Special Moment Frames with High-Strength Reinforcement—Part 2: Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Special Moment Frames with High-Strength Reinforcement—Part 2: Columns

Author(s): Drit Sokoli, Albert Limantono, and Wassim M. Ghannoum

Publication: Structural Journal

Volume: 117

Issue: 2

Appears on pages(s): 253-265

Keywords: high-strength reinforcement; nominal Grade 100 reinforcement; rotation capacity; special moment frame columns; spread of plasticity

DOI: 10.14359/51721319

Date: 3/1/2020

Abstract:
High-strength reinforcing bars (HSRB) with a yield strength of at least 80 ksi (550 MPa) are currently under development in the United States, and are being considered for implementation in the ACI 318 Building Code. The laboratory tests presented in this publication were conducted to support the initiative of introducing these higher-strength bars into ACI 318-19. The primary focus of the testing program was to uncover any major issues in the performance of HSRB in concrete members, and more specifically to assess the influence of the tensile-to-yield strength (T/Y) ratio, fracture elongation, and shape of stress-strain curve of HSRB on the behavior of seismically detailed concrete columns. Four specimens were tested under constant axial load and reverse cyclic lateral loading of increasing amplitudes until fracture of longitudinal bars. Three columns were reinforced with Grade 100 (690 MPa) bars sourced from different manufacturers and therefore having different post-yield mechanical properties. The fourth column was reinforced with conventional Grade 60 (420 MPa) ASTM A706 bars. Concrete columns reinforced with HSRB reached similar lateral drift levels as the specimen reinforced with Grade 60 bars before significant loss in lateral strength. Longitudinal bars with higher T/Y ratios achieved greater plasticity spread and lower strain concentrations compared with those having lower T/Y ratios.

Related References:

1. ASTM A706/A706M-16, “Standard Specification for Deformed and Plain Low-Alloy Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

2. Slavin, C. M., “Defining Structurally Acceptable Properties of High-Strength Steel Bars through Material Testing,” master’s thesis, University of Texas at Austin, Austin, TX, 2015, 136 pp.

3. Hoggsett, G. S., “Defining Structurally Acceptable Properties of High-Strength Reinforcing Bars through Low-Cycle Fatigue Testing,” master’s thesis, University of Texas at Austin, Austin, TX, 2017, 118 pp.

4. Macchi, G.; Pinto, P. E.; and Sanpaolesi, L., “Ductility Requirements for Reinforcement under Eurocodes,” Structural Engineering International, 1996, pp. 249-254.

5. Aoyama, H., Design of Modern Highrise Reinforced Concrete Structures, Imperial College Press, London, UK, 2001.

6. ATC-115, “Roadmap for the Use of High-Strength Reinforcement in Reinforced Concrete Design,” Applied Technology Council, Redwood City, CA, 2015, 197 pp.

7. NIST, “Use of High-Strength Reinforcement in Earthquake-Resistant Concrete Structures (GCR 14-917-30),” NEHRP Consultants Joint Venture, National Institute of Standards and Technology, Gaithersburg, MD, 2014, 231 pp.

8. Sokoli, D., “Seismic Performance of Concrete Columns Reinforced with High Strength Steel,” master’s thesis, University of Texas at Austin, Austin, TX, 2014, 166 pp.

9. Sokoli, D., and Ghannoum, W. M., “High-Strength Reinforcement in Columns under High Shear Stresses,” ACI Structural Journal, V. 113, No. 3, May-June 2016, doi: 10.14359/51688203

10. Slavin, C. M., and Ghannoum, W. M., “Defining Structurally Acceptable Properties of High-Strength Steel Bars through Material and Column Testing, Part I: Material Testing Report,” (05-14), Charles Pankow Foundation, Aug. 2015, 135 pp. http://www.pankowfoundation.org/download.cfm?ID=282

11. Ghannoum, W. M., and Slavin, C. M., “Low-Cycle Fatigue Performance of High-Strength Steel Reinforcing Bars,” ACI Materials Journal, V. 113, No. 6, Nov.-Dec. 2016, doi: 10.14359/51689116

12. Restrepo, J. I.; Seible, F.; Stephan, B.; and Schoettler, M. J., “Seismic Testing of Bridge Columns Incorporating High-Performance Materials,” ACI Structural Journal, V. 103, No. 4, July-Aug. 2006, pp. 496-504.

