Title: Grouted Extruded-Strand Tendons: Friction Coefficients and Differential Individual Strand Forces

Author(s): Hyeongyeop Shin, Thomas H.-K. Kang, and Jong-Hyok Park

Publication: Structural Journal

Volume: 117

Issue: 3

Appears on pages(s): 223-233

Keywords:

DOI: 10.14359/51723520

Date: 5/1/2020

Abstract:
Due to increasing demand and application of grouted extruded- strand tendons, need for analysis of tendon characteristics for design and construction exists. Measured for this paper were friction coefficients and strand tensile force distribution of horizontal circumferential tendons of a nuclear containment structure. Results indicated that grouted extruded-strand tendons had very low curvature and wobble friction coefficients (μ = 0.0277/rad and k = 0.0006/m [0.00018/ft]) in comparison to that observed for grease-filled bare-strand tendons. Furthermore, individual strand tensile forces in grouted extruded-strand tendons achieved lower standard deviation than that of bare-strand tendons.

Related References:

AASHTO, 2017, AASHTO LRFD Bridge Design Specification, eighth edition, American Association of State Highway and Transportation Officials, Washington, DC.

ACI Committee 318, 2008, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary,” American Concrete Institute, Farmington Hills, MI, 473 pp.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

CEN 2004, “Design of Concrete Structures (Eurocode 2),” European Committee for Standardization (CEN), Brussels, Belgium.

Cho, K.; Cho, J.-R.; Kim, S. T.; Park, S. Y.; Kim, Y.-J.; and Park, Y.-H., 2016, “Estimation of Prestress Force Distribution in Multi-Strand System of Prestressed Concrete Structures Using Field Data Measured by Electromagnetic Sensor,” Sensors (Basel), V. 16, No. 8, p. 1317 doi: 10.3390/s16081317

Cho, K.; Park, S. Y.; Cho, J.-R.; Kim, S. T.; and Park, Y.-H., 2015, “Estimation of Prestress Force Distribution in the Multi-Strand System of Prestressed Concrete Structures,” Sensors (Basel), V. 15, No. 6, pp. 14079-14092. doi: 10.3390/s150614079

Domage, J.-B.; Elias, S.; and Laurens, J.-M., 2010, “State of the Art Post-Tensioning for Nuclear Containments,” Proceedings of the 3rd fib International Congress, Washington, DC.

Domage, J.-B.; Ruffray, N.; and Elias, S., 2013, “Full Scale Post-Tensioning Mock-Up to Illustrate New Technologies for Nuclear Containments,” Proceedings of the Technical Innovation in Nuclear Civil Engineering (TINCE 2013), Paris, France.

EOTA, 2006a, “Post-Tensioning Kit for Prestressing of Structures (VSL Post-Tensioning System),” ETA-06/0006, European Organisation for Technical Approvals, Bagneux, France.

EOTA, 2006b, Post-Tensioning Kit for Prestressing of Structures (System Freyssinet), ETA-06/0226, European Organisation for Technical Approvals, Bagneux, France.

fib, 2013, “fib Model Code for Concrete Structures 2010,” International Federation for Structural Concrete (fib), Lausanne, Switzerland.

Jeon, S. J.; Park, J. C.; Park, I. K.; and Shim, B., 2009, “Estimation of Friction Coefficients Based on Field Data,” Journal of the Korean Society of Civil Engineers, V. 29. (in Korean)

Joint ACI-ASCE Committee 423, 2007, “Specification for Unbonded Single-Strand Tendon Materials and Commentary (ACI 423.7-07),” American Concrete Institute, Farmington Hills, MI, 21 pp.

Joint ACI-ASCE Committee 423, 2016, “Guide to Estimating Prestress Loss (ACI 423.10R-16),” American Concrete Institute, Farmington Hills, MI, 64 pp.

Joint ACI-ASME Committee 359, 2017, “ASME Boiler and Pressure Vessel Code, Section III. Rules for Construction of Nuclear Facility Components, Division 2. Code for Concrete Containments,” American Society of Mechanical Engineers, New York, NY.

Kang, T. H.-K., and Park, J.-H., 2016, “Full-Scale Mock-Up Tests of Nuclear Containment with HDPE-Coated Unbonded Tendons,” Presentation, Joint ACI Committee 349, Concrete Nuclear Structures, Working Group B, Nuclear Structures-Design, ACI Fall 2016 Convention, Philadelphia, PA.

Kang, T. H.-K., and Park, J.-H., 2017, “Mock-Up Tests of Unbonded Single Strand Tendons for CPTS,” Presentation, Joint ACI-ASME Committee 359, Concrete Containments for Nuclear Reactors, Working Group on Materials, Fabrication & Examination, ASME BPV Code Week, Phoenix, AZ.

KCI, 2017, “Structural Concrete Design Code,” Korea Concrete Institute, Seoul, Korea.

Kitani, T., and Shimizu, A., 2009, “Friction Coefficient Measurement Test on 13MN Class Tendon of PC Strands for Prestressed Concrete Containment Vessel (PCCV),” Proceedings of the 20th International Conference on Structural Mechanics in Reactor Technology (SMiRT 20), Paper 1825.

Moon, J. K., and Lee, J. H., 1997, “A Study on the Determination of Prestressing Force Considering Frictional Loss in PS Concrete Structures,” Journal of the Korean Society of Civil Engineers, V. 17, No. 1-1. (in Korean)

PCI, 2011, Bridge Design Manual, third edition, Precast/Prestressed Concrete Institute, Chicago, IL.

PTI TAB, 2006, Post-Tensioning Manual, sixth edition, Post-Tensioning Institute, Farmington Hills, MI.

PTI/ASBI 50, 2012, “Guide Specification for Grouted Post-Tensioning (PTI/ASBI M50.3-12),” Post-Tensioning Institute, Farmington Hills, MI.

Shin, H., 2018, “Effect of Individual Strand Force Deviation in Multi-Strand Post-Tensioning Tendon on Structural Behavior,” MS thesis, Seoul National University, Seoul, Korea.


ALSO AVAILABLE IN:

Electronic Structural Journal