Seismic Behavior of Carbon Fiber-Reinforced Polymer-Strengthened Reinforced Concrete Members with Various Anchors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Carbon Fiber-Reinforced Polymer-Strengthened Reinforced Concrete Members with Various Anchors

Author(s): Elias I. Saqan, Hayder A. Rasheed, and Tarek Alkhrdaji

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 3-14

Keywords: carbon fiber-reinforced polymer (CFRP) splay anchors; cyclic load; flexural strengthening; full wrapping; hysteresis; seismic behavior

DOI: 10.14359/51723517

Date: 7/1/2020

Abstract:
Due to the lack of sufficient experimental studies, the subject of fiber-reinforced polymer (FRP) anchorage has not been addressed in ACI 440.2R-17 in a quantifiable sense. This study is intended to examine the seismic performance of flexural frame members strengthened with carbon fiber-reinforced polymer (CFRP) and anchored using CFRP wrapping and CFRP splay anchors. Five full-scale reinforced concrete assemblages were tested as a control, strengthened with full wraps, strengthened with two arrangements of splay anchors, and strengthened with a combination of a splay anchor and full wrap. The seismic response is traced cyclically up to 3% drift ratios. Various response parameters were extracted from the hysteresis curves of the specimens, and are presented and discussed in this paper. The dense splay anchor specimen along with the splay anchors plus full-wrap specimen provided adequate confinement/stabilization to the plastic hinge region and yielded the best seismic performance overall. The dense splay anchorage arrangement is suggested to use when access is not available to provide full wrapping at the critical plastic hinge zone.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2017, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 112 pp.

Ali, O.; Bigaud, D.; and Riahi, H., 2018, “Seismic Performance of Reinforced Concrete Frame Structures Strengthened with FRP Laminates Using a Reliability-Based Advanced Approach,” Composites. Part B, Engineering, V. 139, pp. 238-248. doi: 10.1016/j.compositesb.2017.11.051

Clough, R., and Penzien, J., 1993, Dynamics of Structures, McGraw-Hill, New York, NY.

Dalalbashi, A.; Eslami, A.; and Ronagh, H. R., 2012, “Plastic Hinge Relocation in RC Joints as an Alternative Method of Retrofitting Using FRP,” Composite Structures, V. 94, No. 8, pp. 2433-2439. doi: 10.1016/j.compstruct.2012.02.016

Del Vecchio, C.; Di Ludovico, M.; Prota, A.; and Manfredi, G., 2015, “Analytical Model and Design Approach for FRP Strengthening of Non-Conforming RC Corner Beam–Column Joints,” Engineering Structures, V. 87, pp. 8-20. doi: 10.1016/j.engstruct.2015.01.013

El-Amoury, T., and Ghobarah, A., 2002, “Seismic Rehabilitation of Beam–Column Joint Using GFRP Sheets,” Engineering Structures, V. 24, No. 11, pp. 1397-1407. doi: 10.1016/S0141-0296(02)00081-0

Le-Trung, K.; Lee, K.; Lee, J.; Lee, D.; and Woo, S., 2010, “Experimental Study of RC Beam-Column Joints Strengthened Using CFRP Composites,” Composites. Part B, Engineering, V. 41, No. 1, pp. 76-85. doi: 10.1016/j.compositesb.2009.06.005

Lee, W. T.; Chiou, Y. J.; and Shih, M. H., 2010, “Reinforced Concrete Beam-Column Joint Strengthened with Carbon Fiber Reinforced Polymer,” Composite Structures, V. 92, No. 1, pp. 48-60. doi: 10.1016/j.compstruct.2009.06.011

Mahini, S. S., and Ronagh, H., 2007, “A New Method for Improving Ductility in Existing RC Ordinary Moment Resisting Frames Using FRPs,” Asian Journal of Civil Engineering, V. 8, No. 6, pp. 581-595. (Building and Housing)

Mukherjee, A., and Joshi, M., 2005, “FRPC Reinforced Concrete Beam-Column Joints under Cyclic Excitation,” Composite Structures, V. 70, No. 2, pp. 185-199. doi: 10.1016/j.compstruct.2004.08.022

Niroomandi, A.; Maheri, A.; Maheri, M. R.; and Mahini, S. S., 2010, “Seismic Performance of Ordinary RC Frames Retrofitted at Joints by FRP Sheets,” Engineering Structures, V. 32, No. 8, pp. 2326-2336. doi: 10.1016/j.engstruct.2010.04.008

Parvin, A., and Wu, S., 2008, “Ply Angle Effect on Fiber Composite Wrapped Reinforced Concrete Beam–Column Connections under Combined Axial and Cyclic Loads,” Composite Structures, V. 82, No. 4, pp. 532-538. doi: 10.1016/j.compstruct.2007.02.004

Rasheed, H. A., 2015, Strengthening Design of Reinforced Concrete with FRP, CRC Press, Boca Raton, FL, 230 pp.

Rasheed, H. A.; Decker, B. R.; Esmaeily, A.; Peterman, R. J.; and Melhem, H. G., 2015, “The Influence of CFRP Anchorage on Achieving Sectional Flexural Capacity of Strengthened Concrete Beams,” Fibers, Basel, Switzerland, V. 3, No. 4, pp. 539-559. doi: 10.3390/fib3040539

Realfonzo, R.; Napoli, A.; and Pinilla, J. G. R., 2014, “Cyclic Behavior of RC Beam-Column Joints Strengthened with FRP Systems,��� Construction and Building Materials, V. 54, pp. 282-297. doi: 10.1016/j.conbuildmat.2013.12.043

Ronagh, H. R., and Eslami, A., 2013, “Flexural Retrofitting of RC Buildings Using GFRP/CFRP–A Comparative Study,” Composites. Part B, Engineering, V. 46, pp. 188-196. doi: 10.1016/j.compositesb.2012.09.072

Singh, V.; Bansal, P. P.; Kumar, M.; and Kaushik, S. K., 2014, “Experimental Studies on Strength and Ductility of CFRP Jacketed Reinforced Concrete Beam-Column Joints,” Construction and Building Materials, V. 55, pp. 194-201. doi: 10.1016/j.conbuildmat.2014.01.047

Smith, S. T.; Hu, S.; Kim, S. J.; and Seracino, R., 2011, “FRP-Strengthened RC Slabs Anchored with FRP Anchors,” Engineering Structures, V. 33, No. 4, pp. 1075-1087. doi: 10.1016/j.engstruct.2010.11.018

Smith, S. T.; Rasheed, H. A.; and Kim, S. J., 2017, “Full-Range Load-Deflection Response of FRP-Strengthened RC Flexural Members Anchored with FRP Anchors,” Composite Structures, V. 167, pp. 207-218. doi: 10.1016/j.compstruct.2017.02.002

Smith, S. T.; Zhang, H.; and Wang, Z., 2013, “Influence of FRP Anchors on the Strength and Ductility of FRP-Strengthened RC Slabs,” Construction and Building Materials, V. 49, pp. 998-1012. doi: 10.1016/j.conbuildmat.2013.02.006

Zhang, H., and Smith, S. T., 2017, “Influence of Plate Length and Anchor Position on FRP-to-Concrete Joints Anchored with FRP Anchors,” Composite Structures, V. 159, pp. 615-624. doi: 10.1016/j.compstruct.2016.09.086