Deflection at Incipient Failure as Warning-of-Failure Metric

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Deflection at Incipient Failure as Warning-of-Failure Metric

Author(s): Marcie van Weerdhuizen and F. Michael Bartlett

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 233-241

Keywords: existing structure assessment; flexural ductility; plastic hinge length; reinforced concrete; reinforcement ratio; reliability index; structural safety; Warning Factor

DOI: 10.14359/51723544

Date: 7/1/2020

Abstract:
The target reliability index for the assessment of an existing flexural element depends on the warning of failure provided and therefore on the total deflection at incipient failure. Sensitivity analyses accounting for both the linear-elastic-cracked and plastic responses indicate that the warning of failure depends on the ductility of critical cross sections (and therefore on the flexural reinforcement ratio) and the length of the plastic hinge regions (and therefore on the applied load configuration). Structural redundancy typically reduces the total deflection at incipient member failure and therefore is an inconsistent indicator of warning of failure. The deflections at incipient failure can be normalized as fractions of the span length to quantify the Warning Factor, W, as a function of the reinforcement ratio, span length, and effective beam depth. This continuous variable can replace existing discretized values of the Warning Factor based on somewhat subjective classifications of ductility and redundancy.

Related References:

1. ACI Committee 562, “Code Requirements for Assessment, Repair, and Rehabilitation of Existing Concrete Structures (ACI 562-19) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2019, 94 pp.

2. National Research Council of Canada, “Structural Commentaries (User’s Guide – NBC 2015: Part 4 of Division B),” National Research Council of Canada, Ottawa, ON, Canada, 2015, 219 pp.

3. ASCE/SEI 7-16, “Minimum Design Loads For Buildings and Other Structures,” American Society of Civil Engineers, Reston, VA, 2017, 800 pp.

4. CSA S6-14, “Canadian Highway Bridge Design Code,” Canadian Standards Association, Mississauga, ON, Canada, 2014, 894 pp.

5. CAN/CSA S408-11, “Guideline for the Development of Limit States Design Standards,” Canadian Standards Association, Mississauga, ON, Canada, 2011, 62 pp.

6. CAN/CSA S408-81, “Guideline for the Development of Limit States Design,” Canadian Standards Association, Rexdale, ON, Canada, 1981, 34 pp.

7. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

8. Lequesne, R. D., and Pincheira, J. A., “Proposed Revisions to the Strength-Reduction Factor for Axially Loaded Members,” Concrete International, V. 36, No. 9, Sept. 2014, pp. 43-49.

9. Gamble, W. L., “Phi-Factors Revisited,” Concrete International, V. 37, No. 12, Dec. 2015, pp. 35-38.

10. Asantey, S. B. A., and Bartlett, F. M., “Impact of Posted Load Limits on Highway Bridge Reliability,” Journal of Bridge Engineering, ASCE, V. 10, No. 3, 2005, pp. 321-330. doi: 10.1061/(ASCE)1084-0702(2005)10:3(321)

11. Wight, J. K., Reinforced Concrete: Mechanics and Design, seventh edition, Pearson Education, Inc., Hoboken, NJ, 2016, 1144 pp.

12. Cohn, M. Z., Analysis and Design of Inelastic Structures, Volume 2: Problems, University of Waterloo Press, Waterloo, ON, Canada, 1972, 521 pp.

13. CSA A23.3-19, “Design of Concrete Structures,” Canadian Standards Association, Mississauga, ON, Canada, 2019, 290 pp.

14. Bentz, E., and Collins, M. P., “Response-2000 Shell-2000 Triax-2000 Membrane-2000 User Manual,” University of Toronto, Toronto, ON, Canada, 2001, 85 pp.

15. Cohn, M. Z., and Ghosh, S. K., “Flexural Ductility of Reinforced Concrete Sections,” Publications, International Association for Bridge and Structural Engineering, Zurich, V. 32-II, 1972, pp. 53-83.

16. Leet, K. M.; Uang, C.-M.; and Gilbert, A. M., Fundamentals of Structural Analysis, fourth edition, McGraw-Hill Ltd., New York, NY, 2011, 768 pp.

17. van Weerduizen, M., “Aversion and Warning Factors for Assessing Existing Reinforced Concrete Structures,” Electronic Thesis and Dissertation Repository, 5135, Western University, London, ON, Canada, 2018, 107 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal