Compression Behavior of Seawater and Sea-Sand Concrete Reinforced with Fiber and Glass Fiber-Reinforced Polymer Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compression Behavior of Seawater and Sea-Sand Concrete Reinforced with Fiber and Glass Fiber-Reinforced Polymer Bars

Author(s): Jikai Zhou, Xu He, and Wei Shen

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 103-114

Keywords: axial and eccentric compression; bearing capacity; crack width; glass fiber-reinforced polymer (GFRP) bars; polypropylene (PP) fibers; seawater and sea-sand concrete (SSC)

DOI: 10.14359/51723519

Date: 7/1/2020

Abstract:
To avoid the damage caused by chloride attack and improve the toughness of concrete, glass fiber-reinforced polymer (GFRP) bars and short fibers could be used in seawater and sea-sand concrete (SSC). In this paper, SSC columns reinforced with polypropylene (PP) fibers and GFRP bars under axial and eccentric compression were tested. The bearing capacity of axial and small eccentric compression column and the crack width of eccentric compression column were theoretically analyzed. The research result showed: for axial compression testing, the increase of longitudinal reinforcement ratio had little influence on the test results, and the contribution of GFRP bars to the ultimate bearing capacity for axial compression columns was small. For eccentric compression testing, eccentricity had a significant influence on the mechanical properties of the test columns, while the reinforcement ratio had little effect. In addition, PP fibers could restrain crack development in SSC effectively. The theoretical result of the crack width of eccentric compression columns and the ultimate bearing capacity of axial and small eccentric compression columns agreed well with the experimental data.

Related References:

1. Islam, M. M.; Islam, M. S.; Al-Amin, M.; and Islam, M. M., “Suitability of Sea Water on Curing and Compressive Strength of Structural Concrete,” Journal of Civil Engineering, V. 40, No. 1, 2012, pp. 37-45.

2. Wegian, F. M., “Effect of Seawater for Mixing and Curing on Structural Concrete,” Ies Journal Part A Civil & Structural Engineering, V. 3, No. 4, 2010, pp. 235-243. doi: 10.1080/19373260.2010.521048

3. Limeira, J.; Agullo, L.; and Etxeberria, M., “Dredged Marine Sand in Concrete: An Experimental Section of a Harbor Pavement,” Construction and Building Materials, V. 24, No. 6, 2010, pp. 863-870. doi: 10.1016/j.conbuildmat.2009.12.011

4. Limeira de Araujo, J.; Agulló Fité, L.; and Etxeberria Larrañaga, M., “Dredged Marine Sand as Constructive Material,” XIèmes Journées Nationales Génie Côtier – Génie Civil, Les Sables d'Olonne, France, 2010, pp. 877-886.

5. Issa, M. S.; Metwally, I. M.; and Elzeiny, S. M., “Influence of Fibers on Flexural Behavior and Ductility of Concrete Beams Reinforced with GFRP Rebars,” Engineering Structures, V. 33, No. 5, 2011, pp. 1754-1763. doi: 10.1016/j.engstruct.2011.02.014

6. Caggiano, A.; Cremona, M.; Faella, C.; Lima, C.; and Martinelli, E., “Fracture Behavior of Concrete Beams Reinforced with Mixed Long/Short Steel Fibers,” Construction and Building Materials, V. 37, No. 3, 2012, pp. 832-840. doi: 10.1016/j.conbuildmat.2012.07.060

7. Pereira, E. B.; Fischer, G.; and Barros, J., “Effect of Hybrid Fiber Reinforcement on the Cracking Process in Fiber Reinforced Cementitious Composites,” Cement and Concrete Composites, V. 34, No. 10, 2012, pp. 1114-1123. doi: 10.1016/j.cemconcomp.2012.08.004

8. Yang, J. M.; Min, K. H.; Shin, H. O.; and Yoon, Y. S., “Effect of Steel and Synthetic Fibers on Flexural Behavior of High-Strength Concrete Beams Reinforced with FRP Bars,” Composites. Part B, Engineering, V. 43, No. 3, 2012, pp. 1077-1086. doi: 10.1016/j.compositesb.2012.01.044

9. Wang, H., and Belarbi, A., “Ductility Characteristics of Fiber-Reinforced-Concrete Beams Reinforced with FRP Rebars,” Construction and Building Materials, V. 25, No. 5, 2011, pp. 2391-2401. doi: 10.1016/j.conbuildmat.2010.11.040

