Self-Consolidating Recycled Concrete: Rheological Behavior Over Time

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self-Consolidating Recycled Concrete: Rheological Behavior Over Time

Author(s): I. González-Taboada, B. González-Fonteboa, F. Martínez-Abella, and S. Seara-Paz

Publication: Materials Journal

Volume: 117

Issue: 1

Appears on pages(s): 3-14

Keywords: recycled coarse aggregate; rheographs; rheology; thixotropy; time-dependent evolution; workability loss

DOI: 10.14359/51720289

Date: 1/1/2020

Abstract:
A rheograph is a plastic viscosity-yield stress diagram that systematically reveals the effects of diverse changes on the rheological behavior of the cement-based suspension. In this work, the time-dependent rheological behavior of self-consolidating recycled concrete (SCRC) and conventional self-consolidating concrete (SCC) was compared and the effect of changes in material quantities was assessed using different rheographs. The developed analysis leads to the conclusion that differences obtained depend on the quantity of water compensated in the mixing protocol to take into account the high absorption of recycled aggregates. This fact determines the region of the curves “rheological variations – effective water to cement ratio” where concretes are designed. The high slope region of these curves will be reached when high percentages of recycled aggregate are used, when SCRC is designed with a low water-cement ratio (w/c), and/or when long-term self-consolidating behavior is measured. In these cases, a different time-dependent rheological behavior is expected from an SCRC than from an SCC; otherwise, the rheological behavior over time of an SCRC will be similar to that of an SCC.

Related References:

1. Damtoft, J. S.; Lukasik, J.; Herfort, D.; Sorrentino, D.; and Gartner, E. M., “Sustainable Development and Climate Change Initiatives,” Cement and Concrete Research, V. 38, No. 2, 2008, pp. 115-127. doi: 10.1016/j.cemconres.2007.09.008

2. Vieira, D. R.; Calmon, J. L.; and Coelho, F. Z., “Life Cycle Assessment (LCA) Applied to the Manufacturing of Common and Ecological Concrete: A Review,” Construction and Building Materials, V. 124, 2016, pp. 656-666. doi: 10.1016/j.conbuildmat.2016.07.125

3. Butler, L.; West, J. S.; and Tighe, S. L., “Effect of Recycled Concrete Coarse Aggregate from Multiple Sources on the Hardened Properties of Concrete with Equivalent Compressive Strength,” Construction and Building Materials, V. 47, 2013, pp. 1292-1301. doi: 10.1016/j.conbuildmat.2013.05.074

4. de Juan, M. S., and Gutiérrez, P. A., “Study on the Influence of Attached Mortar Content on the Properties of Recycled Concrete Aggregate,” Construction and Building Materials, V. 23, No. 2, 2009, pp. 872-877. doi: 10.1016/j.conbuildmat.2008.04.012

5. González-Taboada, I.; González-Fonteboa, B.; Martínez-Abella, F.; and Carro-López, D., “Study of Recycled Concrete Aggregate Quality and Its Relationship with Recycled Concrete Compressive Strength Using Database Analysis,” Materiales de Construcción, V. 66, No. 323, 2016, pp. 89-99.

6. Etxeberria, M.; Marí, A. R.; and Vázquez, E., “Recycled Aggregate Concrete as Structural Material,” Materials and Structures, V. 40, No. 5, 2007, pp. 529-541. doi: 10.1617/s11527-006-9161-5

7. Safiuddin, M.; Alengaram, U. J.; Rahman, M. M.; Salam, M. A.; and Jumaat, M. Z., “Use of Recycled Concrete Aggregate in Concrete: A Review,” Journal of Civil Engineering and Management, V. 19, No. 6, 2013, pp. 796-810. doi: 10.3846/13923730.2013.799093

8. Katz, A., and Kulisch, D., “Performance of Mortars Containing Recycled Fine Aggregate from Construction and Demolition Waste,” Materials and Structures, V. 50, No. 4, 2017, pp. 199-214. doi: 10.1617/s11527-017-1067-x

9. Silva, R. V.; De Brito, J.; and Dhir, R. K., “The Influence of the Use of Recycled Aggregates on the Compressive Strength of Concrete: A Review,” European Journal of Environmental and Civil Engineering, V. 19, No. 7, 2015, pp. 825-849. doi: 10.1080/19648189.2014.974831

