Static Experimental Behavior of Peripheral Composite Slab-Beam Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Static Experimental Behavior of Peripheral Composite Slab-Beam Joints

Author(s): Yongzhi Gong, Yingjie Shan, Ping Xiang, Wei Huang, and Faxing Ding

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 255-265

Keywords: beam-slab joint; mechanical property; peripheral composite slabs; thickness of slab; transverse superposed surface

DOI: 10.14359/51723525

Date: 7/1/2020

Abstract:
To improve the assembly rate of composite slabs, an innovative assembled peripheral composite slab is proposed in this paper. The static experimental behavior of beam-slab joints of this novel prefabricated assembly structure are investigated and compared with those of cast-in-place beam-slab joints. In this respect, five assembled composite beam-slab joints and one monolithic beam-slab joint were tested to study the effects of the laminated surface type and the slab thickness on the mechanical properties of these joints, and the steel strain and load-deflection curve of the beam-slab joint were tested. It is observed that the mechanical properties of the non-ribbed composite slab are consistent with that of the cast-in-place slab. The transverse superposed surface has adverse effects on the flexural performance of composite slabs, and the location of this surface is one of the main factors that affect the ultimate bearing capacity of beam-slab joints. It is also found that the thickness of slabs has a great influence on the cracking load, ultimate bearing capacity, and the ductility coefficient of beam-slab joints. The folded steel bar reserved in the rib groove and the napping treatment of the composite surface can ensure the overall working performance of the joint. Setting ribs on precast slabs are helpful to improve the ductility coefficient of specimens, and this advantage is more obvious in specimens with small thickness.

Related References:

1. Siddh, S. P.; Patil, Y. D.; and Patil, H. S., “Experimental Studies on Behaviour of Composite Slab with Profiled Steel Sheeting,” Materials Today: Proceedings, V. 4, No. 9, 2017, pp. 9792-9796. doi: 10.1016/j.matpr.2017.06.268

2. Cho, C. G.; Kappos, A. J.; Moon, H. J.; and Lim, H. J., “Experiments and Failure Analysis of SHCC and Reinforced Concrete Composite Slabs,” Engineering Failure Analysis, V. 56, Oct. 2015, pp. 320-331. doi: 10.1016/j.engfailanal.2015.01.009

3. Ranzi, G.; Al-Deen, S.; Hollingum, G.; Hone, T.; Gowripalan, S.; and Uy, B., “An Experimental Study on the Ultimate Behaviour of Simply-Supported Post-Tensioned Composite Slabs,” Journal of Constructional Steel Research, V. 89, Oct. 2013, pp. 293-306. doi: 10.1016/j.jcsr.2013.07.013

4. Gholamhoseini, A.; Khanlou, A.; MacRae, G.; Scott, A.; Hicks, S.; and Leon, R., “An Experimental Study on Strength and Serviceability of Reinforced and Steel Fibre Reinforced Concrete (SFRC) Continuous Composite Slabs,” Engineering Structures, V. 114, May 2016, pp. 171-180. doi: 10.1016/j.engstruct.2016.02.010

5. Lasheen, M.; Shaat, A.; and Khalil, A., “Behaviour of Lightweight Concrete Slabs Acting Compositely with Steel I-Sections,” Construction and Building Materials, V. 124, Oct. 2016, pp. 967-981. doi: 10.1016/j.conbuildmat.2016.08.007

6. Wieneke, K., and Hegger, J., “Fatigue of Semi-Precast Slabs with Lattice Girders,” High Tech Concrete: Where Technology and Engineering Meet, V. 112, No. 9, 2018, pp. 921-928. doi: 10.1007/978-3-319-59471-2_107

7. Yang, Y.; Chen, Y.; Yang, Y.; and Zeng, S., “Investigation on the Mechanical Performance of Flat Steel Plate-Lightweight Aggregate Concrete Hollow Composite Slab,” Steel and Composite Structures, V. 31, No. 4, 2019, pp. 329-340.

