Behavior of Steel Fiber-Reinforced Concrete under Biaxial Stresses

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Steel Fiber-Reinforced Concrete under Biaxial Stresses

Author(s): S. M. Chiew, I. S. Ibrahim, N. Jamaluddin, N. N. Sarbini, C. K. Ma, and Y. Ahmad

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 267-277

Keywords: biaxial tension; fiber volumetric fraction; steel fiber-reinforced concrete (SFRC); stress ratio; tension-compression

DOI: 10.14359/51723545

Date: 7/1/2020

Abstract:
Biaxial behavior of various types of concrete is essential to be considered in construction design because construction structures normally experience multiaxial stresses rather than uniaxial stress. Research on biaxial behavior of steel fiber-reinforced concrete (SFRC) has been conducted in the past decades. Most of the research, however, is only limited to biaxial compression, whereas information regarding biaxial tension and biaxial tension-compression on SFRC is relatively scarce. This study presents a simple biaxial experimental setup to investigate the biaxial behavior of SFRC with 0.5, 1.0, and 1.5% steel fiber under biaxial tension and biaxial tension-compression. It is found that the smaller stress ratio enhanced the deformability and tensile capacity of SFRC under biaxial tension-compression, whereas the effect of stress ratio on biaxial tensile behavior of SFRC is negligible. The addition of steel fiber eventually enhanced the concrete strength by 15 to 41% under tension-compression compared with plain concrete.

Related References:

1. Nazarimofrad, E.; Shaikh, F. U. A.; and Nili, M., “Effects of Steel Fibre and Silica Fume on Impact Behaviour of Recycled Aggregate Concrete,” Journal of Sustainable Cement-Based Materials, V. 6, No. 1, 2017, pp. 54-68. doi: 10.1080/21650373.2016.1230900

2. Lim, D.-H., and Nawy, E., “Behaviour of Plain and Steel-Fibre-Reinforced High-Strength Concrete under Uniaxial and Biaxial Compression,” Magazine of Concrete Research, V. 57, No. 10, 2005, pp. 603-610. doi: 10.1680/macr.2005.57.10.603

3. Kolle, B., “Behaviour of Steel Fibre Reinforced High Performance Concrete under Biaxial Loading Conditions,” PhD dissertation, University of Glasgow, Glasgow, UK, 2006.

4. Foltz, R. R.; Lee, D. H.; and LaFave, J. M., “Biaxial Behavior of High-Performance Fiber-Reinforced Cementitious Composite Plates,” Construction and Building Materials, V. 143, 2017, pp. 501-514. doi: 10.1016/j.conbuildmat.2017.03.167

5. Hu, X. D.; Day, R.; and Dux, P., “Biaxial Failure Model for Fiber Reinforced Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 6, 2003, pp. 609-615. doi: 10.1061/(ASCE)0899-1561(2003)15:6(609)

6. Seow, P. E. C., and Swaddiwudhipong, S., “Failure Surface for Concrete under Multiaxial Load—A Unified Approach,” Journal of Materials in Civil Engineering, ASCE, V. 17, No. 2, 2005, pp. 219-228. doi: 10.1061/(ASCE)0899-1561(2005)17:2(219)

7. Sirijaroonchai, K.; El-Tawil, S.; and Parra-Montesinos, G., “Behavior of High Performance Fiber Reinforced Cement Composites under Multi-Axial Compressive Loading,” Cement and Concrete Composites, V. 32, No. 1, 2010, pp. 62-72. doi: 10.1016/j.cemconcomp.2009.09.003

8. Kupfer, H.; Hilsdorf, H. K.; and Rusch, H., “Behavior of Concrete under Biaxial Stresses,” ACI Journal Proceedings, V. 66, No. 8, Aug. 1969, pp. 656-666.

9. Lee, S.-K.; Song, Y.-C.; and Han, S.-H., “Biaxial Behavior of Plain Concrete of Nuclear Containment Building,” Nuclear Engineering and Design, V. 227, No. 2, 2004, pp. 143-153. doi: 10.1016/j.nucengdes.2003.09.001

10. Shang, H.-S.; Yang, S.-T.; and Niu, X.-Y., “Mechanical Behavior of Different Types of Concrete under Multiaxial Tension–Compression,” Construction and Building Materials, V. 73, 2014, pp. 764-770. doi: 10.1016/j.conbuildmat.2014.09.035

11. Yin, W.; Su, E. C.; Mansur, M.; and Hsu, T. T., “Fiber-Reinforced Concrete under Biaxial Compression,” Engineering Fracture Mechanics, V. 35, No. 1-3, 1990, pp. 261-268. doi: 10.1016/0013-7944(90)90204-T

12. Murugappan, K.; Paramasivam, P.; and Tan, K., “Failure Envelope for Steel-Fiber Concrete under Biaxial Compression,” Journal of Materials in Civil Engineering, ASCE, V. 5, No. 4, 1993, pp. 436-446. doi: 10.1061/(ASCE)0899-1561(1993)5:4(436)

13. Abdull-Ahad, R., and Abbas, J., “Behaviour of Steel Fibre Reinforced Concrete under Biaxial Stresses,” Fibre Reinforced Cements and Concretes: Recent Developments, Elsevier Science Publishers, Essex, UK, 1989.

14. Lemnitzer, L.; Eckfeldt, L.; Lindorf, A.; and Curbach, M., “Biaxial Tensile Strength of Concrete—Answers From Statistics,” Tailor Made Concrete Structures: New Solutions for Our Society—Proceedings of the International fib Symposium, CRC Press, Boca Raton, FL, 2008.

15. Hussein, A., and Marzouk, H., “Behavior of High-Strength Concrete under Biaxial Stresses,” ACI Materials Journal, V. 97, No. 1, Jan.-Feb. 2000, pp. 27-36.

16. Ren, X.; Yang, W.; Zhou, Y.; and Li, J., “Behavior of High-Performance Concrete under Uniaxial and Biaxial Loading,” ACI Materials Journal, V. 105, No. 6, Nov.-Dec. 2008, pp. 548-558.

17. Mohamed, R.; Zamri, N.; Elliott, K.; Rahman, A.; and Bakhary, N., “Steel Fibre Self-Compacting Concrete under Biaxial Loading,” Construction and Building Materials, V. 224, 2019, pp. 255-265. doi: 10.1016/j.conbuildmat.2019.07.076

18. Bao, J.; Wang, L.; Zhang, Q.; Liang, Y.; Jiang, P.; and Song, Y., “Combined Effects of Steel Fiber and Strain Rate on the Biaxial Compressive Behavior of Concrete,” Construction and Building Materials, V. 187, 2018, pp. 394-405. doi: 10.1016/j.conbuildmat.2018.07.203

19. Torrenti, J., and Djebri, B., “Behaviour of Steel-Fibre-Reinforced Concretes under Biaxial Compression Loads,” Cement and Concrete Composites, V. 17, No. 4, 1995, pp. 261-266. doi: 10.1016/0958-9465(95)00027-A

20. Teychenné, D. C.; Franklin, R. E.; Erntroy, H. C.; and Marsh, B., Design of Normal Concrete Mixes, HM Stationery Office, London, UK, 1975.

21. BS 1881-125, “Testing Concrete. Methods for Mixing and Sampling Fresh Concrete in the Laboratory,” British Standards Institute, London, UK, 2013.

22. Ding, Y., and Kusterle, W., “Compressive Stress–Strain Relationship of Steel Fibre-Reinforced Concrete at Early Age,” Cement and Concrete Research, V. 30, No. 10, 2000, pp. 1573-1579. doi: 10.1016/S0008-8846(00)00348-3

23. Thomas, J., and Ramaswamy, A., “Mechanical Properties of Steel Fiber-Reinforced Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 5, 2007, pp. 385-392. doi: 10.1061/(ASCE)0899-1561(2007)19:5(385)

24. Calixto, J. M. F., “Microcracking of High Performance Concrete Subjected to Biaxial Tension-Compression Stresses,” Materials Research, V. 5, No. 3, 2002, pp. 295-299. doi: 10.1590/S1516-14392002000300013

25. Cho, J.-Y.; Kim, N.-S.; Cho, N.-S.; and Choun, Y.-S., “Stress-Strain Relationship of Reinforced Concrete Subjected to Biaxial Tension,” ACI Structural Journal, V. 101, No. 2, Mar.-Apr. 2004, pp. 202-208.

26. Hampel, T.; Speck, K.; Scheerer, S.; Ritter, R.; and Curbach, M., “High-Performance Concrete under Biaxial and Triaxial Loads,” Journal of Engineering Mechanics, ASCE, V. 135, No. 11, 2009, pp. 1274-1280. doi: 10.1061/(ASCE)0733-9399(2009)135:11(1274)

27. Lee, J.-H.; Hong, S.-G.; Joh, C.; Kwahk, I.; and Lee, J.-W., “Biaxial Tension–Compression Strength Behaviour of UHPFRC In-Plane Elements,” Materials and Structures, V. 50, No. 1, 2017, p. 20. doi: 10.1617/s11527-016-0918-1

28. Traina, L. A., and Mansour, S. A., “Biaxial Strength and Deformational Behavior of Plain and Steel Fiber Concrete,” ACI Materials Journal, V. 88, No. 4, July-Aug. 1991, pp. 353-362.

29. Demeke, A., and Tegos, I., “Steel Fiber-Reinforced Concrete in Biaxial Stress Tension-Compression Conditions,” ACI Structural Journal, V. 91, No. 5, Sept.-Oct. 1994, pp. 579-584.

30. Swaddiwudhipong, S., and Seow, P. E. C., “Modelling of Steel Fiber-Reinforced Concrete under Multi-Axial Loads,” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1354-1361. doi: 10.1016/j.cemconres.2006.03.008


ALSO AVAILABLE IN:

Electronic Structural Journal