Bond Differences at Two Ends of Steel Fiber-Reinforced Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond Differences at Two Ends of Steel Fiber-Reinforced Concrete Columns

Author(s): Kai Wu, Feng Chen, Huiming Zheng, Chuyang Chen, and Jianan Xu

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 77-90

Keywords: bond difference; damage resistance; energy dissipation; loadslip curve; steel fiber-reinforced concrete-encased composite

DOI: 10.14359/51723506

Date: 7/1/2020

Abstract:
To avoid certain difficulties in concrete-encased composite construction such as interference between the shaped steel and reinforcing bars and poor concrete placement quality, steel fiber-reinforced concrete-encased composite (SFRCEC) section was proposed by replacing the steel reinforcing bars with steel fibers. The bond property between shaped steel and steel fiber-reinforced concrete (SFRC) is crucial to composite members. According to the pushout test of 20 specimens, this paper studies the bond property and interface damage between shaped steel and SFRC. The load-slip curve, bond strength, interface energy dissipation, and other important data are obtained. The differences at the interface from uneven bond force distribution are analyzed. The load and slip are not always the same at different locations along the interface. The influences of embedded length of shaped steel (Le), steel fiber ratio (ρsf), and the thickness of concrete cover (Css) are also discussed. For every 100 mm increase in Le, the slip difference between two ends increases by 0.257 mm, which shows a linear growth. When the ratio of steel fiber is between 1 and 3%, the thickness of concrete cover is between 20 and 60 mm, with bigger Css or higher ρsf, and the difference within a unit length becomes smaller. Increasing the ρsf or the Css will enhance the bond and constraint between SFRC and the steel and give higher crack resistance to the concrete cover. This also helps the bond stress distribution along the interface, which means a more balanced loading distribution between two materials at the interface under maximum loading.

Related References:

1. Weng, C. C., and Yen, S. I., “Comparisons of Concrete-Encased Composite Column Strength Provisions of ACI Code and AISC Specification,” Engineering Structures, V. 24, No. 1, 2002, pp. 59-72. doi: 10.1016/S0141-0296(01)00067-0

2. Chen, C. C., and Lin, N. J., “Analytical Model for Predicting Axial Capacity and Behavior of Concrete Encased Steel Composite Stub Columns,” Journal of Constructional Steel Research, V. 62, No. 5, 2006, pp. 424-433. doi: 10.1016/j.jcsr.2005.04.021

3. Ricles, J. M., and Paboojian, S. D., “Seismic Performance of Steel-Encased Composite Columns,” Journal of Structural Engineering, ASCE, V. 120, No. 8, 1994, pp. 2474-2494. doi: 10.1061/(ASCE)0733-9445(1994)120:8(2474)

4. Hsu, H. L.; Hsieh, J. C.; and Juang, J. L., “Seismic Performance of Steel-Encased Composite Members with Strengthening Cross-Inclined Bars,” Journal of Constructional Steel Research, V. 60, No. 11, 2004, pp. 1663-1679. doi: 10.1016/j.jcsr.2004.04.002

5. Chen, C. H.; Wang, C. K.; and Sun, H. Z., “Experimental Study on Seismic Behavior of Full Encased Steel-Concrete Composite Columns,” Journal of Structural Engineering, ASCE, V. 140, No. 6, 2014, p. 04014024 doi: 10.1061/(ASCE)ST.1943-541X.0000951

6. Saw, H. S., and Liew, J. Y. R., “Assessment of Current Methods for the Design of Composite Columns in Buildings,” Journal of Constructional Steel Research, V. 53, No. 2, 2000, pp. 121-147. doi: 10.1016/S0143-974X(99)00062-0

7. Xue, J. Y.; Zhou, C. F.; Liu, Z. Q.; and Qi, L. J., “Seismic Response of Steel Reinforced Concrete Spatial Frame with Irregular Section Columns under Earthquake Excitation,” Earthquakes and Structures, V. 14, No. 4, 2018, pp. 337-347.