13. Rautenberg, J. M.; Pujol, S.; Tavallali, H.; and Lepage, A., “Drift Capacity of Concrete Columns Reinforced with High-Strength Steel,” ACI Structural Journal, V. 110, No. 2, Mar.-Apr. 2013, pp. 307-318.

14. Tavallali, H.; Lepage, A.; Rautenberg, J. M.; and Pujol, S., “Concrete Beams Reinforced with High-Strength Steel Subjected to Displacement Reversals,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct. 2014, pp. 1037-1048, doi: 10.14359/51686967

15. Zhao, D. S., and Ghannoum, W. M., “Setting Bar-Bending Requirements for High-Strength Steel Bars,” (01-15), Charles Pankow Foundation, 2016, 92 pp., http://www.pankowfoundation.org/download.cfm?ID=297

16. Sokoli, D.; Limantono, A.; and Ghannoum, W. M., “Defining Structurally Acceptable Properties of High-Strength Steel Bars through Material and Column Testing, Part II: Column Testing Report,” (05-14), Charles Pankow Foundation, Aug. 2017, 219 pp., http://www.pankowfoundation.org/grants.cfm?prodonly=1

17. To, D. V., and Moehle, J. P., “Seismic Performance Characterization of Beams with High-Strength Reinforcement (06-14),” Charles Pankow Foundation, 2017, 140 pp.

18. Huq, M. S.; Weber-Kamin, A. S.; Ameen, S.; Lequesne, D. R.; and Lepage, A., “High-Strength Steel Bars in Reinforced Concrete Walls: Influence of Steel Mechanical Properties on Deformation Capacity (04-14),” Charles Pankow Foundation, 2017, 311 pp., http://www.pankowfoundation.org/download.cfm?ID=319

19. Puranam, A., and Pujol, S., “Minimum Flexural Reinforcement in Reinforced Concrete Walls,” 16th World Conference on Earthquake Engineering, 16WCEE, Chile, 2017.

20. ASTM A1035/A1035M-16b, “Standard Specification for Deformed and Plain, Low-Carbon, Chromium, Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

21. MMFX Technologies Corporation, “Material Properties and Design Considerations MMFX2 (ASTM A1035/AASHTO MP18),” MMFX Product Information, Dec. 2012, 36 pp.

22. Park, R., and Paulay, T., Reinforced Concrete Structures, Wiley, New York, 1975.

23. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

24. ASTM C39/C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

25. ASTM A370-17a, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2017, 50 pp.

26. ASTM E8/E8M-16a, “Standard Test Methods for Tension Testing of Metallic Materials,” ASTM International, West Conshohocken, PA, 2016.

27. Federal Emergency Management Agency (FEMA), “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” FEMA-461, Federal Emergency Management Agency, Washington, DC, 2007, 138 pp.

28. Sokoli, D.; Shekarchi, W.; Buenrostro, E.; and Ghannoum, W. M., “Advancing Behavioral Understanding and Damage Evaluation of Concrete Members Using High-Resolution Digital Image Correlation Data,” Earthquakes and Structures, V. 7, No. 5, 2014, pp. 609-626. doi: 10.12989/eas.2014.7.5.609

29. Wight, J. K., and Sozen, M., “Shear Strength Decay in Reinforced Concrete Columns Subjected to Large Deflections,” The National Science Foundation, Research Grant 30760X, Urbana, IL, 1973, 308 pp.

30. ASCE/SEI 41-17, “Seismic Rehabilitation of Existing Buildings,” ASCE/SEI Standard 41-17, American Society of Civil Engineering, Reston, VA, 2017.

31. Elwood, K. J., and Eberhard, M. O., “Effective Stiffness of Reinforced Concrete Columns,” ACI Structural Journal, V. 106, No. 4, July-Aug. 2009, pp. 476-484.

32. ASCE/SEI 41-13, “Seismic Rehabilitation of Existing Buildings,” ASCE/SEI Standard 41-13, American Society of Civil Engineering, Reston, VA.


ALSO AVAILABLE IN:

Electronic Structural Journal