Seismic Behavior of Hollow-Core Composite Bridge Columns Having Slender Inner Steel Tubes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Hollow-Core Composite Bridge Columns Having Slender Inner Steel Tubes

Author(s): Mohanad M. Abdulazeez and Mohamed A. ElGawady

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 143-158

Keywords: buckling instabilities; composite bridge column; hollow-core; reparability; seismic behavior; sustainability

DOI: 10.14359/51723521

Date: 7/1/2020

Abstract:
This paper experimentally investigates the seismic behavior of two as-built and one repaired large-scale hollow-core fiber-reinforced polymer-concrete-steel (HC-FCS) columns. Each HC-FCS column consisted of a concrete shell sandwiched between an outer glass fiber-reinforced polymer (GFRP) tube and an inner steel tube. Both tubes provided continuous confinement for the concrete shell along with the height of the column. The columns had two different steel tube diameter-to-thickness ratios (Ds/ts) of 85 and 254. Each steel tube was embedded into the footing, with an embedded length of 1.25 to 1.6 times its diameter, while the GFRP tube was not embedded into the footing. Two columns were tested as as-built specimens. Then, one of these columns was repaired and retested. This study revealed that HC-FCS columns having a high Ds/ts of 254 and short embedded length (1.25Ds) do not dissipate high levels of energy and display nonlinear elastic performance due to severe steel tube buckling and slippage. However, the column with a Ds/ts of 85 combined with substantial embedment length (1.6Ds) results in a nonlinear inelastic behavior, high energy dissipation, and ductile behavior. A repair technique for a high Ds/ts HC-FCS column precluding buckling of the inner steel tube was proposed and examined. The repair method was characterized by use of an anchorage system with steel tube concrete filling at the joint interface region. The repaired column achieved the ductile behavior and performed well under seismic loading with flexural strength increased by 22%. However, the lateral displacement capacity decreased by 26% compared to the virgin column due to the residual deformations and stresses exhibited during the previous test.

Related References:

1. Schrank, D.; Eisele, B.; and Lomax, T., “TTI’s 2012 Urban Mobility Report,” Texas A&M Transportation Institute, Texas A&M University, College Station, TX, 2012, 4 pp.

2. Schrank, D. L., and Lomax, T. J., “2009 Urban Mobility Report,” Texas Transportation Institute, Texas A&M University, College Station, TX, 2009.

3. Dawood, H.; Elgawady, M.; and Hewes, J.,“Factors Affecting the Seismic Behavior of Segmental Precast Bridge Columns,” Frontiers of Structural and Civil Engineering, V. 8, No. 4, 2014, pp. 388-398. doi: 10.1007/s11709-014-0264-8

4. Lin, M., and Tsai, K.-C., “Behavior of Double-Skinned Composite Steel Tubular Columns Subjected to Combined Axial and Flexural Loads,” Proceedings of the First International Conference on the Steel & Composite Structures, pp. 1145-1152. 2001

5. Tao, Z., and Han, L.-H.,“Behavior of Concrete-Filled Double Skin Rectangular Steel Tubular Beam–Columns,” Journal of Constructional Steel Research, V. 62, No. 7, 2006, pp. 631-646. doi: 10.1016/j.jcsr.2005.11.008

6. Wei, S.; Mau, S.; Vipulanandan, C.; and Mantrala, S.,“Performance of New Sandwich Tube under Axial Loading: Experiment,” Journal of Structural Engineering, ASCE, V. 121, No. 12, 1995, pp. 1806-1814. doi: 10.1061/(ASCE)0733-9445(1995)121:12(1806)

7. Zhao, X.-L.; Han, B.; and Grzebieta, R. H.,“Plastic Mechanism Analysis of Concrete-Filled Double-Skin (SHS inner and SHS outer) Stub Columns,” Thin-Walled Structures, V. 40, No. 10, 2002, pp. 815-833. doi: 10.1016/S0263-8231(02)00030-7

8. Anumolu, S.; Abdelkarim, O. I.; and ElGawady, M. A.,“Behavior of Hollow-Core Steel-Concrete-Steel Columns Subjected to Torsion Loading,” Journal of Bridge Engineering, ASCE, V. 21, No. 10, 2016, p. 04016070 doi: 10.1061/(ASCE)BE.1943-5592.0000923

9. Teng, J., and Lam, L., “Behavior and Modeling of Fiber Reinforced Polymer-Confined Concrete,” Journal of Structural Engineering, ASCE, V. 130, No. 11, 2004, pp. 1713-1723. doi: 10.1061/(ASCE)0733-9445(2004)130:11(1713)

10. Teng, J.; Yu, T.; Wong, Y.; and Dong, S.,“Hybrid FRP–Concrete–Steel Tubular Columns: Concept and Behavior,” Construction and Building Materials, V. 21, No. 4, 2007, pp. 846-854. doi: 10.1016/j.conbuildmat.2006.06.017

11. Wong, Y.; Yu, T.; Teng, J.; and Dong, S.,“Behavior of FRP-Confined Concrete in Annular Section Columns,” Composites. Part B, Engineering, V. 39, No. 3, 2008, pp. 451-466. doi: 10.1016/j.compositesb.2007.04.001

12. Abdulazeez, M. M.; Gheni, A.; Abdelkarim, O. I.; and ElGawady, M. A., “Column-Footing Connection Evaluation of Hollow-Core Composite Bridge Columns,” The 13th International Symposium on Fiber-Reinforced Polymer Reinforcement for Concrete Structures, SP-327, American Concrete Institute, Farmington Hills, MI, 2018, 14 pp.

13. Abdelkarim, O. I.; ElGawady, M. A.; Gheni, A.; Anumolu, S.; and Abdulazeez, M.,“Seismic Performance of Innovative Hollow-Core FRP–Concrete–Steel Bridge Columns,” Journal of Bridge Engineering, ASCE, V. 22, No. 2, 2017, p. 04016120 doi: 10.1061/(ASCE)BE.1943-5592.0000985

14. Yu, T.; Wong, Y.; and Teng, J.,“Technical Papers: Behavior of Hybrid FRP-Concrete-Steel Double-Skin Tubular Columns Subjected to Eccentric Compression,” Advances in Structural Engineering, V. 13, No. 5, 2010, pp. 961-974. doi: 10.1260/1369-4332.13.5.961

15. Issa, C. A., and Debs, P.,“Experimental Study of Epoxy Repairing of Cracks in Concrete,” Construction and Building Materials, V. 21, No. 1, 2007, pp. 157-163. doi: 10.1016/j.conbuildmat.2005.06.030

16. Karayannis, C. G., and Sirkelis, G. M.,“Strengthening and Rehabilitation of RC Beam–Column Joints Using Carbon‐FRP Jacketing and Epoxy Resin Injection,” Earthquake Engineering and Structural Dynamics, V. 37, No. 5, 2008, pp. 769-790. doi: 10.1002/eqe.785

17. Saini, A., and Saiidi, M. S., “Post-Earthquake Damage Repair of Various Reinforced Concrete Bridge Components,” Final Report No. CA 13-2180, California Department of Transportation, Sacramento, CA, 2013, 172 pp.

18. Fakharifar, M.; Chen, G.; Arezoumandi, M.; and ElGawady, M.,“Hybrid Jacketing for Rapid Repair of Seismically Damaged Reinforced Concrete Columns,” Transportation Research Record: Journal of the Transportation Research Board, V. 2522, No. 1, 2015, pp. 70-78. doi: 10.3141/2522-07

19. Abdulazeez, M. M.; Gheni, A.; Colbert, N.; and ElGawady, M. A., “Seismic Performance and Retrofit Evaluation of Hollow-Core Composite Bridge Columns,” Maintenance, Safety, Risk, Management and Life-Cycle Performance of Bridges, CRC Press, Boca Raton, FL, 2018, pp. 437-44.

20. Abdelkarim, O. I., and ElGawady, M. A.,“Analytical and Finite-Element Modeling of FRP-Concrete-Steel Double-Skin Tubular Columns,” Journal of Bridge Engineering, ASCE, V. 20, No. 8, 2015, p. B4014005 doi: 10.1061/(ASCE)BE.1943-5592.0000700

21. Yu, T.; Wong, Y.; Teng, J.; and Dong, S., “Structural Behavior of Hybrid FRP-Concrete-Steel Double-Skin Tubular Columns,” ANCER Annual Meeting, Honolulu, HI, 2004, 11 pp.

22. Abdelkarim, O. I.; ElGawady, M. A.; Anumolu, S.; Gheni, A.; and Sanders, G. E.,“Behavior of Hollow-Core FRP-Concrete-Steel Columns under Static Cyclic Flexural Loading,” Journal of Structural Engineering, ASCE, V. 144, No. 2, 2018, p. 04017188 doi: 10.1061/(ASCE)ST.1943-541X.0001905

23. Anumolu, S.; Abdelkarim, O. I.; Abdulazeez, M. M.; Gheni, A.; and ElGawady, M. A.,“Hollow-Core FRP–Concrete–Steel Bridge Columns under Torsional Loading,” Fibers (Basel, Switzerland), V. 5, No. 4, 2017, p. 44 doi: 10.3390/fib5040044

24. AWS D1.8/D1.8M:2009, “Structural Welding Code—Seismic Supplement,” American Welding Society, Miami, FL, 2009, 126 pp.

25. fib Bulletin No. 39, “Seismic Bridge Design and Retrofit—Structural Solutions,” Federation Internationale du Beton, Lausanne, Switzerland, 2007, 300 pp.

26. FEMA 461, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components," Federal Emergency Management Agency, Washington, DC, 2007, 113 pp.

27. Yu, T.; Wong, Y.; Teng, J.; Dong, S.; and Lam, E.,“Flexural Behavior of Hybrid FRP-Concrete-Steel Double-Skin Tubular Members,” Journal of Composites for Construction, ASCE, V. 10, No. 5, 2006, pp. 443-452. doi: 10.1061/(ASCE)1090-0268(2006)10:5(443)

28. Fakharifar, M.; Chen, G.; Wu, C.; Shamsabadi, A.; ElGawady, M. A.; and Dalvand, A.,“Rapid Repair of Earthquake-Damaged RC Columns with Prestressed Steel Jackets,” Journal of Bridge Engineering, V. 21, No. 4, ASCE, 2016, p. 04015075 doi: 10.1061/(ASCE)BE.1943-5592.0000840

29. Miranda, E., and Bertero, V. V.,“Evaluation of Strength Reduction Factors for Earthquake-Resistant Design,” Earthquake Spectra, V. 10, No. 2, 1994, pp. 357-379. doi: 10.1193/1.1585778

30. AASHTO, “AASHTO Guide Specifications for LRFD Seismic Bridge Design,” American Association of State Highway and Transportation Officials, Washington, DC, 2011.

31. Sullivan, T.; Calvi, G.; and Priestley, M., “Initial Stiffness Versus Secant Stiffness in Displacement-Based Design,” 13th World Conference of Earthquake Engineering (WCEE), No. 2888. 2004

32. Youssf, O.; ElGawady, M. A.; and Mills, J. E.,“Displacement and Plastic Hinge Length of FRP-Confined Circular Reinforced Concrete Columns,” Engineering Structures, V. 101, 2015, pp. 465-476. doi: 10.1016/j.engstruct.2015.07.026

33. Calvi, G.; Priestley, M.; and Kowalsky, M., “Displacement-Based Seismic Design of Structures,” New Zealand Conference on Earthquake Engineering, 2007, p. 740. IUSS press, 2007.

34. ElGawady, M.; Endeshaw, M.; McLean, D.; and Sack, R.,“Retrofitting of Rectangular Columns with Deficient Lap Splices,” Journal of Composites for Construction, ASCE, V. 14, No. 1, 2010, pp. 22-35. doi: 10.1061/(ASCE)CC.1943-5614.0000047

35. Gulkan, P., and Sozen, M. A.,“Inelastic Responses of Reinforced Concrete Structures to Earthquake Motions,” Reinforced Concrete Structures in Seismic Zones, SP-53, American Concrete Institute, Farmington Hills, MI, 1977, pp. 109-116.

36. Midorikawa, M.; Hiraishi, H.; Okawa, I.; Iiba, M.; Teshigawara, M.; and Isoda, H., “Development of Seismic Performance Evaluation Procedures in Building Code of Japan,” Proceedings of 12th World Conference of Earthquake Engineering, Auckland, New Zealand, Paper No. 2215, 2000.


ALSO AVAILABLE IN:

Electronic Structural Journal