10. Ding, Y.; Ning, X.; Zhang, Y.; Pacheco-Torgal, F.; and Aguiar, J. B., “Fibres for Enhancing of the Bond Capacity between GFRP Rebar and Concrete,” Construction and Building Materials, V. 51, No. 2, 2014, pp. 303-312. doi: 10.1016/j.conbuildmat.2013.10.089

11. Beglarigale, A., and Yazıcı, H., “Pull-Out Behavior of Steel Fiber Embedded in Flowable RPC and Ordinary Mortar,” Construction and Building Materials, V. 75, 2015, pp. 255-265. doi: 10.1016/j.conbuildmat.2014.11.037

12. Buratti, N.; Ferracuti, B.; and Savoia, M., “Concrete Crack Reduction in Tunnel Linings by Steel Fibre-Reinforced Concretes,” Construction and Building Materials, V. 44, No. 7, 2013, pp. 249-259. doi: 10.1016/j.conbuildmat.2013.02.063

13. Söylev, T. A., and Özturan, T., “Durability, Physical and Mechanical Properties of Fiber-Reinforced Concretes at Low-Volume Fraction,” Construction and Building Materials, V. 73, 2014, pp. 67-75. doi: 10.1016/j.conbuildmat.2014.09.058

14. Tassew, S. T., and Lubell, A. S., “Mechanical Properties of Glass Fiber Reinforced Ceramic Concrete,” Construction and Building Materials, V. 51, No. 1, 2014, pp. 215-224. doi: 10.1016/j.conbuildmat.2013.10.046

15. Sayyar, M.; Soroushian, P.; Sadiq, M. M.; Balachandra, A.; and Lu, J., “Low-Cost Glass Fiber Composites with Enhanced Alkali Resistance Tailored Towards Concrete Reinforcement,” Construction and Building Materials, V. 44, No. 3, 2013, pp. 458-463. doi: 10.1016/j.conbuildmat.2013.03.055

16. Alberti, M. G.; Enfedaque, A.; and Gálvez, J. C., “On the Mechanical Properties and Fracture Behavior of Polyolefin Fiber-Reinforced Self-Compacting Concrete,” Construction and Building Materials, V. 55, No. 4, 2014, pp. 274-288. doi: 10.1016/j.conbuildmat.2014.01.024

17. Pereira-De-Oliveira, L. A.; Castro-Gomes, J. P.; and Nepomuceno, M. C. S., “Effect of Acrylic Fibres Geometry on Physical, Mechanical and Durability Properties of Cement Mortars,” Construction and Building Materials, V. 27, No. 1, 2012, pp. 189-196. doi: 10.1016/j.conbuildmat.2011.07.061

18. Vincent, T., and Ozbakkaloglu, T., “Influence of Fiber Orientation and Specimen End Condition on Axial Compressive Behavior of FRP-Confined Concrete,” Construction and Building Materials, V. 47, 2013, pp. 814-826. doi: 10.1016/j.conbuildmat.2013.05.085

19. Chaves, L. P., and Cunha, J., “Design of Carbon Fiber Reinforcement of Concrete Slabs Using Topology Optimization,” Construction and Building Materials, V. 73, 2014, pp. 688-698. doi: 10.1016/j.conbuildmat.2014.10.011

20. Cao, M.; Zhang, C.; and Lv, H., “Mechanical Response and Shrinkage Performance of Cementitious Composites with a New Fiber Hybridization,” Construction and Building Materials, V. 57, No. 5, 2014, pp. 45-52. doi: 10.1016/j.conbuildmat.2014.01.088

21. Pujadas, P.; Blanco, A.; Cavalaro, S.; de la Fuente, A.; and Aguado, A., “Fibre Distribution in Macro-Plastic Fibre Reinforced Concrete Slab-Panels,” Construction and Building Materials, V. 64, No. 30, 2014, pp. 496-503. doi: 10.1016/j.conbuildmat.2014.04.067

22. JGJ/T 221-2010, “Technical Specification for Application of Fiber Reinforced Concrete,” China Architecture & Building Press, Beijing, China, 2010, 62 pp. (in Chinese)

23. CECS 13:2009, “Standard Test Methods for Fiber Reinforced Concrete,” China Association for Engineering Construction Standardization, Beijing, China, 2009, 116 pp. (in Chinese)

24. Dhinakaran, G.; Manoharan, K.; and Jeyasehar, C. A., “Load Deformation Characteristics of GFRP Reinforced HPC Square Columns,” Journal of Civil Engineering Research & Practice, V. 7, No. 2, 2011. doi: 10.4314/jcerp.v7i2.63726

25. Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., “Concrete Columns Reinforced Longitudinally and Transversally with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 551-558.