8. Azizinamini, A., and Ghosh, S. K., “Steel Reinforced Concrete Structures in 1995 Hyogoken-Nanbu Earthquake,” Journal of Structural Engineering, ASCE, V. 123, No. 8, 1997, pp. 986-992. doi: 10.1061/(ASCE)0733-9445(1997)123:8(986)

9. Ye, M.; Pi, Y. P.; and Ren, M., “Experimental and Analytical Investigation on RC Columns with Distributed-Steel Bar,” Structural Engineering and Mechanics, V. 47, No. 6, 2013, pp. 741-756. doi: 10.12989/sem.2013.47.6.741

10. Seo, J., and Varma, A. H., “Experimental Behavior and Design of Steel Plate Composite-to-Reinforced Concrete Lap Splice Connections,” Journal of Structural Engineering, V. 143, No. 5, 2017, p. 04017011 doi: 10.1061/(ASCE)ST.1943-541X.0001711

11. Nzabonimpa, J. D., and Hong, W. K., “Novel Precast Erection Method of Interlocking Mechanical Joints Using Couplers,” Journal of Construction Engineering and Management, ASCE, V. 144, No. 6, 2018, p. 04018036 doi: 10.1061/(ASCE)CO.1943-7862.0001482

12. Yang, Y.; Yu, Y. L.; Guo, Y. X.; Roeder, C. W.; Xue, Y.; and Shao, Y., “Experimental Study on Shear Performance of Partially Precast Castellated Steel Reinforced Concrete (CPSRC) Beams,” Steel and Composite Structures, V. 21, No. 2, 2016, pp. 289-302. doi: 10.12989/scs.2016.21.2.289

13. Su, Q. T.; Dai, C. Y.; and Xu, C., “Full-Scale Experimental Study on the Negative Flexural Behavior of Orthotropic Steel-Concrete Composite Bridge Deck,” Journal of Bridge Engineering, ASCE, V. 23, No. 12, 2018, p. 04018097 doi: 10.1061/(ASCE)BE.1943-5592.0001320

14. Sharma, S.; Arora, V. V.; Kumar, S.; Daniel, Y. N.; and Sharma, A., “Durability Study of High-Strength Steel Fiber-Reinforced Concrete,” ACI Structural Journal, V. 115, No. 2, Mar. 2018, pp. 219-225.

15. Paultre, P.; Eid, R.; Langlois, Y.; and Lévesque, Y., “Behavior of Steel Fiber-Reinforced High-Strength Concrete Columns under Uniaxial Compression,” Journal of Structural Engineering, ASCE, V. 136, No. 10, 2010, pp. 1225-1235. doi: 10.1061/(ASCE)ST.1943-541X.0000211

16. Song, P. S., and Hwang, S., “Mechanical Properties of High-Strength Steel Fiber-Reinforced Concrete,” Construction and Building Materials, V. 18, No. 9, 2004, pp. 669-673. doi: 10.1016/j.conbuildmat.2004.04.027

17. Amin, A., and Gilbert, R. I., “Steel Fiber-Reinforced Concrete Beams—Part II: Strength, Ductility, and Design,” ACI Structural Journal, V. 116, No. 2, Mar. 2019, pp. 113-123. doi: 10.14359/51713289

18. Chanthabouala, K.; Teng, S.; Chandra, J.; Tan, K.-H.; and Ostertag, C. P., “Punching Tests of Double-Hooked-End Fiber-Reinforced Concrete Slabs,” ACI Structural Journal, V. 115, No. 6, Nov. 2018, pp. 1777-1789. doi: 10.14359/51706891

19. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

20. Dinh, H. H.; Parra-Montesinos, G. J.; and Wight, J. K., “Shear Behavior of Steel Fiber-Reinforced Concrete Beams without Stirrup Reinforcement,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct. 2010, pp. 597-606.

21. Ding, Y. N.; You, Z. G.; and Jalali, S., “The Composite Effect of Steel Fibres and Stirrups on the Shear Behaviour of Beams Using Self-Consolidating Concrete,” Engineering Structures, V. 33, No. 1, 2011, pp. 107-117. doi: 10.1016/j.engstruct.2010.09.023

22. Boita, I. E.; Dan, D.; and Stoian, V., “Seismic Behaviour of Composite Steel Fibre Reinforced Concrete Shear Walls,” IOP Conference Series. Materials Science and Engineering, V. 245, 2017, p. 022006 doi: 10.1088/1757-899X/245/2/022006

23. Yoo, D. Y.; Yuan, T. F.; Yang, J. M.; and Yoon, Y. S., “Feasibility of Replacing Minimum Shear Reinforcement with Steel Fibers for Sustainable High-Strength Concrete Beams,” Engineering Structures, V. 147, 2017, pp. 207-222. doi: 10.1016/j.engstruct.2017.06.004