10. Seara-Paz, S.; González-Fonteboa, B.; Martínez-Abella, F.; and González-Taboada, I., “Time-Dependent Behaviour of Structural Concrete Made with Recycled Coarse Aggregates. Creep and Shrinkage,” Construction and Building Materials, V. 122, 2016, pp. 95-109. doi: 10.1016/j.conbuildmat.2016.06.050

11. Chakradhara Rao, M.; Bhattacharyya, S. K.; and Barai, S. V., “Influence of Field Recycled Coarse Aggregate on Properties of Concrete,” Materials and Structures, V. 44, No. 1, 2011, pp. 205-220. doi: 10.1617/s11527-010-9620-x

12. Silva, R. V.; De Brito, J.; and Dhir, R. K., “Tensile Strength Behaviour of Recycled Aggregate Concrete,” Construction and Building Materials, V. 83, 2015, pp. 108-118. doi: 10.1016/j.conbuildmat.2015.03.034

13. Ajdukiewicz, A., and Kliszczewicz, A., “Influence of Recycled Aggregates on Mechanical Properties of HS/HPC,” Cement and Concrete Composites, V. 24, No. 2, 2002, pp. 269-279. doi: 10.1016/S0958-9465(01)00012-9

14. Malešev, M.; Radonjanin, V.; and Marinković, S., “Recycled Concrete as Aggregate for Structural Concrete Production,” Sustainability, V. 2, No. 5, 2010, pp. 1204-1225. doi: 10.3390/su2051204

15. Bairagi, N. K.; Ravande, K.; and Pareek, V. K., “Behaviour of Concrete with Different Proportions of Natural and Recycled Aggregates,” Resources, Conservation and Recycling, V. 9, No. 1-2, 1993, pp. 109-126. doi: 10.1016/0921-3449(93)90036-F

16. Padmini, A. K.; Ramamurthy, K.; and Mathews, M. S., “Influence of Parent Concrete on the Properties of Recycled Aggregate Concrete,” Construction and Building Materials, V. 23, No. 2, 2009, pp. 829-836. doi: 10.1016/j.conbuildmat.2008.03.006

17. Xiao, J.; Li, J.; and Zhang, C., “Mechanical Properties of Recycled Aggregate Concrete under Uniaxial Loading,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1187-1194. doi: 10.1016/j.cemconres.2004.09.020

18. Bhikshma, V., and Kishore, R., “Development of Stress-Strain Curves for Recycled Aggregate Concrete,” Asian Journal of Civil Engineering, V. 11, No. 2, 2010, pp. 253-261.

19. Ferreira, L.; De Brito, J.; and Barra, M., “Influence of the Pre-Saturation of Recycled Coarse Concrete Aggregates on Concrete Properties,” Magazine of Concrete Research, V. 63, No. 8, 2011, pp. 617-627. doi: 10.1680/macr.2011.63.8.617

20. González, B.; Martínez, F.; Carro, D.; and Seara, S., “Stress-Strain Relationship in Axial Compression for Concrete Using Recycled Saturated Coarse Aggregate,” Construction and Building Materials, V. 25, No. 5, 2011, pp. 2335-2342. doi: 10.1016/j.conbuildmat.2010.11.031

21. Hwang, S.-D.; Khayat, K. H.; and Bonneau, O., “Performance-Based Specifications of Self-Consolidating Concrete Used in Structural Applications,” ACI Materials Journal, V. 103, No. 2, Mar.-Apr. 2006, pp. 121-129.

22. Wallevik, O. H., and Wallevik, J. E., “Rheology as a Tool in Concrete Science: The Use of Rheographs and Workability Boxes,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1279-1288. doi: 10.1016/j.cemconres.2011.01.009

23. Nunes, S.; Figueiras, H.; Milheiro-Oliveira, P.; Coutinho, J. S.; and Figueiras, J., “A Methodology to Assess Robustness of SCC Mixtures,” Cement and Concrete Research, V. 36, No. 12, 2006, pp. 2115-2122. doi: 10.1016/j.cemconres.2006.10.003

24. Kovler, K., and Roussel, N., “Properties of Fresh and Hardened Concrete,” Cement and Concrete Research, V. 41, No. 7, 2011, pp. 775-792. doi: 10.1016/j.cemconres.2011.03.009

25. Khayat, K. H.; Omran, A.; and Magdi, W. A., “Evaluation of Thixotropy of Self-Consolidating Concrete and Influence on Concrete Performance,” I Simpósio latinoamericano sobre concreto autodensável, Oct. 8-10, 2012, Maceió-Alagoas, Brazil.

