Robustness of Ultra-High-Performance Concrete to Changes in Material Temperature

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Robustness of Ultra-High-Performance Concrete to Changes in Material Temperature

Author(s): Mahdi Valipour and Kamal H. Khayat

Publication: Materials Journal

Volume: 117

Issue: 4

Appears on pages(s): 47-56

Keywords: autogenous shrinkage; drying shrinkage; rheological properties; robustness; ultra-high-performance concrete

DOI: 10.14359/51724613

Date: 7/1/2020

Abstract:
Ultra-high-performance concrete (UHPC) can be vulnerable to variations in materials properties and environmental conditions. In this paper, the sensitivity of UHPC to changes in mixing, casting, curing, and testing temperatures ranging between 10 and 30 ± 2°C (50 and 86 ± 3.5°F) was investigated. The investigated rheological properties, mechanical properties, and shrinkage of UHPC are shown to be significantly affected by temperature changes. UHPC made with either binary or ternary binder containing fly ash (FA) or slag cement exhibited greater robustness than mixtures prepared with 25% silica fume. UHPC made with 60% FA necessitated the lowest high-range water-reducing admixture demand. With temperature increase, the yield stress of UHPC mixtures increased by up to 55%, and plastic viscosity decreased by up to 45%. This resulted in accelerating initial and final setting times by up to 4.5 and 5 hours, respectively. The increase of temperature from 10 to 30 ± 2°C (50 ± to 86 ± 3.5°F) led to a 10 to 75% increase in compressive, splitting tensile, and flexural strengths and modulus of elasticity and 15 to 60% increase in autogenous shrinkage.

Related References:

1. Billberg, P., and Khayat, K. H., “Use of Viscosity-Modifying Admixtures to Enhance Robustness,” Proceedings of the Third North American Conference on the Design and Use of Self-Consolidating Concrete, Chicago, IL, 2008.

2. Roy, D. M., and Asaga, K., “Rheological Properties of Cement Mixes: III. the Effects of Mixing Procedures on Viscometric Properties of Mixes Containing Superplasticizers,” Cement and Concrete Research, V. 9, No. 6, 1979, pp. 731-739. doi: 10.1016/0008-8846(79)90068-1

3. Sakata, N.; Marruyama, K.; and Minami, M., “Basic Properties and Effects of Welan Gum on Self-Consolidating Concrete,” RILEM PRO 32, Production Methods and Workability of Concrete, P. J. M. Bartos, D. L. Marrs, and D. J. Cleland, eds., 1996, pp. 237-253.

4. Banfill, P., “An Experimental Study of the Effect of Pfa on the Rheology of Fresh Concrete and Cement Paste,” Proceedings of the International Symposium on the Use of pfa in Concrete, J.G. Cabrera and A. R. Cusens, eds., University of Leeds, Leeds, UK, 1982, pp. 161-171.

5. Bonen, D.; Deshpande, Y.; Olek, J.; Shen, L.; Struble, L.; Lange, D.; and Khayat, K. H., “Robustness of Self-Consolidating Concrete,” RILEM PRO 54 Proceedings of the Fifth International RILEM Symposium on Self-Compacting Concrete, 2007, pp. 33-42.

6. Gettu, R.; Nawaz Shareef, S.; and Ernest, K., “Evaluation of the Robustness of SCC,” Indian Concrete Journal, V. 83, No. 6, 2009, pp. 13-19.

7. Yurugi, M.; Sakai, G.; and Sakata, N., “Viscosity Agent and Mineral Admixtures for Highly Fluidized Concrete,” Proceedings of Concrete under Severe Conditions, Environmental and Loading, K. Sakai, N. Banthia, and O. E. Gjørv, eds., Japan, 1995, pp. 995-1004.

8. Khayat, K. H., “Use of Viscosity-Enhancing Admixtures for Cement-Based Materials—An Overview,” Cement and Concrete Composites, V. 20, No. 2-3, 1998, pp. 171-188. doi: 10.1016/S0958-9465(98)80006-1

9. Billberg, P., and Khayat, K. H., “Use of Viscosity-Modifying Admixtures to Enhance Robustness of SCC,” SCC 2008, 3rd North American Conference on the Design and Use of Self-Consolidating Concrete, Chicago, IL, Nov. 2008, pp. 566-571.

10. Gálvez-Moreno, D.; Durán-Herrera, A.; González-López, J. R.; and Khayat, K. H., “Robustness of Powder-Type SCC with Fly Ash and Limestone Crushed Aggregates,” Proceedings SCC 2016, Supplementary Volume, K. H. Khayat, ed., May 2016, pp. 107-119.

