Shotcrete Incorporated into ACI 318-19 Building Code

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shotcrete Incorporated into ACI 318-19 Building Code

Author(s): Charles Hanskat, Terence C. Holland, and Bruce A. Suprenant

Publication: Concrete International

Volume: 41

Issue: 12

Appears on pages(s): 31-35

Keywords: committee, provision, mix, standard

DOI: 10.14359/51722412

Date: 12/1/2019

Abstract:
Shotcrete has been incorporated into the International Building Code (IBC) for many years but was not expressly covered in the ACI 318 Code. Conversations between ACI and International Code Council staff indicated that it would be possible to delete the shotcrete provisions from the IBC upon satisfactory incorporation of shotcrete into the ACI 318 Code. Thus, ACI Subcommittees 318-A and 318-B worked for 5 years to successfully include shotcrete into ACI 318-19.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

2. “2015 International Building Code,” first edition, International Code Council, Falls Church, VA, 2014, 690 pp.

3. “2000 International Building Code,” International Code Council, Falls Church, VA, 2000, 300 pp.

4. ACI Committee 506, “Guide to Shotcrete (ACI 506R-90),” American Concrete Institute, Farmington Hills, MI, 1990, 81 pp.

5. ACI Committee 506, “Guide to Shotcrete (ACI 506R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 52 pp.

6. ACI Committee 506, “Guide to Fiber-Reinforced Shotcrete (ACI 506.1R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 14 pp.

7. ACI Committee 506, “Specifications for Shotcrete (ACI 506.2-13 (Reapproved 2018)),” American Concrete Institute, Farmington Hills, MI, 2013, 12 pp.

8. ACI Committee 506, “Guide for the Evaluation of Shotcrete (ACI 506.4R-94 (Reapproved 2004)),” American Concrete Institute, Farmington Hills, MI, 1994, 12 pp.

9. ACI Committee 506, “Guide for Specifying Underground Shotcrete (ACI 506.5R-09 (Reapproved 2016)),” American Concrete Institute, Farmington Hills, MI, 2009, 52 pp.

10. ACI Committee 506, “Visual Shotcrete Core Quality Evaluation TechNote (ACI 506.6T-17),” American Concrete Institute, Farmington Hills, MI, 2017, 4 pp.

11. ACI Committee 506, “Guide for the Evaluation of Shotcrete (ACI 506.4R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 18 pp.

12. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

13. Seegebrecht, G.W.; Litvan, A.; and Gebler, S.H., “Durability of Dry-Mix Shotcrete,” Concrete International, V. 11, No. 10, Oct. 1989, pp. 47-50.

14. Bertrand, J., and Vezina, D., “The Development of Air-Entrained Durable Shotcrete for Structural Repairs,” Proceedings of Shotcrete for Underground Support VII, Telfs, Austria, June 11-15, 1994, pp. 58-65.

15. Zhang, L., “Testing Air Content of Dry-Mix Shotcrete,” Shotcrete, V. 17, No. 2, Spring 2015, pp. 22-24.