Title: First-Principles Approach to Water Adsorption Properties of Belite with Dopants

Author(s): R. Sakurada, Y. Hosokawa, Y. Kawazoe, R. Juneja, and A. K. Singh

Publication: Materials Journal

Volume: 117

Issue: 2

Appears on pages(s): 25-32

Keywords: belite; co-doping; first-principles study; trace impurity; water adsorption energy

DOI: 10.14359/51722393

Date: 3/1/2020

Abstract:
Belite-rich cement is beneficial to low-heat liberation, strength development at a later age, and reduction of environmental impact in clinkerization process. However, this cement has to compromise on the lower hydraulic activity at an early age. This study theoretically investigates the effect of additional incorporation of S and P atoms into Mg-doped beta-form belite (ꞵ-C2S) on the improvement of water adsorption ability of Mg-doped ꞵ-C2S having low hydraulic reactivity by first-principles calculations. The numerical simulation based on density functional theory shows that the additional co-doping of S and P into Mg-doped ꞵ-C2S dramatically enhances the absolute value of initial water adsorption energies on ꞵ-C2S surface two to four times as much as that of Mg-doped ꞵ-C2S. The contribution of S and P to reactivation is theoretically proved in PDOS analyses, and the calculation results corroborate with the strength development properties of cement paste containing the synthesized Mg-doped ꞵ-C2S with SO3 and P2O5.

Related References:

1. Chen, Y. L.; Lin, C. J.; Ko, M. S.; Lai, Y. C.; and Chang, J. E., “Characterization of Mortars from Belite-Rich Clinkers Produced from Inorganic Wastes,” Cement and Concrete Composites, V. 33, No. 2, 2011, pp. 261-266. doi: 10.1016/j.cemconcomp.2010.10.012

2. Fierence, P., and Tirlocq, J., “Nature and Concentration Effect of Stabilizing Elements of Beta-Dicalcium Silicate on Its Hydration Rate,” Cement and Concrete Research, V. 13, No. 2, 1983, pp. 267-276. doi: 10.1016/0008-8846(83)90110-2

3. Lai, G. C.; Nojiri, T.; and Nakao, K., “Studies of the Stability of ꞵ-Ca2SiO4 Doped by Minor Ions,” Cement and Concrete Research, V. 22, No. 5, 1992, pp. 743-754. doi: 10.1016/0008-8846(92)90097-F

4. Romano, J. S.; Marcato, P. D.; and Rodrigues, F. A., “Synthesis and Characterization of Manganese Oxide-Doped Dicalcium Silicates Obtained from Rice Hull Ash,” Powder Technology, V. 178, No. 1, 2007, pp. 5-9. doi: 10.1016/j.powtec.2007.03.042

5. Parkash, R.; Mehta, S. K.; Dixit, S.; Ahluwalia, S. C.; and Sharma, J. M., “Kinetics of Hydration of 2CaO•SiO2-xMn2O3 System,” Thermochimica Acta, V. 424, No. 1-2, 2004, pp. 37-42. doi: 10.1016/j.tca.2004.05.006

6. Sakurada, R.; Kawazoe, Y.; and Singh, A. K., “First-Principles Study on Structural Stability of Belite,” ACI Materials Journal, V. 112, No. 1, Jan.-Feb. 2015, pp. 85-93. doi: 10.14359/51687128

7. Sakurada, R.; Uzawa, M.; Hosokawa, Y.; Uchida, S.; Kawazoe, Y.; Manjanath, A.; and Singh, A. K., “First-Principles Study of the Effect of Trace Impurity on Initial Water Adsorption onto Belite,” Journal of Civil Engineering and Architecture Research, V. 3, No. 12, 2016, pp. 1826-1832.

8. Sakurada, R.; Uzawa, M.; Hosokawa, Y.; Uchida, S.; Kawazoe, Y.; Belosludov, R. V.; Manjanath, A.; and Singh, A. K., “Initial Water Adsorption Property of Manganese-Doped Belite by First-Principles Calculation,” Journal of Civil Engineering and Architecture Research, V. 4, No. 5, 2017, pp. 2011-2018.

9. Teoreanu, I., and Andronescu, E., “Orthosilicate Compositions in CaO-SrO-BaO-SiO2 System and Their Water Reactivity,” Proceedings of the 9th International Congress on the Chemistry of Cement, V. 2, 1992, pp. 107-113.

