Stability of Lightweight Self-Consolidating Concrete Containing Coarse and Fine Expanded Slate Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stability of Lightweight Self-Consolidating Concrete Containing Coarse and Fine Expanded Slate Aggregates

Author(s): Mohamed M. Sadek, Mohamed K. Ismail, and Assem A. A. Hassan

Publication: Materials Journal

Volume: 117

Issue: 3

Appears on pages(s): 133-143

Keywords: expanded slate fine and coarse aggregates; fresh properties; semi-lightweight self-consolidating concrete; strength

DOI: 10.14359/51722407

Date: 5/1/2020

Abstract:
This study aimed to optimize the use of fine and coarse expanded slate lightweight aggregates in developing successful semi-lightweight self-consolidating concrete (SLWSCC) mixtures with densities ranging from 1850 to 2000 kg/m3 (115.5 to 124.9 lb/ft3) and strength of at least 50 MPa (7.25 ksi). All SLWSCC mixtures were developed by replacing either the fine or coarse normal-weight aggregates with expanded slate aggregates. Two additional normal-weight self-consolidating concrete mixtures were developed for comparison. The results indicated that due to the challenge in achieving acceptable self-consolidation, a minimum binder content of at least 500 kg/m3 (31.2 lb/ft3) and a minimum water-binder ratio (w/b) of 0.4 were required to develop successful SLWSCC with expanded slate. The use of metakaolin and fly ash were also found to be necessary to develop successful mixtures with optimized strength, flowability, and stability. The results also showed that SLWSCC mixtures made with expanded slate fine aggregate required more high-range water-reducing admixture than mixtures made with expanded slate coarse aggregate. However, at a given density, mixtures developed with expanded slate fine aggregate generally exhibited better fresh properties in terms of flowability and passing ability, as well as higher strength compared to mixtures developed with expanded slate coarse aggregate.

Related References:

1. Dhir, K.; Mays, R. G. C.; and Chua, H. C., “Lightweight Structural Concrete with Aglite Aggregate: Mix and Design Properties,” The International Journal of Cement Composites and Lightweight Concrete, V. 6, No. 4, 1984, pp. 249-261. doi: 10.1016/0262-5075(84)90020-4

2. Balendran, R. V.; Zhou, F. P.; Nadeem, A.; and Leung, A. Y. T., “Influence of Steel Fibres on Strength and Ductility of Normal and Lightweight High Strength Concrete,” Building and Environment, V. 37, No. 12, 2002, pp. 1361-1367. doi: 10.1016/S0360-1323(01)00109-3

3. Real, S.; Bogas, J. A.; Gomes, M. D. G.; and Ferrer, B., “Thermal Conductivity of Structural Lightweight Aggregate Concrete,” Magazine of Concrete Research, V. 68, No. 15, 2016, pp. 798-808. doi: 10.1680/jmacr.15.00424

4. Rossignolo, J. A., and Agnesini, M. V. C., “Mechanical Properties of Polymer-Modified Lightweight Aggregate Concrete,” Cement and Concrete Research, V. 32, No. 3, 2002, pp. 329-334. doi: 10.1016/S0008-8846(01)00678-0

5. Ko, D., and Choi, H., “Truss Rail Method for Punching Shear Strength of Flat-Plate Slab-Column Using High-Strength Lightweight Concrete,” Magazine of Concrete Research, V. 65, No. 10, 2013, pp. 589-599. doi: 10.1680/macr.12.00116

6. Kim, H. K.; Jeon, J. H.; and Lee, H. K., “Workability, and Mechanical, Acoustic and Thermal Properties of Lightweight Aggregate Concrete with a High Volume of Entrained Air,” Construction and Building Materials, V. 29, 2012, pp. 193-200. doi: 10.1016/j.conbuildmat.2011.08.067

7. Haque, N., and Al-Khaiat, H., “Strength and Durability of Lightweight Concrete in Hot Marine Exposure Conditions,” Materials and Structures, V. 32, No. 7, 1999, pp. 533-538. doi: 10.1007/BF02481638

8. Sari, D., and Pasamehmetoglu, A. G., “The Effects of Gradation and Admixture on the Pumice Lightweight Aggregate Concrete,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 936-942. doi: 10.1016/j.cemconres.2004.04.020

9. Kayali, O., “Fly Ash Lightweight Aggregates in High Performance Concrete,” Construction and Building Materials, V. 22, No. 12, 2008, pp. 2393-2399. doi: 10.1016/j.conbuildmat.2007.09.001

10. Raithby, K. D., and Lydon, F. D., “Lightweight Concrete in Highway Bridges,” The International Journal of Cement Composites and Lightweight Concrete, V. 3, No. 2, 1981, pp. 133-146. doi: 10.1016/0262-5075(81)90007-5

11. Abouhussien, A. A.; Hassan, A. A. A.; and Hussein, A. A., “Effect of Expanded Slate Aggregate on Fresh Properties and Shear Behaviour of Lightweight SCC Beams,” Magazine of Concrete Research, V. 67, No. 9, 2015, pp. 433-442. doi: 10.1680/macr.14.00197

12. Jiang, D.; Wang, G.; Montaruli, B. C.; and Richardson, K. L., “Concrete Offshore LNG Terminals a Viable Solution and Technical Challenges,” Proceedings of Offshore Technology Conference, Houston, TX, 2004, pp. 59-68.

