Detrimental Effects of Anti-Icing Brines on Concrete Durability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Detrimental Effects of Anti-Icing Brines on Concrete Durability

Author(s): Colin B. Van Niejenhuis and Carolyn M. Hansson

Publication: Concrete International

Volume: 41

Issue: 11

Appears on pages(s): 30-34

Keywords: chloride, salt, cylinder, strength

DOI: 10.14359/51721346

Date: 11/1/2019

Abstract:
Sodium chloride, calcium chloride, or magnesium chloride anti-icing brines are more efficient at preventing ice build-up on roads than rock salt crystals. However, as shown in various studies, they can be detrimental to concrete and promote scaling or joint deterioration. This article presents results of a 5-year evaluation of mechanical properties of concrete cylinders immersed in four anti-icing brines and tested in compression.

Related References:

1. “Code of Practice: Road Salts Environmental Management,” Government of Canada, Oct. 30, 2018. https://www.canada.ca/en/environment-climate-change/services/pollutants/road-salts/code-practiceenvironmental-management.html.

2. Lilek, J., “Roadway Deicing in the United States,” Factsheet 2017-003, American Geosciences Institute, Alexandria, VA, July 2017, 2 pp.

3. Oswald, C.J.; Giberson, G.; Nicholls, E.; Wellen, C.; and Oni, S., “Spatial Distribution and Extent of Urban Land Cover Control Watershed-Scale Chloride Retention,” Science of the Total Environment, V. 652, Feb. 2019, pp. 278-288.

4. Sutter, L.; Peterson, K.; Touton, S.; Van Dam, T.; and Johnston, D., “Petrographic Evidence of Calcium Oxychloride Formation in Mortars Exposed to Magnesium Chloride Solution,” Cement and Concrete Research, V. 36, No. 8, Aug. 2006, pp. 1533-1541.

5. Suraneni, P.; Monical, J.; Unal, E.; Farnam, Y.; and Weiss, J., “Calcium Oxychloride Formation Potential in Cementitious Pastes Exposed to Blends of Deicing Salt,” ACI Materials Journal, V. 114, No. 4, July-Aug. 2017, pp. 631-641.

6. Ghazy, A., and Bassuoni, M.T., “Resistance of Concrete to Different Exposures with Chloride-Based Salts,” Cement and Concrete Research, V. 101, Nov. 2017, pp. 144-158.

7. Hunt, M.J., and Hansson, C.M., “The Influence of the Cations in Anti-Icing Brines on the Corrosion of Reinforcing Steel in Synthetic Concrete Pore Solution,” Corrosion, V. 71, No. 6, June 2015, pp. 749-757.

8. Hansson, C.M.; Frølund, T.; and Markussen, J.B., “The Effect of Chloride Cation Type on the Corrosion of Steel in Concrete by Chloride Salts,” Cement and Concrete Research, V. 15, No. 1, Jan. 1985, pp. 65-73.

9. Poursaee, A.; Laurent, A.; and Hansson, C.M., “Corrosion of Steel Bars in OPC Mortar Exposed to NaCl, MgCl2 and CaCl2: Macro- and Micro-Cell Corrosion Perspective,” Cement and Concrete Research, V. 40, No. 3, Mar. 2010, pp. 426-430.

10. Wu, Z.; Shi, C.; Gao, P.; Wang, D.; and Cao, Z., “Effects of Deicing Salts on the Scaling Resistance of Concrete,” Journal of Materials in Civil Engineering, V. 27, No. 5, May 2015.

11. Suraneni, P.; Azad, V.J.; Isgor, O.B.; and Weiss, W.J., “Deicing Salts and Durability of Concrete Pavements and Joints,” Concrete International, V. 38, No. 4, Apr. 2016, pp. 48-54.

12. Chatterji, S., “Mechanism of the CaCl2 Attack on Portland Cement Concrete,” Cement and Concrete Research, V. 8, No. 4, July 1978, pp. 461-467.

13. Julio-Betancourt, G.A., “Effect of De-icer and Anti-icer Chemicals on the Durability, Microstructure, and Properties of Cement-Based Materials,” PhD dissertation, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 2009, 854 pp.

14. Suraneni, P.; Azad, V.J.; Isgor, O.B.; and Weiss, W.J., “Calcium Oxychloride Formation in Pastes Containing Supplementary Cementitious Materials: Thoughts on the Role of Cement and Supplementary Cementitious Materials Reactivity,” RILEM Technical Letters, V. 1, 2016, pp. 24-30.

15. De Weerdt, K.; Colombo, A.; Coppola, L.; Justnes, H.; and Geiker, M.R., “Impact of the Associated Cation on Chloride Binding of Portland Cement Paste,” Cement and Concrete Research, V. 68, Feb. 2015, pp. 196-202.

16. Shi, X.; Fay, L.; Galloway, C.; Volkening, K.; Peterson, M.M.; Pan, T.; Creighton, A.; Lawlor, C.; Mumma, S.; Liu, Y.; and Nguyen, T.A., “Evaluation of Alternative Anti-icing and Deicing Compounds Using Sodium Chloride and Magnesium Chloride as Baseline Deicers—Phase I,” Report No. CDOT-2009-1, Colorado Department of Transportation, Denver, CO, 2009, 292 pp.

17. Cremasco, M.J., and Hansson, C.M., “Effects of Anti-icing Agents on the Durability of Concrete,” Corrosion of Reinforcing Steel in Concrete—Future Direction, SP-294, M.S. Khan, ed., 2013, pp. 59-75.

18. Hong, K., and Hooton, R.D., “Effects of Cyclic Chloride Exposure on Penetration of Concrete Cover,” Cement and Concrete Research, V. 29, No. 9, Sept. 1999, pp. 1379-1386.

19. Collepardi, M.; Coppola, L.; and Pistolesi, C., “Durability of Concrete Structures Exposed to CaCl2 Based Deicing Salts, Durability of Concrete, SP-145, V.M. Malhotra, ed., 1994, pp. 107-120.

20. Otsuki, N.; Nagataki, S.; and Nakashita, K., “Evaluation of AgNO3 Solution Spray Method for Measurement of Chloride Penetration into Hardened Cementitious Matrix Materials,” Construction and Building Materials, V. 7, No. 4, Dec. 1993, pp. 195-201.

21. Monticellie, C.; Criado, M.; Fajardo, S.; Bastidas, J.M.; Abbottoni, M.; and Balbo, A., “Corrosion Behaviour of a Low Ni Austenitic Stainless Steel in Carbonated Chloride-Polluted Alkali-Activated Fly Ash Mortar,”