26. Roussel, N., “A Thixotropy Model for Fresh Fluid Concretes: Theory, Validation and Applications,” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1797-1806. doi: 10.1016/j.cemconres.2006.05.025

27. González-Taboada, I.; González-Fonteboa, B.; Pérez-Ordóñez, J. L.; and Eiras-López, J., “Prediction of Self-Compacting Recycled Concrete Mechanical Properties Using Vibrated Recycled Concrete Experience,” Construction and Building Materials, V. 131, 2017, pp. 641-654. doi: 10.1016/j.conbuildmat.2016.11.112

28. Grdic, Z. J.; Toplicic-Curcic, G. A.; Despotovic, I. M.; and Ristic, N. S., “Properties of Self-Compacting Concrete Prepared with Coarse Recycled Concrete Aggregate,” Construction and Building Materials, V. 24, No. 7, 2010, pp. 1129-1133. doi: 10.1016/j.conbuildmat.2009.12.029

29. Corinaldesi, V., and Moriconi, G., “The Role of Industrial By-Products in Self-Compacting Concrete,” Construction and Building Materials, V. 25, No. 8, 2011, pp. 3181-3186. doi: 10.1016/j.conbuildmat.2011.03.001

30. Fakitsas, C.; Papakonstantinou, P.; Kiousis, P.; and Savva, A., “Effects of Recycled Concrete Aggregates on the Compressive and Shear Strength of High-Strength Self-Consolidating Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 4, 2012, pp. 356-361. doi: 10.1061/(ASCE)MT.1943-5533.0000397

31. Güneyisi, E.; Gesŏglu, M.; Algin, Z.; and Yazici, H., “Rheological and Fresh Properties of Self-Compacting Concretes Containing Coarse and Fine Recycled Concrete Aggregates,” Construction and Building Materials, V. 113, 2016, pp. 622-630. doi: 10.1016/j.conbuildmat.2016.03.073

32. Señas, L.; Priano, C.; and Marfil, S., “Influence of Recycled Aggregates on Properties of Self-Consolidating Concretes,” Construction and Building Materials, V. 113, 2016, pp. 498-505. doi: 10.1016/j.conbuildmat.2016.03.079

33. Tuyan, M.; Mardani-Aghabaglou, A.; and Ramyar, K., “Freeze-Thaw Resistance, Mechanical and Transport Properties of Self-Consolidating Concrete Incorporating Coarse Recycled Concrete Aggregate,” Materials and Design, V. 53, 2014, pp. 983-991. doi: 10.1016/j.matdes.2013.07.100

34. Safiuddin, M.; Alengaram, U. J.; Salam, M. A.; Jumaat, M. Z.; Jaafar, F. F.; and Saad, H. B., “Properties of High-Workability Concrete with Recycled Concrete Aggregate,” Materials Research, V. 14, No. 2, 2011, pp. 248-255. doi: 10.1590/S1516-14392011005000039

35. Silva, Y. F.; Robayo, R. A.; Mattey, P. E.; and Delvasto, S., “Properties of Self-Compacting Concrete on Fresh and Hardened with Residue of Masonry and Recycled Concrete,” Construction and Building Materials, V. 124, 2016, pp. 639-644. doi: 10.1016/j.conbuildmat.2016.07.057

36. Tang, W., “Fresh Properties of Self-Compacting Concrete with Coarse Recycled Aggregate,” Advanced Materials Research, V. 602-604, 2012, pp. 938-942. doi: 10.4028/www.scientific.net/AMR.602-604.938

37. Kebaïli, O.; Mouret, M.; Arabi, N.; and Cassagnabere, F., “Adverse Effect of the Mass Substitution of Natural Aggregates by Air-Dried Recycled Concrete Aggregates on the Self-Compacting Ability of Concrete: Evidence and Analysis through an Example,” Journal of Cleaner Production, V. 87, 2015, pp. 752-761. doi: 10.1016/j.jclepro.2014.10.077

38. Carro-López, D.; González-Fonteboa, B.; de Brito, J.; Martínez-Abella, F.; González-Taboada, I.; and Silva, P., “Study of the Rheology of Self-Compacting Concrete with Fine Recycled Concrete Aggregates,” Construction and Building Materials, V. 96, 2015, pp. 491-501. doi: 10.1016/j.conbuildmat.2015.08.091

