Monitoring Concrete Placements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Monitoring Concrete Placements

Author(s):

Publication: Concrete International

Volume: 41

Issue: 12

Appears on pages(s): 42-43

Keywords: data, transmitter, thermocouple, curing

DOI: 10.14359/51722417

Date: 12/1/2019

Abstract:

MaturixTM, a concrete placement monitoring system, can be used to determine the temperature and strength of concrete placements. The system comprises type K or type A temperature sensors coupled to reusable, weatherproof wireless transmitters. After concrete is placed, the transmitters begin sending data that can be monitored using a mobile device or computer.