Degradation in Durability of Magnesium Oxychloride-Coated Reinforced Steel Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Degradation in Durability of Magnesium Oxychloride-Coated Reinforced Steel Concrete

Author(s): Wang Penghui, Qiao Hongxia, Feng Qiong, and Cao Hui

Publication: Materials Journal

Volume: 117

Issue: 2

Appears on pages(s): 33-41

Keywords: Clayton-Copula function; corrosion current density; durability degradation; solution immersion acceleration test

DOI: 10.14359/51720298

Date: 3/1/2020

Abstract:
Because of ordinary reinforced concrete’s poor durability in saline soil areas and Qinghai Salt Lake, magnesium oxychloride-coated steel-cement concrete was adopted in this area. The process of the degradation of coated steel bars’ durability was evaluated according to the actual service situation of magnesium-oxychloridecoated reinforced concrete in saline soil areas and Qinghai Salt Lake. The corrosion parameters of coated steel bars in magnesium oxychloride cement concrete were obtained by the accelerated immersion and natural corrosion tests in a drying environment. Using the Copula function as the connection function, the corrosion current density of the coated steel obtained by accelerated tests and natural rust tests was adopted as the degradation factor of the edge distribution function. The results demonstrated that the Clayton-Copula function reflects the actual process of the degradation in durability of coated steel bars well, and the coated steel bars reached a severe state of corrosion at 18,250 days.

Related References:

1. Wang, F., “A Study on Corrosion and Destruction of Concrete under Natural Condition of Caerhan,” 3rd Beijing International Symposium on Cement and Concrete, 1993, pp. 811-815.

2. Wang, F.; Sun, R.; and Qin, X., “The Investigation of Concrete Durability under Natural Condition of Ca Er Han Salt Lake,” Bulletin of the Chinese Ceramic Society, V. 21, No. 4, 2002, pp. 16-22.

3. Yu, H., “Magnesium Oxychloride Cement and Its Application,” China Building Materials Industry Press, Beijing, China, 1993, pp. 180-417.

4. Qiao, H.; Gong, W.; Wang, P.; Chen, G.; and Cheng, Q., “Experimental Study on Steel Reinforcement Protection in Magnesium Oxychloride Cement Concrete under Sulfate Environment,” Journal of Southwest Jiaotong University, V. 52, No. 2, 2017, pp. 247-253.

5. Qiao, H.; Wei, G.; Chen, G.; and Fan, L., “Experimental Study on Corrosion of Steel Bar in Magnesium Cement Concrete Based on Polarization Curves,” Nature and Science, V. 44, No. 1, 2016, pp. 6-10.

6. Qiao, H.; Wei, G.; Sheng, G.; Chen, G.; and Cheng, Q., “Electrochemical Corrosion of Steel Bar in the Magnesium Cement Concrete,” Materials Science and Technology, V. 24, No. 1, 2016, pp. 63-69.

7. Wang, J.; Liu, G.; Xiao, L.; Di, L.; and Hu, M., “Experimental Study on the Anti-Chloride Ion Performance of Concrete in Salt Spray Environment,” Industrial Construction, V. 43, No. 11, 2013, pp. 89-91,125.

8. Peng, J.; Wang, H.; Zhang, J.; Hu, S.; and Liu, Y., “Experimental Study on Chloride Ion Diffusion Coefficient in Concrete and Probabilistic Analysis of Its Influence on Deterioration Performance of RC Structures,” China Journal of Highway and Transport, V. 27, No. 6, 2014, pp. 77-83.

9. Jin, Z.; Sun, W.; Zhang, Y.; and Jiang, J., “Damage of Concrete in Sulfate and Chloride Solution,” Journal of the Chinese Ceramic Society, V. 34, No. 5, 2006, pp. 630-635.

10. Han, J., “Study on the Durability of Partially-Exposed Concrete in Saline Soil Areas of Qinghai Province,” Chang’an University, Xi’an, China, 2012, pp. 30-43.

11. Zhang, Y., “Durability and Service Life Design of RC Members Exposed to Chloride Salt-Frost Damage,” Nanjing University of Aeronautics and Astronautics, Nanjing, China, 2011, pp. 23-37.

12. Zhang, H.; Qi, X.; Zeng, H.; and Deng, C., “Study on Method of Accelerated Corrosion Experiment in Simulated Seawater,” Fushi Kexue Yu Fanghu Jishu, V. 22, No. 3, 2010, pp. 192-196.

13. Yang, C.; Huang, D.; Zhang, Y.; and Wu, J., “Estimation of Shear Strength Parameters of Rock Mass Based on Copula Theory,” Chinese Journal of Rock Mechanics and Engineering, V. 32, No. 12, 2013, pp. 2463-2470.

14. Tang, X.; Li, D.; Zhou, C.; and Phoon, K., “Probabilistic Analysis of Load-Displacement Hyperbolic Curves of Single Pile Using Copula,” Yantu Lixue, V. 33, No. 1, 2012, pp. 171-178.