39. Kou, S. C., and Poon, C. S., “Properties of Self-Compacting Concrete Prepared with Coarse and Fine Recycled Concrete Aggregates,” Cement and Concrete Composites, V. 31, No. 9, 2009, pp. 622-627. doi: 10.1016/j.cemconcomp.2009.06.005

40. Faleschini, F.; Jiménez, C.; Barra, M.; Aponte, D.; Vázquez, E.; and Pellegrino, C., “Rheology of Fresh Concretes with Recycled Aggregates,” Construction and Building Materials, V. 73, 2014, pp. 407-416. doi: 10.1016/j.conbuildmat.2014.09.068

41. González-Taboada, I.; González-Fonteboa, B.; Martínez-Abella, F.; and Seara-Paz, S., “Analysis of Rheological Behaviour of Self-Compacting Concrete Made with Recycled Aggregates,” Construction and Building Materials, V. 157, 2017, pp. 18-25. doi: 10.1016/j.conbuildmat.2017.09.076

42. Thrane, L. N.; Pade, C.; Nielsen, C. V.; Jeknavorian, A. A.; Schemmel, J. J.; and Dean, S. W., “Determination of Rheology of Self-Consolidating Concrete Using the 4C-Rheometer and How to Make Use of the Results,” Journal of ASTM International, V. 7, No. 1, 2010, pp. 1-10. doi: 10.1520/JAI102003

43. González-Taboada, I.; González-Fonteboa, B.; Eiras-López, J.; and Rojo-López, G., “Tools for the Study of Self-Compacting Recycled Concrete Fresh Behaviour: Workability and Rheology,” Journal of Cleaner Production, V. 156, 2017, pp. 1-18. doi: 10.1016/j.jclepro.2017.04.045

44. Domone, P. L., “Self-Compacting Concrete: An Analysis of 11 Years of Case Studies,” Cement and Concrete Composites, V. 28, No. 2, 2006, pp. 197-208. doi: 10.1016/j.cemconcomp.2005.10.003

45. Vilanova-Fernández, A., “Influence of the Composition and the Use of Different Types of Cement and Additions in the Properties of Self-Compacting Concrete,” PhD dissertation, Polytechnic University of Madrid, Madrid, Spain, 2009. (in Spanish)

46. Yammine, J.; Chaouche, M.; Guerinet, M.; Moranville, M.; and Roussel, N., “From Ordinary Rhelogy Concrete to Self-Compacting Concrete: A Transition between Frictional and Hydrodynamic Interactions,” Cement and Concrete Research, V. 38, No. 7, 2008, pp. 890-896. doi: 10.1016/j.cemconres.2008.03.011

47. Mahaut, F.; Mokéddem, S.; Chateau, X.; Roussel, N.; and Ovarlez, G., “Effect of Coarse Particle Volume Fraction on the Yield Stress and Thixotropy of Cementitious Materials,” Cement and Concrete Research, V. 38, No. 11, 2008, pp. 1276-1285. doi: 10.1016/j.cemconres.2008.06.001

48. Toutou, Z., and Roussel, N., “Multi Scale Experimental Study of Concrete Rheology: From Water Scale to Gravel Scale,” Materials and Structures, V. 39, No. 2, 2007, pp. 189-199. doi: 10.1617/s11527-005-9047-y

49. Roussel, N.; Stefani, C.; and Leroy, R., “From Mini-Cone Test to Abrams Cone Test: Measurement of Cement-Based Materials Yield Stress Using Slump Tests,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 817-822. doi: 10.1016/j.cemconres.2004.07.032

50. Singh, R. B.; Singh, B.; and Kumar, N., “Thixotropy of Self-Compacting Concrete Containing Recycled Aggregates,” Magazine of Concrete Research, V. 71, No. 1, 2019, pp. 14-25. doi: 10.1680/jmacr.17.00273

51. González-Taboada, I.; González-Fonteboa, B.; Martínez-Abella, F.; and Seara-Paz, S., “Thixotropy and Interlayer Bond Strength of Self-Compacting Recycled Concrete,” Construction and Building Materials, V. 161, 2018, pp. 479-488. doi: 10.1016/j.conbuildmat.2017.11.157

52. Struble, L., and Sun, G. K., “Viscosity of Portland Cement Paste as a Function of Concentration,” Advanced Cement Based Materials, V. 2, No. 2, 1995, pp. 62-69. doi: 10.1016/1065-7355(95)90026-8


ALSO AVAILABLE IN:

Electronic Materials Journal