Relationship of Rheology, Fiber Dispersion, and Strengths of Polyvinyl Alcohol Fiber-Reinforced Cementitious Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Relationship of Rheology, Fiber Dispersion, and Strengths of Polyvinyl Alcohol Fiber-Reinforced Cementitious Composites

Author(s): Mingli Cao, Wen Si, and Chaopeng Xie

Publication: Materials Journal

Volume: 117

Issue: 3

Appears on pages(s): 191-204

Keywords: fiber dispersion; fiber factor; flexural strength; orientation coefficient; rheological performance

DOI: 10.14359/51724598

Date: 5/1/2020

Abstract:
Polyvinyl alcohol (PVA) fiber with high elastic modulus and toughness can act as a reinforcing material to improve the brittleness of cement-based materials. However, the difficulty of fiber dispersion in the matrix is correspondingly increased due to its bending and clustering. Poor fiber dispersion not only deteriorates the mechanical properties of PVA fiber-reinforced cementitious composites (PVA-FRCCs) but also increases the difficulty in determining the relationship between fiber dispersion and hardening properties. Rheology, as a vital method to supervise the mixture properties, can improve the fiber distribution and optimize the hardening performance. This paper investigated rheological performance, fiber dispersion, and strengths of three types of PVA-FRCCs and discussed the effect of different fiber factors on the materials properties. Results showed that the rheology of a mixture can affect fiber dispersion and uniform fiber dispersion can be achieved through the experimental design of PVA-FRCCs. Besides, the quantitative relationship between fiber distribution parameters and flexural strengths of PVA-FRCCs was proposed, which showed a superior reliability than the composites theory formula and other traditional fitting equations. However, the relationship between fiber dispersion and compressive strengths was hardly founded due to the deterioration in compressive strength caused by the addition of PVA fibers.

Related References:

1. Bentur, A., and Mindess, S., Fiber Reinforced Cementitious Composites, CRC Press, Boca Raton, FL, 2006.

2. Li, V. C., and Leung, C. K. Y., “Steady-State and Multiple Cracking of Short Random Fiber Composites,” Journal of Engineering Mechanics, V. 118, No. 11, 1992, pp. 2246-2264. doi: 10.1061/(ASCE)0733-9399(1992)118:11(2246)

3. Li, H.; Xu, S.; and Leung, C. K. Y., “Tensile and Flexural Properties of Ultra-High Toughness Cementitious Composite,” Journal of Wuhan University of Technology-Mater. Sci. Ed, V. 24, No. 4, 2009, pp. 677-683. doi: 10.1007/s11595-009-4677-5

4. Horikoshi, T.; Ogawa, A.; Saito, T.; and Hoshiro, H., “Properties of Polyvinylalcohol Fiber as Reinforcing Materials for Cementitious Composites,” International RILEM Workshop on HPFRCC in Structural Applications, Paris, France, 2006.

5. Kim, J.; Robertson, R. E.; and Naaman, A. E., “Structure and Properties of Poly(Vinyl Alcohol)-Modified Mortar and Concrete,” Cement and Concrete Research, V. 29, No. 3, 1999, pp. 407-415. doi: 10.1016/S0008-8846(98)00246-4

6. Zhang, J.; Wang, Q.; and Wang, Z., “Properties of Polyvinyl Alcohol-Steel Hybrid Fiber-Reinforced Composite with High-Strength Cement Matrix,” Journal of Materials in Civil Engineering, V. 29, No. 7, 2017, p. 04017026 doi: 10.1061/(ASCE)MT.1943-5533.0001868

7. Kawamata, A.; Mihashi, H.; and Fukuyama, H., “Properties of Hybrid Fiber Reinforced Cement-Based Composites,” Journal of Advanced Concrete Technology, V. 1, No. 3, 2003, pp. 283-290. doi: 10.3151/jact.1.283

8. Liu, J., and Tan, K. H., “Fire Resistance of Strain Hardening Cementitious Composite with Hybrid PVA and Steel Fibers,” Construction & Building Materials, V. 135, 2017, pp. 600-611. doi: 10.1016/j.conbuildmat.2016.12.204

9. Yun, H., “Effect of Accelerated Freeze-Thaw Cycling on Mechanical Properties of Hybrid PVA and PE Fiber-Reinforced Strain-Hardening Cement-Based Composites (SHCCs),” Composites. Part B, Engineering, V. 52, 2013, pp. 11-20. doi: 10.1016/j.compositesb.2013.03.021

10. Shuxin, W., and Li, V. C., “Polyvinyl Alcohol Fiber Reinforced Engineered Cementitious Composites: Material Design and Performances,” Proceedings of International RILEM Workshop on HPFRCC in Structural Applications, Honolulu, HI, 2005.

