Beams Retrofitted in Shear with CFRP Fabrics,” Engineering Structures, V. 56, pp. 1070-1079. doi: 10.1016/j.engstruct.2013.06.028

Cao, S. Y.; Chen, J. F.; Teng, J. G.; Hao, Z.; and Chen, J., 2005, “Debonding in RC Beams Shear Strengthened with Complete FRP Sheets,” Journal of Composites for Construction, ASCE, V. 9, No. 5, pp. 417-428. doi: 10.1061/(ASCE)1090-0268(2005)9:5(417)

Chen, J. F., and Teng, J. G., 2003a, “Shear Capacity of FRP-Strengthened RC Beams: FRP Debonding,” Construction and Building Materials, V. 17, No. 1, pp. 27-41. doi: 10.1016/S0950-0618(02)00091-0

Chen, J. F., and Teng, J. G., 2003b, “Shear Capacity of Fiber-Reinforced Polymer-Strengthened Reinforced Concrete Beams: Fiber Reinforced Polymer Rupture,” Journal of Structural Engineering, ASCE, V. 129, No. 5, pp. 615-625. doi: 10.1061/(ASCE)0733-9445(2003)129:5(615)

Chu, W.; Wu, L.; and Karbhari, V. M., 2004, “Durability Evaluation of Moderate Temperature Cured E-Glass/Vinylester Systems,” Composite Structures, V. 66, No. 1-4, pp. 367-376. doi: 10.1016/j.compstruct.2004.04.058

Cromwell, J. R.; Harries, K. A.; and Shahrooz, B. M., 2011, “Environmental Durability of Externally Bonded FRP Materials Intended for Repair of Concrete Structures,” Construction and Building Materials, V. 25, No. 5, pp. 2528-2539. doi: 10.1016/j.conbuildmat.2010.11.096

Dias, S. J., and Barros, J. A., 2008, “Shear Strengthening of T Cross Section Reinforced Concrete Beams by Near-Surface Mounted Technique,” Journal of Composites for Construction, ASCE, V. 12, No. 3, pp. 300-311. doi: 10.1061/(ASCE)1090-0268(2008)12:3(300)

Dias, S. J. E., and Barros, J. A. O., 2011, “Shear Strengthening of RC T-Section Beams with Low Strength Concrete Using NSM CFRP Laminates,” Cement and Concrete Composites, V. 33, No. 2, pp. 334-345. doi: 10.1016/j.cemconcomp.2010.10.002

El Hassan, J.; Bressolette, P.; Chateauneuf, A.; and El Tawil, K., 2010, “Reliability-Based Assessment of the Effect of Climatic Conditions on the Corrosion of RC Structures Subject to Chloride Ingress,” Engineering Structures, V. 32, No. 10, pp. 3279-3287. doi: 10.1016/j.engstruct.2010.07.001

El Maaddawy, T.; Soudki, K.; and Topper, T., 2007, “Performance Evaluation of Carbon Fiber-Reinforced Polymer-Repaired Beams under Corrosive Environmental Conditions,” ACI Structural Journal, V. 104, No. 1, Jan.-Feb., pp. 3-11.

Ellingwood, B. R., 2003, “Toward Load and Resistance Factor Design for Fiber-Reinforced Polymer Composite Structures,” Journal of Structural Engineering, ASCE, V. 129, No. 4, pp. 449-458. doi: 10.1061/(ASCE)0733-9445(2003)129:4(449)

fib bulletin 14, 2001, “Externally Bonded FRP Reinforcement for RC Structures,” TG 9.3, International Federation for Structural Concrete, Lausanne, Switzerland.

Firouzi, A.; Taki, A.; and Mohammadzadeh, S., 2016, “Time Dependent Reliability Analysis of Concrete Transportation Infrastructure Shear Strengthened by CFRP Wraps,” Proceedings of the World Congress on Engineering and Computer Science; International Association of Engineers (IAENG), V. 2, San Francisco, CA.

Firouzi, A.; Taki, A.; and Mohammadzadeh, S., 2019, “Time-Dependent Reliability Analysis of RC Beams Shear and Flexural Strengthened with CFRP Subjected to Harsh Environmental Deteriorations,” Engineering Structures, V. 196, p. 109326 doi: 10.1016/j.engstruct.2019.109326

Green, M. F.; Dent, A. J.; and Bisby, L. A., 2003, “Effect of Freeze-Thaw Cycling on the Behavior of Reinforced Concrete Beams Strengthened in Flexure with Fiber Reinforced Polymer Sheets,” Canadian Journal of Civil Engineering, V. 30, No. 6, pp. 1081-1088. doi: 10.1139/l03-059

Iervolino, I., and Galasso, C., 2012, “Comparative Assessment of Load-Resistance Factor Design of FRP-Reinforced Cross Sections,” Construction and Building Materials, V. 34, pp. 151-161. doi: 10.1016/j.conbuildmat.2012.02.021

Karbhari, V. M., and Abanilla, M. A., 2007, “Design Factors, Reliability, and Durability Prediction of Wet Layup Carbon/Epoxy Used in External Strengthening,” Composites. Part B, Engineering, V. 38, No. 1, pp. 10-23. doi: 10.1016/j.compositesb.2006.06.001

Karbhari, V. M.; Chin, J.; Hunston, D.; Benmokrane, B.; Juska, T.; Morgan, R.; Lesko, J. J.; Sorathia, U.; and Reynaud, A. D., 2003, “Durability Gap Analysis for Fiber-Reinforced Polymer Composites in Civil Infrastructure,” Journal of Composites for Construction, ASCE, V. 7, No. 3, pp. 238-247. doi: 10.1061/(ASCE)1090-0268(2003)7:3(238)

Khalifa, A.; Gold, W. J.; Nanni, A.; and Abdel Aziz, M. I., 1998, “Contribution of Externally Bonded FRP to Shear Capacity of RC Flexural Members,” Journal of Composites for Construction, ASCE, V. 2, No. 4, pp. 195-202. doi: 10.1061/(ASCE)1090-0268(1998)2:4(195)

Khalifa, A., and Nanni, A., 2000, “Improving Shear Capacity of Existing RC T-Section Beams Using CFRP Composites,” Cement and Concrete Composites, V. 22, No. 3, pp. 165-174. doi: 10.1016/S0958-9465(99)00051-7

Kim, Y. J.; Kang, J. Y.; Park, J. S.; and Jung, W. T., 2016, “Functional Performance of Bridge Girders Strengthened with Post-Tensioned Near-Surface-Mounted Carbon Fiber-Reinforced Polymer,” ACI Structural Journal, V. 113, No. 2, Mar.-Apr., pp. 239-250. doi: 10.14359/51687801

Lu, X. Z.; Chen, J. F.; Ye, L. P.; Teng, J. G.; and Rotter, J. M., 2009, “RC Beams Shear-Strengthened with FRP: Stress Distributions in the FRP Reinforcement,” Construction and Building Materials, V. 23, No. 4, pp. 1544-1554. doi: 10.1016/j.conbuildmat.2008.09.019

Mofidi, A., and Chaallal, O., 2011, “Shear Strengthening of RC Beams with Externally Bonded FRP Composites: Effect of Strip-Width-to-Strip-Spacing Ratio,” Journal of Composites for Construction, ASCE, V. 15, No. 5, pp. 732-742. doi: 10.1061/(ASCE)CC.1943-5614.0000219

Moshirabadi, S., and Soltani, M., 2019, “Implementation of Smeared Crack Approach in Rigid Block and Spring Modeling of Reinforced Concrete,” Engineering Structures, V. 201, p. 109779. doi: 10.1016/j.engstruct.2019.109779

Nowak, A. S., and Collins, K. R., 2012, Reliability of Structures, CRC Press, London, UK, 407 pp.

Okeil, A. M.; El-Tawil, S.; and Shahawy, M., 2002, “Flexural Reliability of Reinforced Concrete Bridge Girders Strengthened with Carbon Fiber-Reinforced Polymer Laminates,” Journal of Bridge Engineering, ASCE, V. 7, No. 5, pp. 290-299. doi: 10.1061/(ASCE)1084-0702(2002)7:5(290)

Rasheed, H. A., 2015, Strengthening Design of Reinforced Concrete with FRP, CRC Press, New York, NY, 226 pp.