11. Naji, S.; Hwang, S.; and Khayat, K. H., “Robustness of Self-Consolidating Concrete Incorporating Different Viscosity-Enhancing Admixtures,” ACI Materials Journal, V. 108, No. 4, July-Aug. 2011, pp. 432-438.

12. Meng, W.; Valipour, M.; and Khayat, K. H., “Optimization and Performance of Cost-Effective Ultra-High-Performance Concrete,” Materials and Structures, V. 50, No. 1, 2017, p. 29 doi: 10.1617/s11527-016-0896-3

13. Neville, A., Properties of Concrete, fourth edition, Pearson Education Limited, England, 1999.

14. Mouret, M., Bascoul, A., and Escadeillas, G., “Drops in Concrete Strength in Summer Related to the Aggregate Temperature,” Cement and Concrete Research, V. 27, No., 3, 1997, pp. 345-357.

15. Soudki, K.; El-Salakawy, E.; and Elkum, N., “Full Factorial Optimization of Concrete Mix Design for Hot Climates,” Journal of Materials in Civil Engineering, ASCE, V. 13, No. 6, 2001, pp. 427-433. doi: 10.1061/(ASCE)0899-1561(2001)13:6(427)

16. Ortiz, J.; Aguado, A.; Agulló, L.; and García, T., “Influence of Environmental Temperatures on the Concrete Compressive Strength: Simulation of Hot and Cold Weather Conditions,” Cement and Concrete Research, V. 35, No. 10, 2005, pp. 1970-1979. doi: 10.1016/j.cemconres.2005.01.004

17. Nassif, A., and Petrou, M., “Influence of Cold Weather during Casting and Curing on the Stiffness and Strength of Concrete,” Construction and Building Materials, V. 44, 2013, pp. 161-167. doi: 10.1016/j.conbuildmat.2013.03.016

18. Verbeck, G. J., and Helmuth, R. A., “Structures and Physical Properties of Cement Pastes,” Proceedings of the Fifth International Symposium on the Chemistry of Cement, V. III, The Cement Association of Japan, Tokyo, Japan, 1968, p. 9.

19. Flatt, R., and Houst, Y., “A Simplified View on Chemical Effects Perturbing the Action of Superplasticizers,” Cement and Concrete Research, V. 31, No. 8, 2001, pp. 1169-1176. doi: 10.1016/S0008-8846(01)00534-8

20. Yoshioka, K.; Tazawa, E.; Kawai, K.; and Enohata, T., “Adsorption Characteristics of Superplasticizers on Cement Component Minerals,” Cement and Concrete Research, V. 32, No. 10, 2002, pp. 1507-1513. doi: 10.1016/S0008-8846(02)00782-2

21. Randl, N.; Steiner, T.; Ofner, S.; Baumgartner, E.; and Mészöly, T., “Development of UHPC Mixtures from an Ecological Point of View,” Construction and Building Materials, V. 67, 2014, pp. 373-378. doi: 10.1016/j.conbuildmat.2013.12.102

22. Schmidt, W., “Design Concepts for the Robustness Improvement of Self-Compacting Concrete: Effects of Admixtures and Mixture Components on the Rheology and Early Hydration at Varying Temperatures,” Eindhoven: Technische Universiteit Eindhoven, 2014, doi: 10.6100/IR771936.10.6100/IR771936

23. Plank, J., and Hirsch, C., “Impact of Zeta Potential of Early Cement Hydration Phases on Superplasticizer Adsorption,” Cement and Concrete Research, V. 37, No. 4, 2007, pp. 537-542. doi: 10.1016/j.cemconres.2007.01.007

24. Ferraris, C. F.; Obla, K. H.; and Hill, R., “The Influence of Mineral Admixtures on the Rheology of Cement Paste and Concrete,” Cement and Concrete Research, V. 31, No. 2, 2001, pp. 245-255. doi: 10.1016/S0008-8846(00)00454-3

25. Kim, J. H.; Noemi, N.; and Shah, S. P., “Effect of Powder Materials on the Rheology and Formwork Pressure of Self-Consolidating Concrete,” Cement and Concrete Composites, V. 34, No. 6, 2012, pp. 746-753. doi: 10.1016/j.cemconcomp.2012.02.016

26. Yamada, K., “Basics of Analytical Methods Used for the Investigation of Interaction Mechanism between Cements and Superplasticizers,” Cement and Concrete Research, V. 41, No. 7, 2011, pp. 793-798. doi: 10.1016/j.cemconres.2011.03.007

27. Yijin, L.; Shiqiong, Z.; Jian, Y.; and Yingli, G., “The Effect of Fly Ash on the Fluidity of Cement Paste, Mortar, and Concrete,” Proceedings of the International Workshop on Sustainable Development and Concrete Technology, Beijing, China, 2004, pp. 339-345.

