Flexural Strength of Corroded Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Strength of Corroded Reinforced Concrete Beams

Author(s): H. Yalciner, A. Kumbasaroglu, A. K. El-Sayed, A. Pekrioglu Balkıs, E. Dogru, A. I. Turan, A. Karimi, R. Kohistani, M. F. Mermit, and K. Bicer

Publication: Structural Journal

Volume: 117

Issue: 1

Appears on pages(s): 29-41

Keywords: beam; corrosion; flexural strength

DOI: 10.14359/51720195

Date: 1/1/2020

Abstract:
An experimental study was conducted to predict the flexural strength of corroded full-scale reinforced concrete (RC) beams. Two different concrete strength levels at two different steel ratios were tested for different corrosion levels ranging from 0 to 17%. An accelerated corrosion aging method was applied to corrode the reinforcing bars embedded in concrete. The actual corrosion levels were obtained by breaking the concrete and extracting the reinforcing bars. A practical model was developed for the prediction of the flexural strength of corroded RC beams. The developed model predicted the experimentally obtained flexural strength of corroded beams found in the literature well. The results revealed that the structural behavior of corroded RC beams requires consideration of the corrosion levels at both the tensile bars and the stirrups (which are more exposed to corrosion because of their use as outer reinforcing bars) and have significant effects on the flexural strength of corroded RC beams.

Related References:

ACI Committee 318, 2002, “Building Code Requirements for Structural Concrete (ACI 318-02) and Commentary,” American Concrete Institute, Farmington Hills, MI, 445 pp.

Ahmad, S., 2009, “Techniques for Inducing Accelerated Corrosion of Steel in Concrete,” Arabian Journal for Science and Engineering, V. 34, No. 2, pp. 95-104.

Ahmad, S., 2017, “Prediction of Residual Flexural Strength of Corroded Reinforced Concrete Beams,” Anti-Corrosion Methods and Materials, V. 64, No. 1, pp. 69-74. doi: 10.1108/ACMM-11-2015-1599

Amleh, L., and Ghosh, A., 2006, “Modeling the Effect of Corrosion on Bond Strength at the Steel-Concrete Interface with Finite-Element Analysis,” Canadian Journal of Civil Engineering, V. 33, No. 6, pp. 673-682. doi: 10.1139/l06-052

ASTM A370-08a, 2008, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 47 pp.

ASTM G1-03, 2003, “Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 9 pp.

Auyeung, Y.; Balaguru, P.; and Chung, L., 2000, “Bond Behavior of Corroded Reinforcement Bars,” ACI Materials Journal, V. 97, No. 2, Mar.-Apr., pp. 214-220.

Azad, A. K.; Ahmad, S.; and Al-Gohi, B. H. A., 2010, “Flexural Strength of Corroded Reinforced Concrete Beams,” Magazine of Concrete Research, V. 62, No. 6, pp. 405-414. doi: 10.1680/macr.2010.62.6.405

Bažant, Z., 1979, “Physical Model for Steel Corrosion in Concrete Sea Structures—Theory and Application,” Journal of the Structural Division, ASCE, V. 105, No. 6, pp. 1137-1166.

Bicer, K.; Yalciner, H.; Pekrioglu, B. A.; and Kumbasaroglu, A., 2018, “Effect of Corrosion on Flexural Strength of Reinforced Concrete Beams with Polypropylene Fibers,” Construction and Building Materials, V. 185, pp. 574-588. doi: 10.1016/j.conbuildmat.2018.07.021

Cabrera, J. G., 1996, “Deterioration of Concrete Due to Reinforcement Steel Corrosion,” Cement and Concrete Composites, V. 18, No. 1, pp. 47-59. doi: 10.1016/0958-9465(95)00043-7

Campione, G., and Cannella, F., 2018, “Engineering Failure Analysis of Corroded RC Beams in Flexure and Shear,” Engineering Failure Analysis, V. 86, pp. 100-114. doi: 10.1016/j.engfailanal.2017.12.015

Campione, G.; Cannella, F.; and Cavaleri, L., 2017, “Shear and Flexural Strength Prediction of Corroded R. C. Beams,” Construction and Building Materials, V. 149, pp. 395-405. doi: 10.1016/j.conbuildmat.2017.05.125

Chung, L.; Cho, S. H.; Kim, J. H. J.; and Yi, S. T., 2004, “Correction Factor Suggestion for ACI Development Length Provisions Based on Flexural Testing of RC Slabs with Various Levels of Corroded Reinforcing Bars,” Engineering Structures, V. 26, No. 8, pp. 1013-1026. doi: 10.1016/j.engstruct.2004.01.008

Coronelli, D., and Gambarova, P., 2004, “Structural Assessment of Corroded Reinforced Concrete Beams: Modeling Guidelines,” Journal of Structural Engineering, ASCE, V. 130, No. 8, pp. 1214-1224. doi: 10.1061/(ASCE)0733-9445(2004)130:8(1214)

El Maaddawy, T.; Chahrour, A.; and Soudki, K., 2006, “Effect of Fiber-Reinforced Polymer Wraps on Corrosion Activity and Concrete Cracking in Chloride-Contaminated Concrete Cylinders,” Journal of Composites for Construction, ASCE, V. 10, No. 2, pp. 139-147. doi: 10.1061/(ASCE)1090-0268(2006)10:2(139)

El Maaddawy, T.; Soudki, K.; and Topper, T., 2005, “Long-Term Performance of Corrosion-Damaged Reinforced Concrete Beams,” ACI Structural Journal, V. 102, No. 5, Sept.-Oct., pp. 649-656.

