Load-Transfer Design of Wall-Piloti Structure with Lateral Support

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load-Transfer Design of Wall-Piloti Structure with Lateral Support

Author(s): Sung-Hyun Kim, Hong-Gun Park, and Hyeon-Jong Hwang

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 169-180

Keywords: bearing wall; capacity design; cyclic loading; pilotis; strut-and-tie model

DOI: 10.14359/51723543

Date: 7/1/2020

Abstract:
In Korea, bearing-wall structures with pilotis have been frequently used for high-rise residential buildings. In the present study, an economical load-transfer design and the reinforcing bar details were studied for bearing walls with pilotis, which are laterally supported by other vertically continuous walls. Four specimens were tested under gravity loads and cyclic lateral loading. To avoid a brittle failure of the interface between the wall and pilotis, a capacity design was applied to the design of the test specimens. The test results showed that ductile flexural yielding of the upper wall occurred without premature brittle failure of the transfer wall, columns, and the critical interface section. To confirm the test strength, a strut-and-tie model was applied to the test specimens. The strength and damage mode predicted by the strut-and-tie model agreed with the test result. Based on the test results and the strut-and-tie model used for the test specimens, a strut-and-tie model was proposed for the actual design of the prototype wall, and the relevant reinforcing bar details were proposed. The safety of the design was confirmed by nonlinear finite element analysis.

Related References:

1. Lee, H. S., “A Review of Design Practice for the Hybrid Structures with Upper Shear-Wall and Lower-Frame Systems,” Proceedings of Spring Conference, Korea Concrete Institute, Seoul, South Korea, 1999.

2. Architectural Institute of Korea, “Korean Building Code and Commentary,” second edition, Kimoondang, Seoul, Korea, 2012.

3. British Standards Institution, “Eurocode 8: Design of Structures for Earthquake Resistance,” Part 1, London, UK, 2005.

4. Yoshimura, M., “Nonlinear Analysis of a Reinforced Concrete Building with a Soft First Story Collapsed by the 1995 Hyogoken-Nanbu Earthquake,” Cement and Concrete Composites, V. 19, No. 3, 1997, pp. 213-221. doi: 10.1016/S0958-9465(97)00016-4

5. Suff, R.; Chandler, A.; and Li, J., “Seismic Assessment of Transfer Plate High Rise Buildings,” Structural Engineering and Mechanics, V. 14, No. 3, 2002, pp. 287-306. doi: 10.12989/sem.2002.14.3.287

6. Ramdane, K. E.; Kusunoki, K.; Teshigawara, M.; and Kato, H., “Non-Linear Numerical Analyses to Improve the Seismic Design Method for Soft First Story RC Building,” 13th World Conference on Earthquake Engineering, Vancouver, BC, Canada. 2004.

7. Lee, H. S., and Ko, D. W., “Seismic Response of High-Rise RC Bearing-Wall Structures with Irregularities at Bottom Stories,” Proceedings of the 13th World Conference on Earthquake Engineering, Vancouver, BC, Canada, 2004.

8. Li, C. S.; Lam, S. S.; Zhang, M. Z.; and Wong, Y. L., “Shaking Table Test of a 1: 20 Scale High-Rise Building With a Transfer Plate System,” Journal of Structural Engineering, ASCE, V. 132, No. 11, 2006, pp. 1732-1744. doi: 10.1061/(ASCE)0733-9445(2006)132:11(1732)

9. Li, C. S.; Lam, S. S.; Chen, A.; and Wong, Y. L., “Seismic Performance of a Transfer Plate Structure,” Journal of Structural Engineering, ASCE, V. 134, No. 11, 2008, pp. 1705-1716. doi: 10.1061/(ASCE)0733-9445(2008)134:11(1705)

10. Chang, Y.; Chen, W.; and Sui, J., “Seismic Design of RC Frame-Shear Structure Using Viscoelastic Dampers,” Journal of Southeast University, Natural Science Edition, V. 32, No. 5, 2002, pp. 733-736.

11. Zhang, Q.; Liu, W. G.; He, W. F.; and Liu, Y., “Seismic Design and Analysis of Tall Shear Wall-Frame Structure Using Viscous Damping Wall,” Applied Mechanics and Materials, V. 275-277, 2013.

12. Mezzi, M., “Enhancing the Seismic Performance of Existing ‘Pilotis’ Configurations,” IABSE Symposium Report, International Association for Bridge and Structural Engineering, Zurich, Switzerland, 2006.

13. Mezzi, M., and Parducci, A., “Preservation of Existing Soft-First-Story Configurations by Improving the Seismic Performance,” 3rd Specialty Conference on the Conceptual Approach to Structural Design, 2005.

14. Hawkins, N. M., and Ghosh, S., “Acceptance Criteria for Special Precast Concrete Structural Walls Based on Validation Testing,” PCI Journal, V. 49, No. 5, 2004, pp. 78-92. doi: 10.15554/pcij.09012004.78.92

15. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

16. Paulay, T.; Priestley, M J. N.; and Synge, A. J., “Ductility in Earthquake Resisting Squat Shearwalls,” ACI Journal Proceedings, V. 79, No. 4, Apr. 1982, pp. 257-269.

17. Kim, S.-H.; Hwang, H.-J.; and Park, H.-G., “Shear Force Amplification Effect Addressing Nonlinear Dynamic Response in Slender RC Walls,” Journal of the Korea Concrete Institute, V. 30, No. 2, 2018, pp. 135-146. doi: 10.4334/JKCI.2018.30.2.135


ALSO AVAILABLE IN:

Electronic Structural Journal