Ray, I.; Parish, G. C.; Davalos, J. F.; and Chen, A., 2010, “Effect of Concrete Substrate Repair Methods for Beams Aged by Accelerated Corrosion and Strengthened with CFRP,” Journal of Aerospace Engineering, ASCE, V. 24, No. 2, pp. 227-239. doi: 10.1061/(ASCE)AS.1943-5525.0000030

Rousakis, T. C.; Saridaki, M. E.; Mavrothalassitou, S. A.; and Hui, D., 2016, “Utilization of Hybrid Approach Towards Advanced Database of Concrete Beams Strengthened in Shear with FRPs,” Composites. Part B, Engineering, V. 85, pp. 315-335. doi: 10.1016/j.compositesb.2015.09.031

Spinella, N., 2019, “Modeling of Shear Behavior of Reinforced Concrete Beams Strengthened with FRP,” Composite Structures, V. 215, pp. 351-364. doi: 10.1016/j.compstruct.2019.02.073

Stewart, M. G., 1996, “Serviceability Reliability Analysis of Reinforced Concrete Structures,” Journal of Structural Engineering, ASCE, V. 122, No. 7, pp. 794-803. doi: 10.1061/(ASCE)0733-9445(1996)122:7(794)

Stewart, M. G., 2009, “Mechanical Behavior of Pitting Corrosion of Flexural and Shear Reinforcement and Its Effect on Structural Reliability of Corroding RC Beams,” Structural Safety, V. 31, No. 1, pp. 19-30. doi: 10.1016/j.strusafe.2007.12.001

Taki, A.; Firouzi, A.; and Mohammadzadeh, S., 2018, “Life Cycle Reliability Assessment of Reinforced Concrete Beams Shear‐Strengthened with Carbon Fiber Reinforced Polymer Strips in Accordance with fib Bulletin 14,” Structural Concrete, V. 19, No. 6, pp. 2017-2028. doi: 10.1002/suco.201700289

Teng, J. G., and Chen, J. F., 2009, “Mechanics of Debonding in FRP-Plated RC Beams,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 162, No. 5, pp. 335-345. doi: 10.1680/stbu.2009.162.5.335

Teng, J. G.; Lam, L.; and Chen, J. F., 2004, “Shear Strengthening of RC Beams with FRP Composites,” Progress in Structural Engineering and Materials, V. 6, No. 3, pp. 173-184. doi: 10.1002/pse.179

Triantafillou, T. C., 1998, “Shear Strengthening of Reinforced Concrete Beams Using Epoxy-Bonded FRP Composites,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr., pp. 107-115.

Triantafillou, T. C., and Antonopoulos, C. P., 2000, “Design of Concrete Flexural Members Strengthened in Shear with FRP,” Journal of Composites for Construction, ASCE, V. 4, No. 4, pp. 198-205. doi: 10.1061/(ASCE)1090-0268(2000)4:4(198)

Val, D. V., and Trapper, P. A., 2008, “Probabilistic Evaluation of Initiation Time of Chloride-Induced Corrosion,” Reliability Engineering & System Safety, V. 93, No. 3, pp. 364-372. doi: 10.1016/j.ress.2006.12.010

Wieghaus, K.T. and Atadero, R.A., 2010, “Effect of Existing Structure and FRP Uncertainties on the Reliability of FRP-Based Repair,” Journal of Composites for Construction, ASCE, V. 15, No. 4, pp. 635-643.

Yang, D. Y.; Frangopol, D. M.; and Teng, J. G., 2019, “Probabilistic Life-Cycle Optimization of Durability-Enhancing Maintenance Actions: Application to FRP Strengthening Planning,” Engineering Structures, V. 188, pp. 340-349. doi: 10.1016/j.engstruct.2019.02.055


ALSO AVAILABLE IN:

Electronic Structural Journal