Title: Utilization of Reclaimed Asphalt Pavement Aggregates in Portland Cement Concrete for Concrete Pavement

Author(s): Anol Mukhopadhyay and Xijun Shi

Publication: Symposium Paper

Volume: 334

Issue:

Appears on pages(s): 13-32

Keywords: reclaimed asphalt pavement, portland cement concrete, microstructure, durability, life cycle assessment

DOI: 10.14359/51720251

Date: 9/30/2019

Abstract:
Potential issues associated with depletion of good aggregate sources and management of excess RAP stockpiles increasingly motivate use of RAP in PCC as a coarse aggregate replacement. Texas has shown great interest in disposing excess RAP stockpiles and a systematic study on using RAP in PCC for Texas pavement applications was conducted by the authors recently. This paper provides a concise summary of the findings from this study. The major conclusions are (1) PCC mixture with dense aggregate gradation can be achieved by adding coarse RAP with adequate intermediate sized particles, which offers better overall performance in terms of workability and mechanical properties, (2) RAP-PCC with coarse RAP replacement up to 40% showed considerable reduction for modulus of rupture. Asphalt cohesive failure (crack passing through the asphalt layer) was found to be the main mechanism responsible for the strength reductions, (3) the addition of allowable amounts of RAP into PCC provides equivalent durability performance relative to plain PCC, and (4) constructing pavements with RAP-PCC yields economic, environmental and social benefits.

Related References:

1. J. Hu, M.S. Siddiqui, P. David Whitney, Two-lift concrete paving–case studies and reviews from sustainability, cost effectiveness and construction perspectives, TRB 93rd Annual Meeting Compendium of Papers, 2014.

2. V. Patankar, R. Williams, Bitumen in dry lean concrete, Highways and Traffic Engineering (1970).

3. S. Kolias, Mechanical properties of cement-treated mixtures of milled bituminous concrete and crushed aggregates, Materials and Structures 29(7) (1996) 411-417.

4. M. Delwar, M. Fahmy, R. Taha, Use of reclaimed asphalt pavement as an aggregate in Portland cement concrete, ACI Materials Journal 94(3) (1997).

5. I. Dumitru, G. Smorchevsky, V. Caprar, Trends in the utilisation of recycled materials and byproducts in the concrete industry in Australia, Proc. of the Concrete Institute of Australia 19th Biennial Conf., Sydney, 1999, pp. 289-301.

6. K. Hassan, J. Brooks, M. Erdman, The use of reclaimed asphalt pavement (RAP) aggregates in concrete, Waste Management Series 1 (2000) 121-128.

7. V. Mathias, T. Sedran, F. de Larrard, Recycling reclaimed asphalt pavement in concrete roads, PRO 40: International RILEM Conference on the Use of Recycled Materials in Buildings and Structures (Volume 1), RILEM Publications, 2004, p. 66.

8. B. Huang, X. Shu, G. Li, Laboratory investigation of portland cement concrete containing recycled asphalt pavements, Cement and Concrete Research 35(10) (2005) 2008-2013.

9. S. Al-Oraimi, H.F. Hassan, A. Hago, Recycling of reclaimed asphalt pavement in portland cement concrete, The Journal of Engineering Research 6(1) (2009) 37-45.

10. F.O. Okafor, Performance of recycled asphalt pavement as coarse aggregate in concrete, Leonardo Electronic Journal of Practices and Technologies 9(17) (2010) 47-58.

11. M. Tia, N. Hossiney, Y.-M. Su, Y. Chen, T.A. Do, Use of reclaimed asphalt pavement in concrete pavement slabs, Report 00088115, U.S Dep. of Transportation, Florida, 2012.

12. A.S. Brand, J.R. Roesler, I.L. Al-Qadi, P. Shangguan, Fractionated reclaimed asphalt pavement (FRAP) as a coarse aggregate replacement in a ternary blended concrete pavement,

Report ICT-12-008, Illinois State Toll Highway Authority, Downers Grove, 2012.

13. M. Berry, J. Stephens, B. Bermel, A. Hagel, D. Schroeder, Feasibility of reclaimed asphalt pavement as aggregate in portland cement concrete pavement, Report FHWA/MT-13-009/8207, U.S. Dep. of Transportation, Montana. 2013.

14. A. Mukhopadhyay, X. Shi, Validation of RAP and/or RAS in hydraulic cement concrete: technical report, Report FHWA/TX-17/0-6855-1, U.S. Dep. of Transportation, Texas, 2017.

15. S. Singh, G. Ransinchung, P. Kumar, Feasibility study of RAP aggregates in cement concrete pavements, Road Materials and Pavement Design (2017) 1-20.

16. S. Singh, G. Ransinchung, P. Kumar, Effect of mineral admixtures on fresh, mechanical and durability properties of RAP inclusive concrete, Construction and Building Materials 156 (2017) 19-27.

17. S. Singh, S. Debbarma, P. Kumar, Utilization of reclaimed asphalt pavement aggregates containing waste from Sugarcane Mill for production of concrete mixes, Journal of Cleaner Production 174 (2017) 42-52.

18. M. Berry, K. Dalton, F. Murray, Feasibility of reclaimed asphalt pavement as aggregate in portland cement concrete pavement phase II: field demonstration, Report FHWA/MT-15-003/8207, U.S. Dep. of Transportation, Montana, 2015.

19. A. Mukhopadhyay, X. Shi, Validation of RAP and/or RAS in hydraulic cement concrete: guidelines and implementation recommendations, Report FHWA/TX-17/0-6855-P1, U.S. Dep. of Transportation, Texas, 2017.

20. K.R. Hansen, A. Copeland, Asphalt pavement industry survey on recycled materials and warm-mix asphalt usage: 2014, Report IS-138, National Asphalt Pavement Association, Lanham, MD. 2015.

21. X. Shi, A. Mukhopadhyay, K.-W. Liu, Mix design formulation and evaluation of portland cement concrete paving mixtures containing reclaimed asphalt pavement, Construction and Building Materials 152 (2017) 756-768.

22. TxDOT, Standard specifications for construction and maintenance of highways, streets, and bridges, Texas Department of Transportation, Austin, Texas, 2014.

23. X. Shi, Evaluation of portland cement concrete containing reclaimed asphalt pavement for pavement applications, PhD dissertation, Texas A&M University, College Station, Texas, 2018.

24. X. Shi, D.G. Zollinger, A. Mukhopadhyay, Punchout study for continuously reinforced concrete pavement containing reclaimed asphalt pavement using pavement ME models, International Journal of Pavement Engineering (2018) 1-14.

25. X. Shi, M. Mirsayar, A.K. Mukhopadhyay, D.G. Zollinger, Characterization of Two-Parameter Fracture Properties of Portland Cement Concrete Containing Reclaimed Asphalt Pavement Aggregates by Semicircular Bending Specimens, Cement Concrete Composites 95 (2019) 56-69.

26. X. Shi, A. Mukhopadhyay, D.G. Zollinger, Sustainability assessment for portland cement concrete pavement containing reclaimed asphalt pavement aggregates, Journal of Cleaner Production 192 (2018) 569-581.