Advanced Calibration of Historic Apparent Moisture Diffusivity Models for Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Advanced Calibration of Historic Apparent Moisture Diffusivity Models for Mortar

Author(s): Milena Rangelov, Somayeh Nassiri, Deviyani Gurung, and Timothy Ginn

Publication: Materials Journal

Volume: 117

Issue: 2

Appears on pages(s): 65-74

Keywords: diffusion; moisture transfer; shrinkage; transport properties

DOI: 10.14359/51722397

Date: 3/1/2020

Abstract:
Models are available to estimate the apparent moisture diffusivity (Da) of cement-based materials (CbMs) for internal relative humidity (h) prediction; however, these models include multiple nonunique shape parameters and are therefore impossible to manually calibrate. A common workaround is to use typical values, which are mostly outdated and inadequate for contemporary CbMs. This study presents an integrated procedure in which a finite difference inverse solution of Fick’s second law is linked with an advanced calibration software to identify and optimize the critical parameters of two widely used Da models. The observation dataset was h-profiles collected in mortar prisms from seven mixtures exposed to one-dimensional drying. Using the integrated method, the models’ parameters were optimized to fit the observation dataset. The impact of water-cement ratio and fly ash content on Da was established. Further, the critical parameters in both models were identified and correlated to different aspects of the pore system.

Related References:

1. Radlinska, A.; Pease, B.; and Weiss, J., “A Preliminary Numerical Investigation on the Influence of Material Variability in the Early-Age Cracking Behavior of Restrained Concrete,” Materials and Structures, V. 40, No. 4, 2007, pp. 375-386. doi: 10.1617/s11527-006-9118-8

2. Baroghel-Bouny, V., “Water Vapour Sorption Experiments on Hardened Cementitious Materials: Part I: Essential Tool for Analysis of Hygral Behaviour and its Relation to Pore Structure,” Cement and Concrete Research, V. 37, No. 3, 2007, pp. 414-437. doi: 10.1016/j.cemconres.2006.11.019

3. Addassi, M.; Johannesson, B.; and Wadsö, L., “Inverse Analyses of Effective Diffusion Parameters Relevant for a Two-Phase Moisture Model of Cementitious Materials,” Cement and Concrete Research, V. 106, 2018, pp. 117-129. doi: 10.1016/j.cemconres.2018.01.011

4. Villani, C.; Lucero, C.; Bentz, D.; Hussey, D.; Jacobson, D. L.; and Weiss, W. J., “Analysis of Drying Processes in Mortars with and without Shrinkage Reducing Admixtures,” Novel Characterization Techniques and Advanced Cementitious Materials: Tribute to James J. Beaudoin, SP-312, American Concrete Institute, Farmington Hills, MI.

5. Villani, C.; Spragg, R.; Pour‐Ghaz, M.; and Weiss, W. J., “The Influence of Pore Solutions Properties on Drying in Cementitious Materials,” Journal of the American Ceramic Society, V. 97, No. 2, 2014, pp. 386-393. doi: 10.1111/jace.12604

6. Zhang, Z.; Thiery, M.; and Baroghel-Bouny, V., “Investigation of Moisture Transport Properties of Cementitious Materials,” Cement and Concrete Research, V. 89, 2016, pp. 257-268. doi: 10.1016/j.cemconres.2016.08.013

7. Philip, J. R., and De Vries, D. A., “Moisture Movement in Porous Materials under Temperature Gradients,” Eos (Washington, D.C.), V. 38, No. 2, 1957, pp. 222-232.

8. Huang, K.; Zollinger, D. G.; Shi, X.; and Sun, P., “A Developed Method of Analyzing Temperature and Moisture Profiles in Rigid Pavement Slabs,” Construction and Building Materials, V. 151, 2017, pp. 782-788. doi: 10.1016/j.conbuildmat.2017.06.120

9. Hajibabaee, A.; Grasley, Z.; and Ley, M. T., “Mechanisms of Dimensional Instability Caused by Differential Drying in Wet Cured Cement Paste,” Cement and Concrete Research, V. 79, 2016, pp. 151-158. doi: 10.1016/j.cemconres.2015.09.007