13. Lachemi, M.; Bae, S.; Hossain, K. M. A.; and Sahmaran, M., “Steel-Concrete Bond Strength of Lightweight Self-Consolidating Concrete,” Materials and Structures, V. 42, No. 7, 2009, pp. 1015-1023. doi: 10.1617/s11527-008-9440-4

14. Assaad, J. J., and Issa, C. A., “Mixture Optimisation of Polymer-Modified Lightweight SCC,” Magazine of Concrete Research, V. 69, No. 14, 2017, pp. 745-756. doi: 10.1680/jmacr.16.00409

15. Aslani, F., “Effects of Specimen Size and Shape on Compressive and Tensile Strengths of Self-Compacting Concrete with or without Fibres,” Magazine of Concrete Research, V. 65, No. 15, 2013, pp. 914-929. doi: 10.1680/macr.13.00016

16. Safiuddin, M.; Salam, M. A.; and Jumaat, M. Z., “Flowing Ability of Self-Consolidating Concrete and Its Binder Paste Phase Including Palm Oil Fuel Ash,” Magazine of Concrete Research, V. 64, No. 10, 2012, pp. 931-944. doi: 10.1680/macr.11.00135

17. Rao, S. V.; Rao, M. V. S.; Ramaseshu, D.; and Kumar, P. R., “Durability Performance of Self-Compacting Concrete,” Magazine of Concrete Research, V. 64, No. 11, 2012, pp. 1005-1013. doi: 10.1680/macr.11.00165

18. Okamura, H., and Ouchi, M., “Self-Compacting Concrete,” Journal of Advanced Concrete Technology, V. 1, No. 1, 2003, pp. 5-15. doi: 10.3151/jact.1.5

19. Shi, C., and Yang, X., “Design and Application of Self-Consolidating Lightweight Concrete,” Proceedings of China 1st International Symposium on Design, Performance and Use of Self-Consolidating Concrete, RILEM Publication SARL, Paris, France, 2005, pp. 55-64.

20. Yao, S. X., and Gerwick, B. C., “Development of Self-Compacting Lightweight Concrete for RFP Reinforced Floating Concrete Structures,” Technical Report, U.S. Army Corps of Engineers Research and Development Center, San Francisco, CA, 2006.

21. Hubertova, M., and Hela, R., “The Effect of Metakaolin and Silica Fume on the Properties of Lightweight Self-Consolidating Concrete,” 9th CANMET/ACI International Conference on Recent Advances in Concrete Technology, SP-243, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 2007, pp. 35-48.

22. Papanicolaou, C. G., and Kaffetzakis, M. I., “Lightweight Aggregate Self-Compacting: State-of-the-Art & Pumice Application,” Journal of Advanced Concrete Technology, V. 9, No. 1, 2011, pp. 15-29. doi: 10.3151/jact.9.15

23. Lotfy, A.; Hossain, K. M. A.; and Lachemi, M., “Durability Properties of Lightweight Self-Consolidating Concrete Developed with Three Types of Aggregates,” Construction and Building Materials, V. 106, 2016, pp. 43-54. doi: 10.1016/j.conbuildmat.2015.12.118

24. Karahan, O.; Hossain, K. M. A.; Ozbay, E.; Lachemi, M.; and Sancak, E., “Effect of Metakaolin Content on the Properties Self-Consolidating Lightweight Concrete,” Construction and Building Materials, V. 31, 2012, pp. 320-325. doi: 10.1016/j.conbuildmat.2011.12.112

25. Wu, Z.; Zhang, Y.; Zheng, J.; and Ding, Y., “An Experimental Study on the Workability of Self-Compacting Lightweight Concrete,” Construction and Building Materials, V. 23, No. 5, 2009, pp. 2087-2092. doi: 10.1016/j.conbuildmat.2008.08.023

26. Abouhussien, A. A.; Hassan, A. A. A.; and Ismail, M. K., “Properties of Semi-Lightweight Self-Consolidating Concrete Containing Lightweight Slag Aggregate,” Construction and Building Materials, V. 75, 2015, pp. 63-73. doi: 10.1016/j.conbuildmat.2014.10.028

27. Hassan, A. A. A.; Ismail, M. K.; and Mayo, J., “Mechanical Properties Of Self-Consolidating Concrete Containing Lightweight Recycled Aggregate In Different Mixture Compositions,” Journal of Building Engineering, V. 4, 2015, pp. 113-126. doi: 10.1016/j.jobe.2015.09.005

28. Granata, M. F., “Pumice Powder as Filler of Self-Compacting Concrete,” Construction and Building Materials, V. 96, 2015, pp. 581-590. doi: 10.1016/j.conbuildmat.2015.08.040

29. Atmaca, N.; Abbas, M. L.; and Atmaca, A., “Effects of Nano-Silica on the Gas Permeability, Durability and Mechanical Properties of High-Strength Lightweight Concrete,” Construction and Building Materials, V. 147, 2017, pp. 17-26. doi: 10.1016/j.conbuildmat.2017.04.156

30. Lo, T. Y.; Tang, W. C.; and Cui, H. Z., “The Effects of Aggregate Properties on Lightweight Concrete,” Building and Environment, V. 42, No. 8, 2007, pp. 3025-3029. doi: 10.1016/j.buildenv.2005.06.031

31. ASTM C150/C150M-12, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2012, 9 pp.

32. ASTM C618-12, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2012, 3 pp.

33. EFNARC, “The European Guidelines for Self-Compacting Concrete Specification, Production and Use,” English edition, European Federation for Specialist Construction Chemicals and Concrete Systems, Norfolk, UK, 2005.

34. ASTM C1621-09b, “Standard Test Method for Passing Ability of Self-Consolidating Concrete by J-ring,” ASTM International, West Conshohocken, PA, 2009, 5 pp.

35. ASTM C39/C39M-11, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2011, 7 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal