Drop-Weight Testing on Concrete Beams and ACI Design Equations for Maximum and Residual Deflections under Low-Velocity Impact

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Drop-Weight Testing on Concrete Beams and ACI Design Equations for Maximum and Residual Deflections under Low-Velocity Impact

Author(s): Andrew Nghiem and Thomas H.-K. Kang

Publication: Structural Journal

Volume: 117

Issue: 2

Appears on pages(s): 199-210

Keywords: ACI design equation; drop-weight testing; fiber-reinforced concrete beams; prestressed concrete beams; reinforced concrete beams

DOI: 10.14359/51721316

Date: 3/1/2020

Abstract:
A thorough review was performed to outline the general procedures used for performing drop-weight testing on concrete beam members. Highlights of this review include the problems associated with early tests and the methods used to overcome them, which have now become standard practice. The findings of various types of concrete beams under low-velocity impact have also been examined. These include the impact behavior of conventionally reinforced, fiber-reinforced, and prestressed concrete beams. Next, a database of various concrete beam types has been carefully built for the development and discussion of observed trends. When applicable, comparison of the recorded drop-weight behavior of conventional reinforced concrete (RC) beams was aggregated to its ACI design capacity. Finally, empirical relations for both flexural-and shear-critical members are suggested, with applicability to the ACI design standard.

Related References:

1. Bentur, A.; Mindess, S.; and Banthia, N., “The Behaviour of Concrete Under Impact Loading: Experimental Procedures and Method of Analysis,” Materials and Structures, V. 19, No. 5, 1986, pp. 371-378. doi: 10.1007/BF02472127

2. Tachibana, S., Masuya, H., and Nakamura, S., “Performance Based Design of Reinforced Concrete Beams under Impact,” Natural Hazards and Earth System Sciences, V. 10, No. 6, 2010.

3. Adhikary, S. D.; Li, B.; and Fujikake, K., “Residual Resistance of Impact-damaged Reinforced Concrete Beams,” Magazine of Concrete Research, V. 67, No. 7, 2015, pp. 364-378. doi: 10.1680/macr.14.00312

4. Chen, Y., and May. I., M., “Reinforced Concrete Members under Drop-weight Impacts,” Structures and Buildings, V. 162, No. 1, 2009.

5. Kishi, N.; Nakano, O.; Matsuoka, K. G.; and Ando, T., “Experimental Study on Ultimate Strength of Flexural-Failure-Type RC Beams under Impact Loading,” Transactions of the 16th International Conference on Structural Mechanics in Reactor Technology, Washington, DC, 2001.

6. Kishi, N.; Mikami, H.; and Ando, T., “Impact-Resistance Behavior of Shear-Failure-Type RC Beams under Falling-Weight Impact Loading,” Structures under Shock and Impact VII, Witpress New Forest, England, 2002.

7. Kishi, N., and Mikami, H., “Empirical Formulas for Designing Reinforced Concrete Beams under Impact Loading,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 509-520.

8. Mindess, S., and Bentur, A., “A Preliminary Study of the Fracture of Concrete Beams under Impact Loading, Using High Speed Photography,” Cement and Concrete Research, V. 15, No. 3, 1985, pp. 474-484. doi: 10.1016/0008-8846(85)90121-8

9. Pham, T. M., and Hao, H., “Impact Behavior of FRP-Strengthened RC Beams without Stirrups,” Journal of Composites for Construction, ASCE, V. 20, No. 4, 2016, p. 04016011 doi: 10.1061/(ASCE)CC.1943-5614.0000671

10. Mindess, S.; Banthia, N.; and Bentur, A., “The Response of Reinforced Concrete Beams with a Fibre Matrix to Impact Loading,” International Journal of Cement Composites and Lightweight Concrete, V. 8, No. 3, 1986.

11. Banthia, N.; Yan, C.; and Sakai, K., “Impact Resistance of Fiber Reinforced Concrete at Subnormal Temperatures,” Cement and Concrete Composites, V. 20, No. 5, 1998.

12. Sukontasukkul, P., and Mindess, S., “The Shear Fracture of Concrete under Impact Loading Using End Confined Beams,” Materials and Structures, V. 36, No. 6, 2003, pp. 372-378. doi: 10.1007/BF02481062

13. Soleimani, S. M.; Banthia, N.; and Mindess, S., “Sprayed GFRP Shear-Strengthened Reinforced Concrete Beams under Impact Loading,” Advances in Construction Materials, 2007, pp. 279-286.