28. Alshamsi, A. M.; Sabouni, A. R.; and Bushlaibi, A. H., “Influence of Set-Retarding Superplasticisers and Microsilica on Setting Times of Pastes at Various Temperatures,” Cement and Concrete Research, V. 23, No. 3, 1993, pp. 592-598. doi: 10.1016/0008-8846(93)90009-X

29. Yamada, K.; Ogawa, S.; and Hanehara, S., “Controlling of the Adsorption and Dispersing Force of Polycarboxylate-Type Superplasticizer by Sulfate Ion Concentration in Aqueous Phase,” Cement and Concrete Research, V. 31, No. 3, 2001, pp. 375-383. doi: 10.1016/S0008-8846(00)00503-2

30. Soliman, A., and Nehdi, M., “Effect of Drying Conditions on Autogenous Shrinkage in Ultra-High-Performance Concrete at Early-Age,” Materials and Structures, V. 44, No. 5, 2011, pp. 879-899. doi: 10.1617/s11527-010-9670-0

31. Yajun, J., and Cahyadi, J., “Effects of Densified Silica Fume on Microstructure and Compressive Strength of Blended Cement Pastes,” Cement and Concrete Research, V. 33, No. 10, 2003, pp. 1543-1548. doi: 10.1016/S0008-8846(03)00100-5

32. Diamond, S., and Sahu, S., “Densified Silica Fume: Particle Sizes and Dispersion in Concrete,” Materials and Structures, V. 39, No. 9, 2006, pp. 849-859. doi: 10.1617/s11527-006-9087-y

33. Güneyisi, E.; Gesoğlu, M.; and Özbay, E., “Strength and Drying Shrinkage Properties of Self-Compacting Concretes Incorporating Multi-System Blended Mineral Admixtures,” Construction and Building Materials, V. 24, No. 10, 2010, pp. 1878-1887. doi: 10.1016/j.conbuildmat.2010.04.015

34. Loukili, A.; Khelidj, A.; and Richard, P., “Hydration Kinetics, Change of Relative Humidity, and Autogenous Shrinkage of Ultra-High-Strength Concrete,” Cement and Concrete Research, V. 29, No. 4, 1999, pp. 577-584. doi: 10.1016/S0008-8846(99)00022-8

35. Jensen, O., and Hansen, P., “Influence of Temperature on Autogenous Deformation and Relative Humidity Change in Hardening Cement Paste,” Cement and Concrete Research, V. 29, No. 4, 1999, pp. 567-575.

36. Yang, Y.; Sato, R.; and Kawai, K., “Autogenous Shrinkage of High-Strength Concrete Containing Silica Fume under Drying at Early Ages,” Cement and Concrete Research, V. 35, No. 3, 2005, pp. 449-456.

37. Baroghel-Bouny, V.; Mounanga, P.; Khelidj, A.; Loukili, A.; and Rafai, N., “Autogenous Deformations of Cement Pastes: Part II. W/C Effects, Micro-Macro Correlations, and Threshold Values,” Cement and Concrete Research, V. 36, No. 1, 2006, pp. 123-136. doi: 10.1016/j.cemconres.2004.10.020

38. Zhang, M.; Tam, C.; and Leow, M., “Effect of Water-to-Cementitious Materials Ratio and Silica Fume on the Autogenous Shrinkage of Concrete,” Cement and Concrete Research, V. 33, No. 10, 2003, pp. 1687-1694. doi: 10.1016/S0008-8846(03)00149-2

39. Li, J., and Yao, Y., “A Study on Creep and Drying Shrinkage of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 8, 2001, pp. 1203-1206. doi: 10.1016/S0008-8846(01)00539-7

40. Lura, P.; Van Breugel, K.; and Maruyama, I., “Effects of Curing Temperature and Type of Cement on Early Age Shrinkage of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 12, 2001, pp. 1867-1872. doi: 10.1016/S0008-8846(01)00601-9

41. Yang, Y.; Li, M.; Deng, H.; and Liu, Q., “Effects of Temperature on Drying Shrinkage of Concrete,” Applied Mechanics and Materials, V. 584-586, 2014, pp. 1176-1181. doi: 10.4028/www.scientific.net/AMM.584-586.1176


ALSO AVAILABLE IN: