ACI 318.2-19 Building Code Requirements for Concrete Thin Shells and Commentary

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI 318.2-19 Building Code Requirements for Concrete Thin Shells and Commentary

Author(s): ACI Committee 318

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: folded plates; inelastic analysis; ribbed shells; thin shells

DOI:

Date: 5/1/2019

Abstract:
This document governs the design of thin shell concrete structures. Where required for design of thin shell concrete structures, provisions of ACI 318 are to be used to complement the provisions of this Code.