26. Luca, A. D.; Matta, F.; and Nanni, A., “Behavior of Full-Scale Glass Fiber-Reinforced Polymer Reinforced Concrete Columns under Axial Load,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct. 2010, pp. 589-596.

27. Sharma, U. K.; Bhargava, P.; and Kaushik, S., “Behavior of Confined High Strength Concrete Columns under Axial Compression,” Journal of Advanced Concrete Technology, V. 3, No. 2, 2005, pp. 267-281. doi: 10.3151/jact.3.267

28. Hasan, H. A.; Sheikh, M. N.; and Hadi, M. N. S., “Maximum Axial Load Carrying Capacity of Fibre Reinforced-Polymer (FRP) Bar Reinforced Concrete Columns under Axial Compression,” Structures, V.  19, 2019, pp. 227-233. doi: 10.1016/j.istruc.2018.12.012

29. Naderpour, H.; Nagai, K.; Fakharian, P.; and Haji, M., “Innovative Models for Prediction of Compressive Strength of FRP-Confined Circular Reinforced Concrete Columns Using Soft Computing Methods,” Composite Structures, V. 215, 2019, pp. 69-84. doi: 10.1016/j.compstruct.2019.02.048

30. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

31. GB 50608-2010, “Technical Code for Infrastructure Application of FRP Composites,” China Metallurgical Construction Association, Beijing, China, 2010, 183 pp. (in Chinese)

32. CAN/CSA S806-12, “Design and Construction of Building Structures with Fibre-Reinforced Polymers,” Canadian Standards Association, Mississauga, ON, Canada, 2012, 177 pp.

33. Sun, L.; Wei, M.; and Zhang, N., “Experimental Study on the Behavior of GFRP Reinforced Concrete Columns under Eccentric Axial Load,” Construction and Building Materials, V. 152, 2017, pp. 214-225. doi: 10.1016/j.conbuildmat.2017.06.159

34. Salah-Eldin, A.; Mohamed, H. M.; and Benmokrane, B., “Structural Performance of High-Strength-Concrete Columns Reinforced with GFRP Bars and Ties Subjected to Eccentric Loads,” Engineering Structures, V. 185, 2019, pp. 286-300. doi: 10.1016/j.engstruct.2019.01.143

35. Choo, C. C.; Harik, I. E.; and Gesund, H., “Strength of Rectangular Concrete Columns Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 103, No. 3, May-June 2006, pp. 452-459.

36. Choo, C. C.; Harik, I. E.; and Gesund, H., “Minimum Reinforcement Ratio for Fiber-Reinforced Polymer Reinforced Concrete Rectangular Columns,” ACI Structural Journal, V. 103, No. 3, May-June 2006, pp. 460-466.

37. Khorramian, K., and Sadeghian, P., “Experimental and Analytical Behavior of Short Concrete Columns Reinforced with GFRP Bars under Eccentric Loading,” Engineering Structures, V. 151, 2017, pp. 761-773. doi: 10.1016/j.engstruct.2017.08.064

38. ASTM D1141-98(2013), “Standard Practice for the Preparation of Substitute Ocean Water,” ASTM International, West Conshohocken, PA, 2013, 3 pp.

39. GB/T 50081-2002, “Standard for Test Method of Mechanical Properties on Ordinary Concrete,” China Architecture & Building Press, Beijing, China, 2003, 33 pp. (in Chinese)

40. GB 50010-2010, “Code for Design of Concrete Structures,” China Architecture & Building Press, Beijing, China, 2011, 425 pp. (in Chinese)

41. Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., “Behavior of Concentrically Loaded Fiber-Reinforced Polymer Reinforced Concrete Columns with Varying Reinforcement Types and Ratios,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 375-385.

42. Kobayashi, K., and Fujisaki, T., “Compressive Behavior of FRP Reinforcement in Non-Prestressed Concrete Members,” NonMetallic (FRP) Reinforcement for Concrete Structures: Proceedings of the Second International RILEM Conference, CRC Press, Boca Raton, FL, 1995, pp. 267-274.


ALSO AVAILABLE IN:

Electronic Structural Journal