24. Valipour, H.; Vessali, N.; and Foster, S., “Fibre-Reinforced Concrete Beam Assemblages Subject to Column Loss,” Magazine of Concrete Research, V. 68, No. 6, 2016, pp. 305-317. doi: 10.1680/macr.15.00095

25. Ghazizadeh, S., and Cruz-Noguez, C. A., “Damage-Resistant Reinforced Concrete Low-Rise Walls with Hybrid GFRP-Steel Reinforcement and Steel Fibers,” Journal of Composites for Construction, ASCE, V. 22, No. 2, 2018, p. 04018002 doi: 10.1061/(ASCE)CC.1943-5614.0000834

26. Hung, C. C., and Hu, F. Y., “Behavior of High-Strength Concrete Slender Columns Strengthened with Steel Fibers under Concentric Axial Loading,” Construction and Building Materials, V. 175, 2018, pp. 422-433. doi: 10.1016/j.conbuildmat.2018.04.201

27. Muttoni, A., and Fernández Ruiz, M., “Shear Strength of Members without Transverse Reinforcement as Function of Critical Shear Crack Width,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr. 2008, pp. 163-172.

28. Qian, C. X., and Indubhushan, P., “Properties of High-Strength Steel Fiber-Reinforced Concrete Beams in Bending,” Cement and Concrete Composites, V. 21, No. 1, 1999, pp. 73-81. doi: 10.1016/S0958-9465(98)00040-7

29. Chen, Z. P.; Xu, J. J.; Liang, Y.; and Su, Y. S., “Bond Behaviors of Shape Steel Embedded in Recycled Aggregate Concrete and Recycled Aggregate Concrete Filled in Steel Tubes,” Steel and Composite Structures, V. 17, No. 6, 2014, pp. 929-949. doi: 10.12989/scs.2014.17.6.929

30. Roeder, C. W.; Chmielowski, R.; and Brown, C. B., “Shear Connector Requirements for Embedded Steel Sections,” Journal of Structural Engineering, ASCE, V. 125, No. 2, 1999, pp. 142-151. doi: 10.1061/(ASCE)0733-9445(1999)125:2(142)

31. Wang, W. H.; Han, L. H.; Tan, Q. H.; and Tao, Z., “Tests on the Steel–Concrete Bond Strength in Steel Reinforced Concrete (SRC) Columns after Fire Exposure,” Fire Technology, V. 53, No. 2, 2017, pp. 917-945. doi: 10.1007/s10694-016-0610-6

32. Chen, L. H.; Dai, J. X.; Jin, Q. L.; Chen, L. F.; and Liu, X. L., “Refining Bond–Slip Constitutive Relationship between Checkered Steel Tube and Concrete,” Construction and Building Materials, V. 79, 2015, pp. 153-164. doi: 10.1016/j.conbuildmat.2014.12.058

33. Feng, R.; Chen, Y.; He, K.; Wei, J. G.; Chen, B. C.; and Zhang, X. T., “Push-Out Tests of Concrete-Filled Stainless Steel SHS Tubes,” Journal of Constructional Steel Research, V. 145, 2018, pp. 58-69. doi: 10.1016/j.jcsr.2018.02.016

34. Zhao, Y. X.; Lin, H. W.; Wu, K.; and Jin, W. L., “Bond Behavior of Normal/Recycled Concrete and Corroded Steel Bars,” Construction and Building Materials, V. 48, No. 11, 2013, pp. 348-359. doi: 10.1016/j.conbuildmat.2013.06.091

35. Wang, B.; Bai, G. L.; Dai, H. J.; and Wu, S. H., “Experimental and Mechanical Analysis of Bond-Slip Performance between Recycled Concrete and Rebar,” Engineering Mechanics, V. 30, No. 10, 2013, pp. 54-64. doi: 10.3901/JME.2016.10.054

36. Ding, Y.; Wu, M.; Xu, L. H.; Zhu, H. T.; and Li, Z. X., “Seismic Damage Evolution of Steel–Concrete Hybrid Space-Frame Structures,” Engineering Structures, V. 119, 2016, pp. 1-12. doi: 10.1016/j.engstruct.2016.04.007

37. Maeda, M., and Kang, D. E., “Post-Earthquake Damage Evaluation of Reinforced Concrete Buildings,” Journal of Advanced Concrete Technology, V. 7, No. 3, 2009, pp. 327-335. doi: 10.3151/jact.7.327


ALSO AVAILABLE IN:

Electronic Structural Journal