Mechanical Performance of Concrete Incorporating Slender Elements from Recycling GFRP Waste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical Performance of Concrete Incorporating Slender Elements from Recycling GFRP Waste

Author(s): Yuan Tian and Ardavan Yazdanbakhsh

Publication: Symposium Paper

Volume: 334

Issue:

Appears on pages(s): 1-12

Keywords: Concrete, Discrete reinforcement, GFRP waste, Mechanical performance, Recycled composites

DOI: 10.14359/51720250

Date: 9/30/2019

Abstract:
Due to their unique mechanical characteristics, glass fiber reinforced polymer (GFRP) composite materials are difficult to recycle at the end of their service lives. In the present work, a specific approach of recycling GFRP waste for use in concrete is investigated. Scrap from GFRP rebar and waste from a GFRP wind turbine blade shell were processed into slender elements, referred to as “needles,” with a length of 100 mm and used in concrete to replace 5% and 10% of natural coarse aggregate. The results of testing various concrete specimens revealed that the incorporation of needles with longitudinally aligned glass fibers increased the splitting tensile strength of concrete significantly. Both types of recycled needles, regardless of the source of waste and orientation of glass fibers, increased the tensile toughness of concrete significantly. In addition, it was observed that incorporating needles did not reduce concrete’s slump, due to the relatively high specific surface area of the needles. The findings suggest that recycling GFRP waste into needles as concrete reinforcement may be a viable GFRP waste management strategy and deserves further research.

Related References:

1. Yazdanbakhsh, A., Bank, L. C., Chen, C., and Tian, Y., 2017, “FRP-Needles as Discrete Reinforcement in Concrete,” Journal of Materials in Civil Engineering, V. 29, No.10, pp.1-9.

2. Yazdanbakhsh, A., Bank, L. C., Rieder, K. A., Tian, Y., and Chen, C., 2018, “Concrete with discrete slender elements from mechanically recycled wind turbine blades,” Resources,

Conservation and Recycling, V. 128, No. 07, pp. 11-21.

3. Osmani, M., and Pappu, A., 2010, “An assessment of the compressive strength of glass reinforcedplastic waste filled concrete for potential applications in construction,” Concrete

Research Letterts, V.1, No.1, pp. 1-5.

4. Tittarelli, F, and Shah, S.P., 2013, “Effect of low dosages of waste GRP dust on fresh and hardened properties of mortars: Part 1,” Construction and Building Materials, V.47, pp.

1532-1538.

5. Correia, J. R., Almeida, N. M., and Figueira, J. R., 2011, “Recycling of FRP composites: Reusing fine GFRP waste in concrete mixtures,” Journal of Cleaner Production, V. 19,

No.15, pp. 1745-1753.

6. Shahria Alam, M.; Slater, E.; and Muntasir Billah, A. H. M., 2013, “Green Concrete Made with RCA and FRP Scrap Aggregate: Fresh and Hardened Properties,” Journal of Materials in Civil Engineering, V. 25, No.12, pp. 1783-1794.

7. Yazdanbakhsh, A., Bank, L. C., and Chen, C., 2016, “Use of recycled FRP reinforcing bar in concrete as coarse aggregate and its impact on the mechanical properties of concrete,”

Construction and Building Materials, V.121, pp. 278-284.

8. Bank, L. C., Yazdanbakhsh, A., Chen, C., and Tian, Y., 2016, “Reuse of Waste Gfrp Composites As Coarse Aggregates for Concrete.” Proc., 8th International Conference on

Fibre-Reinforced Polymer Composites in Civil Engineering, CICE, Hong Kong, China, pp. 593-598.

9. Bank, L. C., and Yazdanbakhsh, A., 2016, “Concrete containing coarse aggregate recycled from scrap GFRP rebars,” Proc., 6th International Conference on Structural Engineering,

Mechanics and Computation - Insights and Innovations in Structural Engineering, SEMC, Cape Town, South Africa, pp. 1410-1415.

10. ASTM C143/C143M., 2015, Standard Test Method for Slump of Hydraulic-Cement Concrete, West Conshohocken, PA.

11. ASTM C469/C469M., 2014, Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression, West Conshohocken, PA.

12. ASTM C39, 2016, Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens, West Conshohocken, PA.

13. ASTM D2584-94, 2000, Standard Test Method for Ignition Loss of Cured Reinforce Resin, West Conshohocken, PA.