Experimental Evaluation and Modeling of Corroded Reinforced Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Evaluation and Modeling of Corroded Reinforced Concrete Columns

Author(s): Hakan Yalciner and Atila Kumbasaroglu

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 61-76

Keywords: assessment; column; corrosion; reinforcement bar; seismic

DOI: 10.14359/51721372

Date: 7/1/2020

Abstract:
A total of 30 full-scale reinforced concrete (RC) columns were tested to develop models for the prediction of the structural behavior of corroded RC columns. Of these, 25 RC columns were tested under cyclic loading for two different applied axial load ratios—namely, 0.20 and 0.40—at three concrete strength levels—namely, 9, 27, and 37 MPa (1305, 3915, and 5365 psi)—and at four corrosion levels. Five RC columns were loaded monotonically with an axial load ratio of 0.20 at four corrosion levels to calculate the damage index. The actual corrosion levels were obtained by breaking the concrete and extracting all the reinforcing bars. The test results demonstrated that the ductility ratios of the corroded RC columns, which were not determined in accordance with energy-based or bilateral failure criteria, could be misleading. The determined energy dissipation capacity and damage index of the columns further revealed the corrosion effects.

Related References:

AIJ, 1997, “Recommendations for Practice of Survey, Diagnosis and Repair for Deterioration of Reinforced Concrete Structures,” Architectural Institute of Japan, Tokyo, Japan.

ASTM G1-03, 2003, “Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 9 pp.

ASTM A370-08a, 2008, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 47 pp.

Bicer, K.; Yalciner, H.; Pekrioglu Balkıs, A.; and Kumbasaroglu, A., 2018, “Effect of Corrosion on Flexural Strength of Reinforced Concrete Beams with Polypropylene Fibers,” Construction and Building Materials, V. 185, pp. 574-588. doi: 10.1016/j.conbuildmat.2018.07.021

Cağatay, I. H., 2005, “Experimental Evaluation of Buildings Damaged in Recent Earthquakes in Turkey,” Engineering Failure Analysis, V. 12, No. 3, pp. 440-452. doi: 10.1016/j.engfailanal.2004.02.007

Di Carlo, F.; Meda, A.; and Rinaldi, Z., 2017, “Numerical Evaluation of the Corrosion Influence on the Cyclic Behaviour of RC Columns,” Engineering Structures, V. 153, pp. 264-278. doi: 10.1016/j.engstruct.2017.10.020

FEMA 461, 2007, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” Federal Emergency Management Agency, Washington, DC, pp. 1-113.

Grandić, D., and Bjegović, D., 2011, “Reinforcement Corrosion Rate in Cracked Areas of RC-Members Subjected to Sustained Load,” Modelling of Corroding Concrete Structures,” RILEM, V. 5, pp. 65-83.

Guo, A.; Li, H.; Ba, X.; Guan, X.; and Li, H., 2015, “Experimental Investigation on the Cyclic Performance of Reinforced Concrete Piers with Chloride-Induced Corrosion in Marine Environment,” Engineering Structures, V. 105, pp. 1-11. doi: 10.1016/j.engstruct.2015.09.031

Li, D.; Wei, R.; Xing, F.; Sui, L.; Zhou, Y.; and Wang, W., 2018, “Influence of Non-Uniform Corrosion of Steel Bars on the Seismic Behavior of Reinforced Concrete Columns,” Construction and Building Materials, V. 167, pp. 20-32. doi: 10.1016/j.conbuildmat.2018.01.149

Liu, X.; Jiang, H.; and He, L., 2017, “Experimental Investigation on Seismic Performance of Corroded Reinforced Concrete Moment-Resisting Frames,” Engineering Structures, V. 153, pp. 639-652. doi: 10.1016/j.engstruct.2017.10.034

Ma, Y.; Che, Y.; and Gong, J., 2012, “Behavior of Corrosion Damaged Circular Reinforced Concrete Columns under Cyclic Loading,” Construction and Building Materials, V. 29, pp. 548-556. doi: 10.1016/j.conbuildmat.2011.11.002

Meda, A.; Mostosi, S.; Rinaldi, Z.; and Riva, P., 2014, “Experimental Evaluation of the Corrosion Influence on the Cyclic Behaviour of RC Columns,” Engineering Structures, V. 76, pp. 112-123. doi: 10.1016/j.engstruct.2014.06.043

Park, Y. J., and Ang, A. H. S., 1985, “Mechanistic Seismic Damage Model for Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 111, No. 4, pp. 722-739. doi: 10.1061/(ASCE)0733-9445(1985)111:4(722)

Park, Y. J.; Ang, H. S.; and Wen, Y. K., 1987, “Damage-Limiting Aseismic Design of Buildings,” Earthquake Spectra, V. 3, No. 1, pp. 1-26. doi: 10.1193/1.1585416

Sezen, H., and Moehle, J. P., 2004, “Strength and Deformation Capacity of Reinforced Concrete Columns with Limited Ductility,” Proceedings of the 13th World Conference on Earthquake Engineering, V. 279, pp. 1-15.

