Proposed Design Equations for Lap Splice of Glass Fiber-Reinforced Polymer Bars under Compression in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Design Equations for Lap Splice of Glass Fiber-Reinforced Polymer Bars under Compression in Concrete

Author(s): Amirhomayoon Tabatabaei, Hamdy M. Mohamed, Abolfazl Eslami, and Brahim Benmokrane

Publication: Structural Journal

Volume: 117

Issue: 2

Appears on pages(s): 291-302

Keywords: analytical model; column; compression; design equation; glass fiber-reinforced polymer (GFRP) bars; lap splice

DOI: 10.14359/51721370

Date: 3/1/2020

Abstract:
This paper presents the results of an experimental and analytical investigation of the splice length of glass fiber-reinforced polymer (GFRP) bars under compression in concrete. The experimentation comprises 29 full-scale circular concrete columns. The experimental parameters evaluated in this study were composed of the compressive strength of concrete, bar diameter, splice length, and amount of transverse reinforcement. The experimental results indicated that the requisite splice length of GFRP bars would be less than that of steel. In addition, the bond strength of GFRP bars to concrete was improved by increasing the bar diameter of transverse reinforcement and compressive strength of concrete. Reducing the spacing of transverse reinforcement and longitudinal bar diameter can also lead to decreasing the splice length. However, splice length was independent of the ultimate strength of transverse reinforcement. The obtained experimental data of the present study was augmented with the results of 39 additional specimens collected from the literature to develop design recommendations for lap splicing of GFRP bars under compression. In addition, a relation for splice length was derived by applying methodologies similar to those already used for steel bars. The proposed equation for design purpose of the splice length of GFRP bars under compression was found to be in a reliable agreement with the available experimental data.

Related References:

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318M-14) and Commentary (ACI 318RM-14),” American Concrete Institute, Farmington Hills, MI, 520 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., 2014, “Axial Capacity of Circular Concrete Columns Reinforced with GFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 1, pp. 1-11. doi: 10.1061/(ASCE)CC.1943-5614.0000438

Aly, R.; Benmokrane, B.; and Ebead, U., 2006, “Tensile Lap Splicing of Bundled CFRP Reinforcing Bars in Concrete,” Journal of Composites for Construction, ASCE, V. 10, No. 4, pp. 287-294. doi: 10.1061/(ASCE)1090-0268(2006)10:4(287)

Benmokrane, B.; Tighiouart, B.; and Chaallal, O., 1996, “Bond Strength and Load Distribution of Composite GFRP Reinforcing Bars in Concrete,” ACI Materials Journal, V. 93, No. 3, May-June, pp. 246-253.

Cairns, J., 1985, “Strength of Compression Splices: A Reevaluation of Test Data,” ACI Journal Proceedings, V. 82, No. 4, July-Aug., pp. 510-516.

Cairns, J., and Arthur, P. D., 1979, “Strength of Lapped Splices in Reinforced Concrete Columns,” ACI Journal Proceedings, V. 76, No. 2, Feb., pp. 277-296.

Canbay, E., and Frosch, R. J., 2005, “Bond Strength of Lap-Spliced Bars,” ACI Structural Journal, V. 102, No. 4, July-Aug., pp. 605-614.

CAN/CSA A23.3-14, 2014, “Design of Concrete Structures,” Canadian Standards Association, Mississauga, ON, Canada.

CAN/CSA S6-14, 2014, “Canadian Highway Bridge Design Code,” Canadian Standards Association, Mississauga, ON, Canada.

CAN/CSA S806-12, 2012, “Design and Construction of Building Structures with Fiber Reinforced Polymers,” Canadian Standards Association, Mississauga, ON, Canada.

Chun, S., 2017, “Components of Compression Splice Resistances in High-Strength Concrete,” Magazine of Concrete Research, V. 69, No. 10, pp. 502-511. doi: 10.1680/jmacr.16.00412

Chun, S.; Lee, S.; and Oh, B., 2010a, “Compression Splices in Confined Concrete of 40 and 60 MPa (5800 and 8700 psi) Compressive Strengths,” ACI Structural Journal, V. 107, No. 4, July-Aug., pp. 1-10.

Chun, S.; Lee, S.; and Oh, B., 2010b, “Compression Lap Splice in Unconfined Concrete of 40 and 60 MPa (5800 and 8700 psi) Compressive Strengths,” ACI Structural Journal, V. 107, No. 2, Mar.-Apr., pp. 170-178.

Chun, S.; Lee, S.; and Oh, B., 2011, “Compression Splices in High-Strength Concrete of 100 MPa (14,500 psi) and Less,” ACI Structural Journal, V. 108, No. 6, Nov.-Dec., pp. 715-724.

Darwin, D.; Tholen, M. L.; Idun, E. K.; and Zuo, J., 1996a, “Bond Strength of High Relative Rib Area Reinforcing Bars,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb., pp. 95-107.

Darwin, D.; Zuo, J.; Tholen, M. L.; and Idun, E. K., 1996b, “Development Length Criteria for Conventional and High Relative Rib Area Reinforcing Bars,” ACI Structural Journal, V. 93, No. 3, May-June, pp. 347-359.

De Luca, A.; Matta, F.; and Nanni, A., 2010, “Behavior of Full-Scale Glass Fiber-Reinforced Polymer Reinforced Concrete Columns under Axial Load,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct., pp. 589-596.