14. Wu, M.; Zhang, C.; and Chen, Z., “Drop-weight Tests of Concrete Beams Prestressed with Unbonded Tendons and Meso-scale Simulation,” International Journal of Impact Engineering, V. 93, 2016, p. 93 doi: 10.1016/j.ijimpeng.2016.02.011

15. Yoo, D.-Y.; Banthia, N.; and Yoon, Y.-S., “Impact Residence of Reinforced of Ultra-High-Performance Concrete Beams with Different Steel Fibers,” ACI Structural Journal, V. 114, No. 1, Jan.-Feb. 2017, pp. 113-124. doi: 10.14359/51689430

16. Ulzurrun, S. D. G., and Zanuy, C., “Enhancement of Impact Performance of Reinforced Concrete Beams without Stirrups by Adding Steel Fiber,” Construction and Building Materials, V. 145, No. 1, 2017, pp. 166-182. doi: 10.1016/j.conbuildmat.2017.04.005

17. Ishikawa, N.; Katsuki, S.; and Takemoto, K., “Dynamic Analysis of Prestressed Concrete Beams under Impact and High Speed Loadings,” N. Jones, C. A. Brebbia, and A. M. Rejendran, eds., Structures under Shock and Impact VI, Witpress, New Forest, UK, 2000.

18. Fujikake, K.; Li, B.; and Soeun, S., “Impact Response of Reinforced Concrete Beam and its Analytical Evaluation,” Journal of Structural Engineering, ASCE, V. 135, No. 8, 2009, pp. 938-950. doi: 10.1061/(ASCE)ST.1943-541X.0000039

19. Adhikary, S. D.; Li, B.; and Fujikake, K., “State-of-the-Art Review on Low-Velocity Impact Response of Reinforced Concrete Beams,” Magazine of Concrete Research, V. 68, No. 14, 2016, pp. 701-723. doi: 10.1680/jmacr.15.00084

20. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

21. Naaman, A. E., and Gopalaratnam, V. S., “Impact Properties of Steel Fibre Reinforced Concrete in Bending,” International Journal of Cement Composites and Lightweight Concrete, V. 5, No. 4, 1983.

22. Bhatti, A. Q.; Kishi, N.; Mikami, H.; and Ando, T., “Elasto-Plastic Impact Response Analysis of Shear-Failure-Type RC Beams with Shear Rebars,” Materials & Design, V. 30, No. 3, 2009

23. Barr, B., and Baghli, A., “A Repeated Drop-weight Impact Testing Apparatus for Concrete,” Magazine of Concrete Research, V. 40, No. 144, 1988, pp. 167-176. doi: 10.1680/macr.1988.40.144.167

24. Shafei, E., and Kabir, M. Z., “Effects of CFRP Retrofit on Impact Response of Shear-deficient Scaled Reinforced Concrete Beams,” Latin American Journal of Solids and Structures, V. 12, No. 1, 2015, pp. 60-76. doi: 10.1590/1679-78251290

25. Kishi, N.; Ikeda, K.; Mikami, H.; and Yamaguchi, E., “Dynamic Behaviour of RC Beams under Steel Weight Impact Loading—Effects of Nose-Shaped of Steel Weight,” 3rd International Conference on Concrete under Severe Conditions, Vancouver, BC, Canada, 2001.

26. Ishikawa, N.; Katsuki, S.; and Takemoto, K., “Incremental Impact Tests and Simulation of Prestressed Concrete Beam,” N. Jones, C. A. Brebbia, and A. M. Rejendran, eds., Structures under Shock and Impact VII, Witpress, New Forest, UK, 2002.

27. Hughes, B., and Ai-Dafiry, H., “Impact Energy Absorption at Contact Zone and Supports of Reinforced Plain and Fibrous Concrete Beams,” Construction and Building Materials, V. 9, No. 4, 1995, pp. 239-244. doi: 10.1016/0950-0618(95)00026-C

28. Kishi, N.; Mikami, H.; Matsuoka, K. G.; and Ando, T., “Impact Behavior of Shear-failure-type RC Beams Without Shear Rebar,” International Journal of Impact Engineering, V. 27, No. 9, 2002, pp. 955-968. doi: 10.1016/S0734-743X(01)00149-X

29. Tang, T., and Saadatmanesh, H., “Analytical and Experimental Studies of Fiber-Reinforced Polymer-Strengthened Concrete Beams under Impact Loading,” ACI Structural Journal, V. 102, No. 1, Jan.-Feb. 2005, pp. 139-149.