8. Hossain, K. M. A.; Attarde, S.; and Anwar, M. S., “Finite Element Modeling of Profiled Steel Deck Composite Slab System with Engineered Cementitious Composite Under Monotonic Loading,” Engineering Structures, V. 186, May 2019, pp. 13-25. doi: 10.1016/j.engstruct.2019.02.008

9. Lee, C. H.; Mansouri, I.; Kim, E.; Hwang, K. S.; and Woo, W.-T., “Flexural Strength of One-Way Composite Steel Deck Slabs Voided by Circular Paper Tubes,” Journal of Structural Engineering, ASCE, V. 145, No. 2, 2019, p. 04018246 doi: 10.1061/(ASCE)ST.1943-541X.0002259

10. Ryu, J.; Kim, Y. Y.; Park, M. W.; Yoon, S. W.; Lee, C. H.; and Ju, Y. K., “Experimental and Numerical Investigations of Steel-Polymer Hybrid Floor Panels Subjected to Three-Point Bending,” Engineering Structures, V. 175, No. 15, 2018, pp. 467-500. doi: 10.1016/j.engstruct.2018.08.030

11. Henin, E.; Morcous, G.; and Tadros, M. K., “Shallow Flat Soffit Precast Concrete Floor System,” Practice Periodical on Structural Design and Construction, ASCE, V. 18, No. 2, 2013, pp. 101-110. doi: 10.1061/(ASCE)SC.1943-5576.0000135

12. Lam, S. S. E.; Wong, V.; and Lee, R. S. M., “Bonding Assessment of Semi-Precast Slabs Subjected to Flexural Load and Differential Shrinkage,” Engineering Structures, V. 187, Feb. 2019, pp. 25-33. doi: 10.1016/j.engstruct.2019.02.029

13. Zheng, H. Y.; Jiang, H. Y.; Wu, Y. Q.; Zhao, Z. Q.; Zeng, Y. C.; and Cheng, X. H., “Experimental Study on Flexural Performance of Prefabricated RC Slabs with Different Rebar Forms at Seam,” Advanced Materials Research, V. 1065-1069, Dec. 2014, pp. 1187-1190. doi: 10.4028/www.scientific.net/AMR.1065-1069.1187

14. Amadio, C.; Bedon, C.; and Fasan, M., “Numerical Assessment of Slab-Interaction Effects on the Behaviour of Steel-Concrete Composite Joints,” Journal of Constructional Steel Research, V. 139, Dec. 2017, pp. 397-410. doi: 10.1016/j.jcsr.2017.10.003

15. Ibrahim, I. S.; Elliott, K. S.; Abdullah, R.; Kueh, A. B. H.; and Sarbini, N. N., “Experimental Study on the Shear Behavior of Precast Concrete Hollow Core Slabs with Concrete Topping,” Engineering Structures, V. 125, Oct. 2016, pp. 80-90. doi: 10.1016/j.engstruct.2016.06.005

16. Keipour, N.; Valipour, H. R.; and Bradford, M. A., “Steel-Timber Composite Beam-to-Column Joints: Effect of Connections Between Timber Slabs,” Journal of Constructional Steel Research, V. 151, Dec. 2018, pp. 132-145. doi: 10.1016/j.jcsr.2018.09.019

17. Wang, Y. H.; Yu, J.; Liu, J. P.; and Chen, Y. F., “Experimental Study on Assembled Monolithic Steel-Concrete Composite Beam in Positive Moment,” Engineering Structures, V. 180, Feb. 2019, pp. 494-509. doi: 10.1016/j.engstruct.2018.11.034

18. Liu, X. P.; Bradford, M. A.; and Ataei, A., “Flexural Performance of Innovative Sustainable Composite Steel-Concrete Beams,” Engineering Structures, V. 130, Jan. 2017, pp. 282-296. doi: 10.1016/j.engstruct.2016.10.009

19. Corney, S. R.; Ingham, J. M.; and Henry, R. S., “Seismic Testing of Support Connections in Deep Hollow-Core Floor Units,” ACI Structural Journal, V. 115, No. 3, May 2018, pp. 735-748. doi: 10.14359/51702062