Ehsani, M. R.; Saadatmanesh, H.; and Tao, S., 1996, “Design Recommendations for Bond of GFRP Rebars to Concrete,” Journal of Structural Engineering, ASCE, V. 122, No. 3, pp. 247-254. doi: 10.1061/(ASCE)0733-9445(1996)122:3(247)

Elinea, A.; Yehia, S.; and Tadros, M. K., 1999, “Lap Splices in Confined Concrete,” ACI Structural Journal, V. 96, No. 6, Nov.-Dec., pp. 937-946.

Ferguson, P. M., and Breen, J. E., 1965, “Lapped Splices for High Strength Reinforcing Bars,” ACI Journal Proceedings, V. 62, No. 9, Sept., pp. 1063-1078.

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017a, “Failure Envelope of Circular Concrete Columns Reinforced with Glass Fiber-­Reinforced Polymer Bars and Spirals,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec., pp. 1417-1428. doi: 10.14359/51689498

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017b, “Experimental Study of Circular High-Strength Concrete Columns Reinforced with GFRP Bars and Spirals under Concentric and Eccentric Loading,” Journal of Composites for Construction, ASCE, V. 21, No. 2.

Hadhood, A.; Mohamed, H. M.; Ghrib, F.; and Benmokrane, B., 2017c, “Efficiency of Glass-Fiber Reinforced-Polymer (GFRP) Discrete Hoops and Bars in Concrete Columns under Combined Axial and Flexural Loads,” Composites. Part B, Engineering, V. 114, pp. 223-236. doi: 10.1016/j.compositesb.2017.01.063

Hales, T. A.; Pantelides, C. P.; Sankholkar, P.; and Reaveley, L. D., 2017, “Analysis-Oriented Stress-Strain Model for Concrete Confined with Fiber-Reinforced Polymer Spirals,” ACI Structural Journal, V. 114, No. 5, Sept.-Oct., pp. 1263-1272. doi: 10.14359/51689788

Intelligent Sensing for Innovative Structures, 2007, “Reinforcing Concrete Structures with Fibre Reinforced Polymers,” ISIS-Canada Design Manual No. 3, University of Manitoba, Winipeg, MB, Canada, 31 pp.

Joint ACI-ASCE Committee 408, 2003, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03),” American Concrete Institute, Farmington Hills, MI, 49 pp.

JSCE Guideline for Concrete No, 15, 2007, “Standard Specifications for Concrete Structures: Design,” Japan Society of Civil Engineers, Tokyo, Japan.

Orangun, C. O.; Jirsa, J. O.; and Breen, J. E., 1977, “A Reevaluation of Test Data on Development Length and Splices,” ACI Journal Proceedings, V. 74, No. 3, Mar., pp. 114-122.

Park, R., and Paulay, T., 1974, Reinforced Concrete Structures, John Wiley & Sons Inc., New York.

Pay, C.; Canbay, E.; and Frosch, R. J., 2014, “Bond Strength of Spliced Fiber-Reinforced Polymer Reinforcement,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr., pp. 257-266.

Pfister, J. P., and Mattock, A. H., 1963, “High Strength Bars as Concrete Reinforcement, Part 5: Lap Splices in Concentrically Loaded Columns,” Journal of the PCA Research and Development Laboratories, V. 5, No. 2, pp. 27-40.

Russo, G.; Pauletta, M.; and Mitri, D., 2009, “Solution for Bond Distribution in Asymmetric R. C. Structural Members,” Engineering Structures, V. 31, No. 3, pp. 633-641. doi: 10.1016/j.engstruct.2008.11.003

Saatcioglu, B. M., and Razvi, S. R., 1992, “Strength and Ductility of Confined Concrete,” Journal of Structural Engineering, ASCE, V. 118, No. 6, pp. 1590-1607. doi: 10.1061/(ASCE)0733-9445(1992)118:6(1590)

Tighiouart, B.; Benmokrane, B.; and Gao, D., 1998, “Investigation of Bond in Concrete Member with Fibre Reinforced Polymer (FRP) Bars,” Construction and Building Materials, V. 12, No. 8, pp. 453-462. doi: 10.1016/S0950-0618(98)00027-0

Tighiouart, B.; Benmokrane, B.; and Mukhopadhyaya, P., 1999, “Bond Strength of Glass FRP Rebar Splices in Beams under Static Loading,” Construction and Building Materials, V. 13, No. 7, pp. 383-392. doi: 10.1016/S0950-0618(99)00037-9

Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2012, “Concrete Columns Reinforced Longitudinally and Transversally with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 109, No. 4, July-Aug., pp. 551-558.

Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2014, “Strength Model for Concrete Columns Reinforced with Fiber-Reinforced Polymer Bars and Ties,” ACI Structural Journal, V. 111, No. 4, July-Aug., pp. 789-798. doi: 10.14359/51686630

Wambeke, B. W., and Shield, C. K., 2006, “Development Length of Glass Fiber-Reinforced Polymer Bars in Concrete,” ACI Structural Journal, V. 103, No. 1, Jan.-Feb., pp. 11-17.

Wight, J. K., and MacGregor, J. G., 2012, Reinforced Concrete: Mechanics and Design, sixth edition, Pearson, London, UK.

Zadeh, H. J., and Nanni, A., 2013, “Design of RC Columns Using Glass FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 294-304. doi: 10.1061/(ASCE)CC.1943-5614.0000354

Zuo, J., and Darwin, D., 2000, “Splice Strength of Conventional and High Relative Rib Area Bars in Normal and High-Strength Concrete,” ACI Structural Journal, V. 97, No. 4, July-Aug., pp. 630-641.