10. Nii-jima, S.; Ohno, M.; Kurokawa, D.; and Hirao, H., “Effects of Manufacturing Conditions on Hydration Reactivity of Synthesized C2S Solid Solution,” Cement Science and Concrete Technology, V. 68, No. 1, 2014, pp. 96-102. doi: (in Japanese)10.14250/cement.68.96

11. Amano, M., “Hydration Properties of Belite Rich Cements with Different MgO Contents,” Cement Science and Concrete Technology, V. 51, No. 1, 1997, pp. 56-62. (in Japanese)

12. Soga, R.; Merko, P.; Hayashi, K.; Hosokawa, Y.; and Uchida, S., “The Effect of Minor Elements on Clinker Minerals and Cement Hydration,” Journal of the Research of the Taiheiyo Cement Corporation, No. 172, 2017, pp. 16-29.

13. Staněk, T., and Sulovský, P., “Active Low-Energy Belite Cement,” Cement and Concrete Research, V. 68, 2015, pp. 203-210. doi: 10.1016/j.cemconres.2014.11.004

14. Ohno, M.; Nii-jima, S.; Kurokawa, D.; and Hirao, H., “Strength Improvement of High Belite Cement Containing Abundant MgO,” Cement Science and Concrete Technology, V. 70, No. 1, 2016, pp. 61-68. (in Japanese) doi: 10.14250/cement.70.61

15. Manjanath, A.; Roy, A.; Samanta, A.; and Singh, A. K., “Negative Differential Resistance in Armchair Silicene Nanoribbons,” Nanotechnology, V. 28, No. 27, 2017, pp. 275-402. doi: 10.1088/1361-6528/aa75b6

16. Singh, A. K., and Yakobson, B. I., “First Principles Calculations of H-Storage in Sorption Materials,” Journal of Materials Science, V. 47, No. 21, 2012, pp. 7356-7366. doi: 10.1007/s10853-012-6551-7

17. Wang, Q.; Li, F.; Shen, X.; Shi, W.; Li, X.; Guo, Y.; Xiong, S.; and Zhu, Q., “Relation between Reactivity and Electronic Structure for α'L-, β- and γ-dicalcium silicate: A First-Principles Study,” Cement and Concrete Research, V. 57, 2014, pp. 28-32. doi: 10.1016/j.cemconres.2013.12.004

18. Atkins, P., and Friedman, R., Molecular Quantum Mechanics, Oxford University Press, Oxford, UK, 2005, pp. 316-320.

19. Jost, K. H.; Ziemer, B.; and Seydel, R., “Redetermination of the Structure of β-Dicalcium Silicate,” Acta Crystallographica. Section B, Structural Crystallography and Crystal Chemistry, V. 33, No. 6, 1977, pp. 1696-1700. doi: 10.1107/S0567740877006918

20. Kresse, G., and Furthmüller, J., “Efficient Iterative Schemes for Ab Initio Total-Energy Calculations Using a Plane-Wave Basis Set,” Physical Review. B, V. 54, No. 16, 1996, pp. 11169-11186. doi: 10.1103/PhysRevB.54.11169

21. Blöchl, P. E., “Projector Augmented-Wave Method,” Physical Review. B, V. 50, No. 24, 1994, pp. 17953-17979. doi: 10.1103/PhysRevB.50.17953

22. Perdew, J. P.; Burke, K.; and Ernzerhof, M., “Generalized Gradient Approximation Made Simple,” Physical Review Letters, V. 77, No. 18, 1996, pp. 3865-3868. doi: 10.1103/PhysRevLett.77.3865

23. Halim, W. S. A., and Shalabi, A. S., “Surface Morphology and Interaction between Water and MgO, CaO, and SrO Surfaces Periodic HF and DFT Calculations,” Applied Surface Science, V. 221, No. 1-4, 2004, pp. 53-61. doi: 10.1016/S0169-4332(03)00620-2

24. Sasaki, K.; Wakuta, K.; Tokuda, N.; Belosludov, R. V.; Ueda, S.; Inoue, R.; Kawazoe, Y.; and Ariyama, T., “Experimental Study and Atomic Level Description of Adsorption Process of CO2 on Doped Alkaline Earth Oxides,” ISIJ International, V. 52, No. 7, 2012, pp. 1233-1240. doi: 10.2355/isijinternational.52.1233


ALSO AVAILABLE IN:

Electronic Materials Journal