20. Kwon, K. Y.; Foreman, J. M. Jr.; Azimov, U. U.; Klingner, R. E.; Bayrak, O.; and Jirsa, J. O., “Control of Cracking in Precast, Prestressed Concrete Panels for Bridge Decks,” ACI Structural Journal, V. 111, No. 6, Nov.-Dec. 2014, pp. 1461-1467. doi: 10.14359/51687164

21. Wang, J.; Wang, W.; Lehman, D.; and Roeder, C., “Effects of Different Steel-Concrete Composite Slabs on Rigid Steel Beam-Column Connection Under a Column Removal Scenario,” Journal of Constructional Steel Research, V. 153, Feb. 2019, pp. 55-70. doi: 10.1016/j.jcsr.2018.09.025

22. Lee, C. H.; Jung, J. H.; Kim, S. Y.; and Kim, J. J., “Investigation of Composite Slab Effect on Seismic Performance of Steel Moment Connections,” Journal of Constructional Steel Research, V. 117, Feb. 2016, pp. 91-100. doi: 10.1016/j.jcsr.2015.10.004

23. Li, W., and Han, L. H., “Seismic Performance of CFST Column to Steel Beam Joint with RC Slab: Joint Model,” Journal of Constructional Steel Research, V. 73, June 2012, pp. 66-79. doi: 10.1016/j.jcsr.2012.01.011

24. Lew, H. S.; Bao, Y.; Pujol, S.; and Sozen, M. A., “Experimental Study of Reinforced Concrete Assemblies under Column Removal Scenario,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 861-892. doi: 10.14359/51686739

25. Wang, X.-Q.; Xu, L.-Y.; and Tao, M.-X., “Influence of Slab Spatial Composite Effect on Dynamic Behavior of Composite Frame Structures Under Earthquake Excitation,” Bulletin of Earthquake Engineering, V. 17, No. 6, 2019, pp. 3071-3094. doi: 10.1007/s10518-019-00568-6

26. Qian, K., and Li, B., “Slab Effects on Response of Reinforced Concrete Substructures after Loss of Corner Column,” ACI Structural Journal, V. 109, No. 6, Nov.-Dec. 2012, pp. 845-855.

27. Lee, J. K., and Lee, S. H., “Flexural Behavior of Ultra-High-­Performance Fiber-Reinforced Concrete Moment Connection for Precast Concrete Decks,” ACI Structural Journal, V. 112, No. 4, July-Aug. 2015, pp. 451-462. doi: 10.14359/51687657

28. Ministry of Housing and Urban-Rural Development of the People’s Republic of China, (GB/T 51231-2016), “Technical Standard for Assembled Buildings with Concrete Structure,” Building Industry Press, Beijing, China, 2017.

29. Ministry of Housing and Urban-Rural Development of the People’s Republic of China, (GB/T 50152-2012), “Standard for Test Method of Concrete Structures,” Building Industry Press, Beijing, China, 2012.

30. Wu, Y., and Wang, Y. L., “Bearing Capacity Test of Composite Floors and Analysis of Influencing Factors,” Low Temperature Architecture Technology, V. 10, 2013, pp. 37-39.

31. Supriyadi, B.; Siswosukarto, S.; and Effi, C. P. Y. P., “The Behavior Semi-Precast Slab Under Dynamic Load,” Procedia Engineering, V. 171, 2017, pp. 1204-1213. doi: 10.1016/j.proeng.2017.01.488

32. Zhu, W. Z.; Zhang, J. C.; Chen, Y.; Wang, K. Y.; Li, M.; and Li, H. Y., “Experimental Study on Beam-Plate Joints of New Prefabricate Assembly Structure,” Construction Technology, V. 44, No. 3, Feb. 2015, pp. 49-52.

33. Zhou, W. H., “Modern Concrete Composite Structure,” Construction Industry Press, Beijing, China, 1998, pp. 12-16.


ALSO AVAILABLE IN:

Electronic Structural Journal