A Finite Element-Based Methodology for the Thermo-mechanical Analysis of Early Age Behavior in Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Finite Element-Based Methodology for the Thermo-mechanical Analysis of Early Age Behavior in Concrete Structures

Author(s): H. Cifuentes , F. Montero-Chacón, J. Galán, J. Cabezas4 and A. Martínez-De la Concha

Publication: IJCSM

Volume: 13

Issue:

Appears on pages(s):

Keywords: heat of hydration, early age cracking, thermo-mechanical model, fracture mechanics of concrete

DOI: 10.1186/s40069-019-0353-0

Date: 9/30/2019

Abstract:
This paper presents a general procedure based on fracture mechanics models in order to analyze the level of crack-ing and structural safety in reinforced concrete elements at early ages, depending on the stripping time. Our proce-dure involves the development of a thermo-mechanical numerical model based on the finite element method that accounts for the change in the mechanical properties of concrete with time. Moreover, fracture mechanisms are analyzed by means of a material damage model, which is characterized via specific experimental results obtained for standard specimens and notched beams under three-point bending testing. The loading conditions are both thermal and mechanical, and are obtained from the hydration process for a given concrete dosage. The presented methodol-ogy allows for the determination of the optimal stripping time, whereas it helps assessing the analysis of the cracking and the stress states of the elements under consideration. A practical application, namely the analysis of a retaining wall, is used to validate our methodology, showing its suitability in engineering practice.