Shimizu, Y.; Hirosawa, M.; and Zhou, J., 2000, “Statistical Analysis of Concrete Strength in Existing Reinforced Concrete Buildings in Japan,” Department Architecture, Faculty of Engineering, Kogakuin University, Tokyo, Japan, pp. 1-88.

Sun, Z.; Si, B.; Wang, D.; and Guo, X., 2008, “Experimental Research and Finite Element Analysis of Bridge Piers Failed in Flexure-Shear Modes,” Earthquake Engineering and Engineering Vibration, V. 7, No. 4, pp. 403-414. doi: 10.1007/s11803-008-1006-5

Varum, H., 2003, “Seismic Assessment, Strengthening and Repair of Existing Buildings,” PhD Thesis, University of Aveiro, Aveiro, Portugal.

Vision 2000, 1995, “Performance Based Seismic Engineering of Buildings,” Structural Engineers Association of California, Sacramento, CA.

Yalciner, H.; Eren, O.; and Sensoy, S., 2012b, “An Experimental Study on the Bond Strength Between Reinforcement Bars and Concrete as a Function of Concrete Cover, Strength and Corrosion Level,” Cement and Concrete Research, V. 42, No. 5, pp. 643-655. doi: 10.1016/j.cemconres.2012.01.003

Yalciner, H.; Kumbasaroglu, A.; Ertuc, İ.; and Turan, A. İ., 2018, “Confinement Effect of Geo-Grid and Conventional Shear Reinforcement Bars Subjected to Corrosion,” Structures, V. 13, pp. 139-152. doi: 10.1016/j.istruc.2017.12.004

Yalciner, H.; Sensoy, S.; and Eren, O., 2012a, “Time-Dependent Seismic Performance Assessment of a Single-Degree-of-Freedom Frame Subject to Corrosion,” Engineering Failure Analysis, V. 19, pp. 109-122. doi: 10.1016/j.engfailanal.2011.09.010

Yalciner, H.; Sensoy, S.; and Eren, O., 2015, “Seismic Performance Assessment of a Corroded 50-Year-Old Reinforced Concrete Building,” Journal of Structural Engineering, ASCE, V. 141, No. 12, pp. 1-11. doi: 10.1061/(ASCE)ST.1943-541X.0001263

Yang, S. Y.; Song, X. B.; Jia, H. X.; Chen, X.; and Liu, X. L., 2016, “Experimental Research on Hysteretic Behaviors of Corroded Reinforced Concrete Columns with Different Maximum Amounts of Corrosion of Rebar,” Construction and Building Materials, V. 121, pp. 319-327. doi: 10.1016/j.conbuildmat.2016.06.002

Yuan, W.; Guo, A.; and Li, H., 2017, “Experimental Investigation on the Cyclic Behaviors of Corroded Coastal Bridge Piers with Transfer of Plastic Hinge Due to Non-Uniform Corrosion,” Soil Dynamics and Earthquake Engineering, V. 102, pp. 112-123. doi: 10.1016/j.soildyn.2017.08.019

Yuan, Y.; Ji, Y.; and Shah, S. P., 2007, “Comparison of Two Accelerated Corrosion Techniques for Concrete Structures,” ACI Structural Journal, V. 104, No. 3, May-June, pp. 344-347.

Zhang, R.; Castel, A.; and François, R., 2009, “Serviceability Limit State Criteria Based on Steel–Concrete Bond Loss for Corroded Reinforced Concrete in Chloride Environment,” Materials and Structures, V. 42, No. 10, pp. 1407-1421. doi: 10.1617/s11527-008-9460-0

Zhu, W., and François, R., 2014, “Corrosion of the Reinforcement and Its Influence on the Residual Structural Performance of a 26-Year-Old Corroded RC Beam,” Construction and Building Materials, V. 51, pp. 461-472. doi: 10.1016/j.conbuildmat.2013.11.015


ALSO AVAILABLE IN:

Electronic Structural Journal