10. Xin, D.; Zollinger, D. G.; and Allen, G. D., “An Approach To Determine Diffusivity in Hardening Concrete Based on Measured Humidity Profiles,” Advanced Cement Based Materials, V. 2, No. 4, 1995, pp. 138-144. doi: 10.1016/1065-7355(95)90014-4

11. Bažant, Z. P., and Najjar, L. J., “Nonlinear Water Diffusion in Nonsaturated Concrete,” Materiales de Construcción, V. 5, No. 1, 1972, pp. 3-20. doi: 10.1007/BF02479073

12. Xi, Y.; Bažant, Z. P.; and Jennings, H. M., “Moisture Diffusion in Cementitious Materials Adsorption Isotherms,” Advanced Cement Based Materials, V. 1, No. 6, 1994, pp. 248-257. doi: 10.1016/1065-7355(94)90033-7

13. Baroghel-Bouny, V., “Water Vapour Sorption Experiments on Hardened Cementitious Materials. Part II: Essential Tool for Assessment of Transport Properties and for Durability Prediction,” Cement and Concrete Research, V. 37, No. 3, 2007, pp. 438-454. doi: 10.1016/j.cemconres.2006.11.017

14. Mindess, S.; Young, J. F.; and Darwin, D., Concrete, second edition, Pearson Education, Inc., Upper Saddle River, NJ, 2003.

15. Zhang, J.; Hou, D.; Gao, Y.; and Wei, S., “Determination of Moisture Diffusion Coefficient of Concrete at Early Age from Interior Humidity Measurements,” Drying Technology, V. 29, No. 6, 2011, pp. 689-696. doi: 10.1080/07373937.2010.528106

16. Bažant, Z. P., and Najjar, L. J., “Drying of Concrete as a Nonlinear Diffusion Problem,” Cement and Concrete Research, V. 1, No. 5, 1971, pp. 461-473. doi: 10.1016/0008-8846(71)90054-8

17. Akita, H.; Fujiwara, T.; and Ozaka, Y., “A Practical Procedure for the Analysis of Moisture Transfer within Concrete due to Drying,” Magazine of Concrete Research, V. 49, No. 179, 1997, pp. 129-137. doi: 10.1680/macr.1997.49.179.129

18. Huang, Q.; Jiang, Z.; Gu, X.; Zhang, W.; and Guo, B., “Numerical Simulation of Moisture Transport in Concrete Based on a Pore Size Distribution Model,” Cement and Concrete Research, V. 67, 2015, pp. 31-43. doi: 10.1016/j.cemconres.2014.08.003

19. Ranaivomanana, H.; Verdier, J.; Sellier, A.; and Bourbon, X., “Toward a Better Comprehension and Modeling of Hysteresis Cycles in The Water Sorption-Desorption Process for Cement Based Materials,” Cement and Concrete Research, V. 41, No. 8, 2011, pp. 817-827. doi: 10.1016/j.cemconres.2011.03.012

20. Zhang, J.; Wang, J.; and Gao, Y., “Moisture Movement in Early-Age Concrete under Cement Hydration and Environmental Drying,” Magazine of Concrete Research, V. 68, No. 8, 2016, pp. 391-408. doi: 10.1680/jmacr.15.00293

21. Ouyang, Z., and Wan, B., “Modeling of Moisture Diffusion in FRP Strengthened Concrete Specimens,” Journal of Composites for Construction, ASCE, V. 12, No. 4, 2008, pp. 425-434. doi: 10.1061/(ASCE)1090-0268(2008)12:4(425)

22. Comite Euro-International du Beton, “CEB-FIP Model Code 1990,” Lausanne, Switzerland, 1993.

23. Jafarifar, N.; Pilakoutas, K.; and Bennett, T., “Moisture Transport and Drying Shrinkage Properties of Steel–Fibre-Reinforced-Concrete,” Construction and Building Materials, V. 73, 2014, pp. 41-50. doi: 10.1016/j.conbuildmat.2014.09.039

24. Sheban, M. A.; Ayman, N. A.; and Scott, R. F., “Numerical Simulation of Moisture Diffusion in Concrete,” Joint International Conference on Computing and Decision Making in Civil and Building Engineering, Montréal, QC, Canada, 2006, pp. 1015-1024.

25. Hajibabaee, A., and Ley, M. T., “The Impact of Wet Curing on Curling in Concrete Caused by Drying Shrinkage,” Materials and Structures, V. 49, No. 5, 2016, pp. 1629-1639. doi: 10.1617/s11527-015-0600-z

26. ASTM C305-14, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2014, 3 pp.

27. ASTM C192/C192M-15, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2015, 8 pp.

28. Sensirion, “Datasheet: SHT7x_V5_C1,” Staefa, Switzerland, 2011, https://www.sensirion.com/fileadmin/user_upload/customers/sensirion/Dokumente/0_Datasheets/Humidity/Sensirion_Humidity_Sensors_SHT7x_Datasheet.pdf.

29. Grasley, Z. C.; Lange, D. A.; and D’Ambrosia, M. D., “Internal Relative Humidity and Drying Stress Gradients in Concrete,” Materials and Structures, V. 39, No. 9, 2006, pp. 901-909. doi: 10.1617/s11527-006-9090-3

30. Federal Specification TT-P-1536a (GSA-FSS), “Plumbing Fixture Setting,” 1975.

31. Gilat, A., and Subramaniam, V., Numerical Methods for Engineers and Scientists, third edition, Wiley, New York, 2008.

32. Doherty, J., Calibration and Uncertainty Analysis for Complex Environmental Models, Watermark Numerical Computing, 2015.

33. Bahremand, A., and De Smedt, F., “Parameter Sensitivity and Uncertainty Analysis of the WetSpa Model Using PEST,” Proceedings of the 2006 IASME/WSEAS Int. Conf. on Water Resources, Hydraulics & Hydrology, 2006, pp. 26-35.

34. Finsterle, S., and Zhang, Y., “Solving iTOUGH2 Simulation and Optimization Problems Using the PEST protocol,” Environmental Modelling & Software, V. 26, No. 7, 2011, pp. 959-968. doi: 10.1016/j.envsoft.2011.02.008

35. Rangelov, M., “Characterization of Chloride Diffusivity, Moisture Diffusivity, and Drying Shrinkage of Mortar as a Function Of Pore System Parameters,” PhD dissertation, Washington State University, Pullman, WA, 2018.

36. Rangelov, M., and Nassiri, S., “Empirical Time-Dependent Tortuosity Relations for Hydrating Mortar Mixtures Based on Modified Archie’s Law,” Construction & Building Materials, V. 171, 2018, pp. 825-838. doi: 10.1016/j.conbuildmat.2018.03.173

37. Manmohan, D., and Mehta, P. K., “Influence of Pozzolanic, Slag, and Chemical Admixtures on Pore Size Distribution and Permeability of Hardened Cement Pastes,” Cement, Concrete and Aggregates, V. 3, No. 1, 1981, pp. 63-67. doi: 10.1520/CCA10203J

38. Zeng, Q.; Li, K.; Fen-Chong, T.; and Dangla, P., “Pore Structure Characterization of Cement Pastes Blended with High-Volume Fly-Ash,” Cement and Concrete Research, V. 42, No. 1, 2012, pp. 194-204. doi: 10.1016/j.cemconres.2011.09.012

39. Dullien, F. A. L., Porous Media: Fluid Transport and Pore Structure, Academic Press, New York, 2012.

40. Radlinska, A.; Rajabipour, F.; Bucher, B.; Henkensiefken, R.; Sant, G.; and Weiss, W. J., “Shrinkage Mitigation Strategies in Cementitious Systems: A Closer Look at Differences in Sealed and Unsealed Behavior,” Transportation Research Record: Journal of the Transportation Research Board, V. 2070, No. 1, 2008, pp. 59-67. doi: 10.3141/2070-08

41. Juenger, M. C. G., and Siddique, R., “Recent Advances in Understanding the Role of Supplementary Cementitious Materials in Concrete,” Cement and Concrete Research, V. 78, 2015, pp. 71-80. doi: 10.1016/j.cemconres.2015.03.018

42. Maekawa, K.; Ishida, T.; and Kishi, T., Multi-Scale Modeling of Structural Concrete, CRC Press, Boca Raton, FL, 2008.


ALSO AVAILABLE IN:

Electronic Materials Journal