11. Wang, J.; Dai, Q.; Si, R.; and Guo, S., “Investigation of Properties and Performances of Polyvinyl Alcohol (PVA) Fiber-Reinforced Rubber Concrete,” Construction & Building Materials, V. 193, 2018, pp. 631-642. doi: 10.1016/j.conbuildmat.2018.11.002

12. Noushini, A.; Vessalas, K.; and Samali, B., “Static Mechanical Properties of Polyvinyl Alcohol Fibre Reinforced Concrete (PVA-FRC),” Magazine of Concrete Research, V. 66, No. 9, 2014, pp. 465-483. doi: 10.1680/macr.13.00320

13. Jang, J. G.; Kim, H. K.; Kim, T. S.; Min, B. J.; and Lee, H. K., “Improved Flexural Fatigue Resistance of PVA Fiber-Reinforced Concrete Subjected to Freezing and Thawing Cycles,” Construction & Building Materials, V. 59, 2014, pp. 129-135. doi: 10.1016/j.conbuildmat.2014.02.040

14. Wittmann, F., and Van Zijl, G., “Durability of Strain-Hardening Fibre-Reinforced Cement-Based Composites (SHCC),” RILEM State of the Art Reports, Springer, 2011.

15. Şahmaran, M.; Özbay, E.; Yücel, H. E.; Lachemi, M.; and Li, V. C., “Frost Resistance and Microstructure of Engineered Cementitious Composites: Influence of Fly Ash and Micro Poly-Vinyl-Alcohol Fiber,” Cement and Concrete Composites, V. 34, No. 2, 2012, pp. 156-165. doi: 10.1016/j.cemconcomp.2011.10.002

16. Yang, E., and Li, V. C., “Tailoring Engineered Cementitious Composites for Impact Resistance,” Cement and Concrete Research, V. 42, No. 8, 2012, pp. 1066-1071. doi: 10.1016/j.cemconres.2012.04.006

17. Li, M., and Li, V. C., “Rheology, Fiber Dispersion, and Robust Properties of Engineered Cementitious Composites,” Materials and Structures, V. 46, No. 3, 2013, pp. 405-420. doi: 10.1617/s11527-012-9909-z

18. Tosun-Felekoğlu, K.; Felekoğlu, B.; Ranade, R.; Lee, B. Y.; and Li, V. C., “The Role of Flaw Size and Fiber Distribution on Tensile Ductility of PVA-ECC,” Composites. Part B, Engineering, V. 56, 2014, pp. 536-545. doi: 10.1016/j.compositesb.2013.08.089

19. Zhou, J.; Qian, S.; Ye, G.; Copuroglu, O.; van Breugel, K.; and Li, V. C., “Improved Fiber Distribution and Mechanical Properties of Engineered Cementitious Composites by Adjusting the Mixing Sequence,” Cement and Concrete Composites, V. 34, No. 3, 2012, pp. 342-348. doi: 10.1016/j.cemconcomp.2011.11.019

20. França, M. S. D.; Cardoso, F. A.; and Pileggi, R. G., “Influence of the Addition Sequence of PVA-Fibers and Water on Mixing and Rheological Behavior of Mortars,” Revista IBRACON de Estruturas e Materiais, V. 9, No. 2, 2016, pp. 226-243. doi: 10.1590/S1983-41952016000200005

21. Woo, L. Y.; Wansom, S.; Ozyurt, N.; Mu, B.; Shah, S. P.; and Mason, T. O., “Characterizing Fiber Dispersion in Cement Composites using AC-Impedance Spectroscopy,” Cement and Concrete Composites, V. 27, No. 6, 2005, pp. 627-636. doi: 10.1016/j.cemconcomp.2004.06.003

22. Liu, J.; Li, C.; Liu, J.; Cui, G.; and Yang, Z., “Study on 3D Spatial Distribution of Steel Fibers in Fiber Reinforced Cementitious Composites Through Micro-CT Technique,” Construction & Building Materials, V. 48, 2013, pp. 656-661. doi: 10.1016/j.conbuildmat.2013.07.052

23. Felekoğlu, B.; Tosun-Felekoğlu, K.; and Gödek, E., “A Novel Method for the Determination of Polymeric Micro-Fiber Distribution of Cementitious Composites Exhibiting Multiple Cracking Behavior under Tensile Loading,” Construction & Building Materials, V. 86, 2015, pp. 85-94. doi: 10.1016/j.conbuildmat.2015.03.094

24. Torigoe, S.; Horikoshi, T.; Ogawa, A.; Saito, T.; and Hamada, T., “Study on Evaluation Method for PVA Fiber Distribution in Engineered Cementitious Composite,” Journal of Advanced Concrete Technology, V. 1, No. 3, 2003, pp. 265-268. doi: 10.3151/jact.1.265

25. Lee, B. Y.; Kim, T.; and Kim, Y. Y., “Fluorescence Characteristic Analysis for Discriminating Fibers in Cementitious Composites,” Journal of Advanced Concrete Technology, V. 8, No. 3, 2010, pp. 337-344. doi: 10.3151/jact.8.337

26. Kobayashi, K., Fiber Reinforced Concrete, Ohm-Sha, Tokyo, Japan, 1981.

27. Xia, M.; Hamada, H.; and Maekawa, Z., “Flexural Stiffness of Injection Molded Glass Fiber Reinforced Thermoplastics,” International Polymer Processing, V. 10, No. 1, 1995, pp. 74-81. doi: 10.3139/217.950074

28. Kang, S., and Kim, J., “The Relation between Fiber Orientation and Tensile Behavior in an Ultra-High-Performance Fiber Reinforced Cementitious Composite (UHPFRCC),” Cement and Concrete Research, V. 41, No. 10, 2011, pp. 1001-1014. doi: 10.1016/j.cemconres.2011.05.009

29. Kang, S. T.; Lee, B. Y.; Kim, J.-K.; and Kim, Y. Y., “The Effect of Fibre Distribution Characteristics on the Flexural Strength of Steel Fibre-Reinforced Ultra-High Strength Concrete,” Construction & Building Materials, V. 25, No. 5, 2011, pp. 2450-2457. doi: 10.1016/j.conbuildmat.2010.11.057

30. Liu, J.; Zhang, L.; Li, C.; and Liu, J., “Dispersive Characterization and Control of Fiber in Polyvinyl Alcohol Fiber Cement Composites,” Journal of the Chinese Ceramic Society, V. 43, No. 8, 2015, pp. 1061-1066.

31. Banfill, P. F. G.; Starrs, G.; Derruau, G.; McCarter, W. J.; and Chrisp, T. M., “Rheology of Low Carbon Fibre Content Reinforced Cement Mortar,” Cement and Concrete Composites, V. 28, No. 9, 2006, pp. 773-780. doi: 10.1016/j.cemconcomp.2006.06.004

32. ACI Committee 544, “Report on Measuring Mechanical Properties of Hardened Fiber-Reinforced Concrete (ACI 544.9R-17),” American Concrete Institute, Farmington Hills, MI, 2017.

33. Lee, B. Y.; Kim, J.; Kim, J.; and Kim, Y. Y., “Quantitative Evaluation Technique of Polyvinyl Alcohol (PVA) Fiber Dispersion in Engineered Cementitious Composites,” Cement and Concrete Composites, V. 31, No. 6, 2009, pp. 408-417. doi: 10.1016/j.cemconcomp.2009.04.002

34. Cao, M.; Xu, L.; and Zhang, C., “Rheological and Mechanical Properties of Hybrid Fiber Reinforced Cement Mortar,” Construction & Building Materials, V. 171, 2018, pp. 736-742. doi: 10.1016/j.conbuildmat.2017.09.054

35. Bentz, D. P.; Ferraris, C. F.; Galler, M. A.; Hansen, A. S.; and Guynn, J., “Influence of Particle Size Distributions on Yield Stress and Viscosity of Cement-Fly Ash Pastes,” Cement and Concrete Research, V. 42, No. 2, 2012, pp. 404-409. doi: 10.1016/j.cemconres.2011.11.006

36. Barnes, H. A., A Handbook of Elementary Rheology, Institute of Non-Newtonian Fluid Mechanics, University of Wales, Aberystwyth, UK, 2000.

37. Çavdar, A., “A Study on the Effects of High Temperature on Mechanical Properties of Fiber Reinforced Cementitious Composites,” Composites. Part B, Engineering, V. 43, No. 5, 2012, pp. 2452-2463. doi: 10.1016/j.compositesb.2011.10.005

38. Singh, N. B., and Rai, S., “Effect of Polyvinyl Alcohol on the Hydration of Cement with Rice Husk Ash,” Cement and Concrete Research, V. 31, No. 2, 2001, pp. 239-243. doi: 10.1016/S0008-8846(00)00475-0

39. Mehdipour, I.; Libre, N. A.; Shekarchi, M.; and Khanjani, M., “Effect of Workability Characteristics on the Hardened Performance of FRSCCMs,” Construction & Building Materials, V. 40, 2013, pp. 611-621. doi: 10.1016/j.conbuildmat.2012.11.051

40. Banfill, P., “The Rheology of Fresh Cement and Concrete—A Review,” Proceedings of the 11th International Congress on the Chemistry of Cement, Durban, South Africa, 2003.

41. Pan, Z.; Wu, C.; Liu, J.; Wang, W.; and Liu, J., “Study on Mechanical Properties of Cost-Effective Polyvinyl Alcohol Engineered Cementitious Composites (PVA-ECC),” Construction & Building Materials, V. 78, 2015, pp. 397-404. doi: 10.1016/j.conbuildmat.2014.12.071


ALSO AVAILABLE IN:

Electronic Materials Journal