30. Fujikake, K.; Senga, T.; Ueda, N.; Ohno, T.; and Katagiri, M., “Study on Impact Response of Reactive Powder Concrete Beam and Its Analytical Model,” Journal of Advanced Concrete Technology, V. 4, No. 1, 2006, pp. 99-108. doi: 10.3151/jact.4.99

31. Soleimani, S. M.; Banthia, N.; and Mindess, S., “Behavior of RC Beams under Impact Loading: Some New Findings,” Proceedings of the 6th International Conference on Fracture Mechanics of Concrete and Concrete Structures, Catania, Italy, 2007.

32. Saatci, S., and Vecchio, F. J., “Effects of Shear Mechanisms on Impact Behavior of Reinforced Concrete Beams,” ACI Structural Journal, V. 106, No. 1, Jan.-Feb. 2009, pp. 78-86.

33. Zhang, X. X.; Ruiz, G.; and Yu, R. C., “A New Drop-weight Impact Machine for Studying Fracture Processes in Structural Concrete,” Strain, V. 46, No. 3, 2010, pp. 252-257. doi: 10.1111/j.1475-1305.2008.00574.x

34. Soleimani, S., and Banthia, N., “Impact Resistance of Shear-strengthened RC Beams with Sprayed GFRP,” International Journal of GEOMATE, V. 1, No. 2, 2011.

35. Hao, Y.; Hao, H.; and Chen, G., “Experimental Investigation of the Behaviour of Spiral Steel Fibre Reinforced Concrete Beams Subjected to Drop-Weight Impact Loads,” Materials and Structures, V. 49, No. 1-2, 2014, pp. 353-370. doi: 10.1617/s11527-014-0502-5

36. Wu, M.; Chen, Z.; and Zhang, C., “Determining the Impact Behavior of Concrete Beams Through Experimental Testing and Meso-Scale Simulation: I. Drop Weight Tests,” Engineering Fracture Mechanics, V. 135, No. 1, 2015, pp. 94-112. doi: 10.1016/j.engfracmech.2014.12.019

37. Pham, T. M., and Hao, H., “Behavior of FRP Strengthened RC Beams under Static and Impact Loads,” International Journal of Protective Structures, V. 8, No. 1, 2017.

38. Goldston, M.; Remennikov, A.; and Sheikh, M. N., “Experimental Investigation of the Behaviour of Concrete Beams Reinforced with GFRP Bars under Static and Impact Loading,” Engineering Structures, V. 113, 2016, pp. 113. doi: 10.1016/j.engstruct.2016.01.044

39. Chorzepa, M. G.; Masud, M.; Yaghoobi, A.; and Jiang, H., “Impact Test: Multiscale Fiber-Reinforced Concrete Including Polypropylene and Steel Fibers,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec. 2017, pp. 1429-1444. doi: 10.14359/51700832

40. Liu, T., and Xiao, Y., “Impact Behavior of CFRP-strip-wrapped RC Beams without Stirrups,” Journal of Composites for Construction, ASCE, V. 21, No. 5, 2017, pp. 04017035. doi: 10.1061/(ASCE)CC.1943-5614.0000815

41. Huo, J.; Li, Z.; Zhao, L.; and Xia, Y., “Dynamic Behavior of Carbon Fiber-Reinforced Polymer-Strengthened Reinforced Concrete Beams Without Stirrups Under Impact Loading,” ACI Structural Journal, V. 115, No. 3, May 2018, pp. 775-787. doi: 10.14359/51701283

42. Ishikawa, N.; Enrin, H.; Katsuki, S.; and Ohta, T., “Dynamic Behavior of Prestressed Concrete Beams under Rapid Speed Loading,” Structures under Shock and Impact V, Witpress, New Forest, UK, 1998.


ALSO AVAILABLE IN:

Electronic Structural Journal