Influence of Curing Methods on Moisture Loss and Drying Shrinkage of Shotcrete at Early Age

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Curing Methods on Moisture Loss and Drying Shrinkage of Shotcrete at Early Age

Author(s): Bruce Menu, Thomas Jacob-Vaillancourt, Marc Jolin, and Benoit Bissonnette

Publication: Materials Journal

Volume: 117

Issue: 4

Appears on pages(s): 95-103

Keywords: cracking; curing; drying; evaporation; moisture loss; shotcrete; shrinkage; surface protection

DOI: 10.14359/51724624

Date: 7/1/2020

Abstract:
The experimental program reported in this paper sought to evaluate the efficiency of a range of curing methods in view of minimizing the evaporation rate at the surface of freshly placed shotcrete and preventing the detrimental consequences of early-age shrinkage. CSA A23.1-14 states that severe drying conditions should be considered to exist when the surface moisture evaporation rate exceeds 0.50 kg/m2/h (0.1 lb/ft2/h). In fact, the environmental conditions that lead to such evaporation rates are regularly experienced on construction sites, requiring that adequate protection of the concrete surface be carried out in a timely manner after placement. This research effort is aimed at quantifying the influence of selected curing methods upon the early-age moisture loss and the resulting shrinkage. The results show that early-age volume change of freshly sprayed shotcrete can be significantly reduced by adequate surface protection. Among the investigated methods, moist curing is found to be the most effective.

Related References:

1. Mishra, R.; Tripathi, R.; and Dubey, V., “Early Age Shrinkage Pattern of Concrete on Replacement of Fine Aggregate with Industrial By-Product,” Journal of Radiation Research and Applied Sciences, V. 9, No. 4, 2016, pp. 386-391. doi: 10.1016/j.jrras.2016.05.003

2. Holt, E. E., “Early Age Autogenous Shrinkage of Concrete,” VTT Publications 446, Technical Research Centre of Finland, Espoo, Finland, 2001, 197 pp.

3. Bissonnette, B.; Pierre, P.; and Pigeon, M., “Influence of Key Parameters on Drying Shrinkage of Cementitious Materials,” Cement and Concrete Research, V. 29, No. 10, 1999, pp. 1655-1662. doi: 10.1016/S0008-8846(99)00156-8

4. Soroka, I., Concrete in Hot Environments, CRC Press, Boca Raton, FL, 2003.

5. Austin, S. A., and Robins, P. J., Sprayed Concrete: Properties, Design and Application, Whittles Publishing, Caithness, UK, 1995, 393 pp.

6. Ansell, A., “Investigation of Shrinkage Cracking in Shotcrete on Tunnel Drains,” Tunnelling and Underground Space Technology, V. 25, No. 5, 2010, pp. 607-613. doi: 10.1016/j.tust.2010.04.006

7. Jolin, M.; Beaupré, D.; and Mindess, S., “Tests to Characterise Properties of Fresh Dry-Mix Shotcrete,” Cement and Concrete Research, V. 29, No. 5, 1999, pp. 753-760. doi: 10.1016/S0008-8846(99)00071-X

8. Al-Gahtani, A., “Effect of Curing Methods on the Properties of Plain and Blended Cement Concretes,” Construction and Building Materials, V. 24, No. 3, 2010, pp. 308-314. doi: 10.1016/j.conbuildmat.2009.08.036

9. Sant, G.; Bentz, D.; and Weiss, J., “Capillary Porosity Depercolation in Cement-based Materials: Measurement Techniques and Factors which Influence their Interpretation,” Cement and Concrete Research, V. 41, No. 8, 2011, pp. 854-864. doi: 10.1016/j.cemconres.2011.04.006

10. Austin, S.; Robins, P.; and Issaad, A., “Influence of Curing Methods on the Strength and Permeability of GGBFS Concrete in a Simulated Arid Climate,” Cement and Concrete Composites, V. 14, No. 3, 1992, pp. 157-167. doi: 10.1016/0958-9465(92)90009-K

11. Studebaker, C. H., “Report on Gunite at Arrowrock Dam,” U.S. Bureau of Reclamation Memorandum, V. 10, Mar. 10, 1939, 66 pp.

12. ACI Committeee 506, “Guide to Shotcrete (ACI 506R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 52 pp.

13. Kreijger, P., “The Skin of Concrete Composition and Properties,” Materiales de Construcción, V. 17, No. 4, 1984, pp. 275-283. doi: 10.1007/BF02479083

14. Nassif, H.; Suksawang, N.; and Mohammed, M., “Effect of Curing Methods on Early-age and Drying Shrinkage of High-performance Concrete,” Transportation Research Record: Journal of the Transportation Research Board, V. 1834, No. 1, 2003, pp. 48-58. doi: 10.3141/1834-07

15. Morgan, D. R.; McAskill, N.; Neill, J.; and Duke, N. F., “Evaluation of Silica Fume Shotcrete,” Proceedings of CANMET/ACI Workshop on Condensed Silica Fume in Concrete, Montreal, QC, Canada, 1987.

16. Kosmatka, S. H.; Kerkhoff, B.; Hooton, D.; and McGrath, J. R., Design and Control of Concrete Mixtures, eighth Canadian edition, Cement Association of Canada, Ottawa, ON, Canada, 2011.

17. El Hindy, E.; Miao, B.; Chaallal, O.; and Aitcin, P.-C., “Drying Shrinkage of Ready-Mixed High-Performance Concrete,” ACI Materials Journal, V. 91, No. 3, May-June 1994, pp. 300-305.

18. Neville, A. M., Properties of Concrete, fifth edition, Pearson, Harlow, UK, 2011, 436 pp.

19. ASTM C1581/C1581M-09, “Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage,” ASTM International, West Conshohocken, PA, 2009, 7 pp.