15. Li, D. Q.; Tang, X. S.; Zhou, C. B.; and Phoon, K.-K., “Uncertainty Analysis of Correlated Non-Normal Geotechnical Parameters Using Gaussian Copula,” Science China Technological Sciences, V. 55, No. 11, 2012, pp. 3081-3089. doi: 10.1007/s11431-012-4937-z

16. Tang, X.-S.; Li, D.-Q.; Rong, G.; Phoon, K.-K.; and Zhou, C.-B., “Impact of Copula Selection on Geotechnical Reliability under Incomplete Probability Information,” Computers and Geotechnics, V. 49, No. 4, 2013, pp. 264-278. doi: 10.1016/j.compgeo.2012.12.002

17. Lei, Z.; Tang, X.; and Li, D., “System Reliability Analysis of Geotechnical Structures Based on the Copula Function,” Yantu Lixue, V. 37, No. 1, 2016, pp. 193-202.

18. Pan, X.; Wang, L.; Xu, Y.; Zhang, L.; Liu, W.; and Wu, R., “A Wind Farm Power Modeling Method Based on Mixed Copula,” Dianli Xitong Zidonghua, V. 38, No. 14, 2014, pp. 17-22.

19. Pan, X.; Liu, Z.; and Liu, W., “Wind Farm Polymerization Influences on Security and Economic Operation in Power System Based on Copula Function,” Journal of Modern Power Systems and Clean Energy, V. 3, No. 3, 2015, pp. 381-392. doi: 10.1007/s40565-015-0147-6

20. Sun, M.; Konstantelos, I.; and Strbac, G., “C-Vine Copula Mixture Model for Clustering of Residential Electrical Load Pattern Data,” IEEE Transactions on Power Systems, V. 32, No. 3, 2017, pp. 2382-2393. doi: 10.1109/TPWRS.2016.2614366

21. Xie, Z. Q.; Ji, T. Y.; Li, M. S.; and Wu, Q. H., “Quasi-Monte Carlo Based Probabilistic Optimal Power Flow Considering the Correlation of Wind Speeds Using Copula Function,” IEEE Transactions on Power Systems, V. 33, No. 2, 2018, pp. 2239-2247. doi: 10.1109/TPWRS.2017.2737580

22. He, Q.; Zhang, H.; and Zheng, M., “Research of the Risk of the Portifolio Cluding Index Future—The Application of Copula Method to the Financial Risk Management,” Application of Statistics and Management, V. 28, No. 1, 2009, pp. 159-166.

23. Ben Saida, A., and Jean-luc, P., “On the Robustness of Portfolio Allocation under Copula Misspecification,” Annals of Operations Research, V. 262, No. 2, 2018, pp. 631-652. doi: 10.1007/s10479-016-2137-0

24. Nguyen, C.; Bhatti, M. I.; and Hayat, A., “Volatility Linkages in the Spot and Futures Market in Australia: A Copula Approach,” Quality & Quantity, V. 48, No. 5, 2014, pp. 2589-2603. doi: 10.1007/s11135-013-9909-2

25. Riccetti, L., “A Copula–GARCH Model for Macro Asset Allocation of a Portfolio with Commodities: An Out-of-Sample Analysis,” Empirical Economics, V. 44, No. 3, 2013, pp. 1315-1366. doi: 10.1007/s00181-012-0577-1

26. Ni, Z.; Liu, H.; Luo, Y.; and Tan, J., “Copulas Application in Precipitation Probability Forecast of Flood Disasters in Guangxi,” Journal of Guangxi Meteorology, V. 35, No. 2, 2014, pp. 32-39.

27. Li, Y.; Gu, W.; Cui, W.; Chang, Z.; and Xu, Y., “Exploration of Copula Function Use in Crop Meteorological Drought Risk Analysis: A Case Study of Winter Wheat in Beijing, China,” Natural Hazards, V. 77, No. 2, 2015, pp. 1289-1303. doi: 10.1007/s11069-015-1649-2

28. Tosunoglu, F., and Can, I., “Application of Copulas for Regional Bivariate Frequency Analysis of Meteorological Droughts in Turkey,” Natural Hazards, V. 82, No. 3, 2016, pp. 1457-1477. doi: 10.1007/s11069-016-2253-9

29. Zuo, D.; Feng, G.; Zhang, Z.; and Hou, W., “Application of Archimedean Copulas to the Analysis of Drought Decadal Variation in China,” Asia-Pacific Journal of Atmospheric Sciences, V. 54, No. 2, 2018, pp. 125-143. doi: 10.1007/s13143-017-0065-9

30. Gang, L., and Shi, Y., “Review of Non-Destructive Methods in Assessment Corrosion in Reinforced Concrete Member,” Fujian Architecture & Construction, V. 9, No. 4, 2002, pp. 55-57.

31. Isgor, O. B., “A Durability Model for Chloride and Carbonation Induced Steel Corrosion in Reinforced Concrete Members,” Carleton University, Ottawa, ON, Canada, 2002, pp. 30-43.

32. Nelsen, R. B., An Introduction to Copulas, second edition, Springer, New York, 2006, 63 pp.

33. Sklar, A., “Functioned repartition a Dimension Etleurs Merges,” Publications de l’Institut de Statistique de l’Universite de Paris, V. 8, No. 5, 1959, pp. 229-231.


ALSO AVAILABLE IN:

Electronic Materials Journal