El-Sayed, A. K.; Hussain, R. R.; and Shuraim, A. B., 2016, “Influence of Stirrup Corrosion on Shear Strength of Reinforced Concrete Slender Beams,” ACI Structural Journal, V. 113, No. 6, Nov.-Dec., pp. 1223-1232. doi: 10.14359/51689147

Eligehausen, R.; Ozbolt, J.; and Mayer, U., 1998, “Contribution of Concrete Between Cracks at Inelastic Steel Strains and Conclusions for the Optimization of Bond,” SP-180, Bond and Development Length of Reinforcement, A Tribute to Dr. Peter Gergely, R. Leon, ed., American Concrete Institute, Farmington Hills, MI, pp. 45-80.

Hanjari, K. Z.; Kettil, P.; and Lundgren, K., 2011, “Analysis of Mechanical Behavior of Corroded Reinforced Concrete Structures,” ACI Structural Journal, V. 108, No. 5, Sept.-Oct., pp. 532-541.

Jnaid, F., and Aboutaha, R. S., 2016, “Residual Flexural Strength of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 119, pp. 198-216. doi: 10.1016/j.engstruct.2016.04.018

Khan, I.; Francois, R.; and Castel, A., 2014, “Prediction of Reinforcement Corrosion Using Corrosion Induced Cracks Width in Corroded Reinforced Concrete Beams,” Cement and Concrete Research, V. 56, pp. 84-96. doi: 10.1016/j.cemconres.2013.11.006

Lee, H. S.; Kage, T.; Noguchi, T.; and Tomosawa, F., 1999, “The Evaluation of Flexural Strength of RC Beams Damaged by Rebar Corrosion,” Proceedings of the 8th International Conference, Durability of Building Materials and Components, Ottawa, ON, Canada, pp. 321-330.

Liu, Y., and Weyers, R. E., 1998, “Modeling the Time-to-Corrosion Cracking in Chloride Contaminated Reinforced Concrete Structures,” ACI Materials Journal, V. 95, No. 6, Nov.-Dec., pp. 675-680.

Ma, Y.; Che, Y.; and Gong, J., 2012, “Behavior of Corrosion Damaged Circular Reinforced Concrete Columns under Cyclic Loading,” Construction and Building Materials, V. 29, pp. 548-556. doi: 10.1016/j.conbuildmat.2011.11.002

Mousa, M. I., 2016, “Effect of Bond Loss of Tension Reinforcement on the Flexural Behaviour of Reinforced Concrete Beams,” HBRC Journal, V. 12, No. 3, pp. 235-241. doi: 10.1016/j.hbrcj.2015.01.003

O’Flaherty, F. J.; Mangart, P. S.; Lambert, P.; and Browne, E. H., 2008, “Effect of Under-Reinforcement on the Flexural Strength of Corroded Beams,” Materials and Structures, V. 41, No. 2, pp. 311-321. doi: 10.1617/s11527-007-9241-1

Paul, S. C.; Babafemi, A. J.; Conradie, K.; and van Zijl, G. P. A. G., 2016, “Applied Voltage on Corrosion Mass Loss and Cracking Behavior of Steel-Reinforced SHCC and Mortar Specimens,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 5, pp. 1-9.

Rodriguez, J.; Ortega, L. M.; and Casal, J., 1997, “Load-Carrying Capacity of Concrete Structures with Corroded Reinforcement,” Construction and Building Materials, V. 11, No. 4, pp. 239-248. doi: 10.1016/S0950-0618(97)00043-3

Suffern, C.; El-Sayed, A. K.; and Soudki, K., 2010, “Shear Strength of Disturbed Regions with Corroded Stirrups in Reinforced Concrete Beams,” Canadian Journal of Civil Engineering, V. 37, No. 8, pp. 1045-1056. doi: 10.1139/L10-031

Torres-Acosta, A. A.; Navarro-Gutierreza, S.; and Terán-Guillén, J., 2007, “Residual Flexure Capacity of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 29, No. 6, pp. 1145-1152. doi: 10.1016/j.engstruct.2006.07.018

Vecchio, F. J., and Collins, M. P., 1986, “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr., pp. 219-231.

Vidal, T.; Castel, A.; and François, R., 2004, “Analyzing Crack Width to Predict Corrosion in Reinforced Concrete,” Cement and Concrete Research, V. 34, No. 1, pp. 165-174. doi: 10.1016/S0008-8846(03)00246-1

Yalciner, H.; Eren, O.; and Sensoy, S., 2012, “An Experimental Study on the Bond Strength between Reinforcement Bars and Concrete as a Function of Concrete Cover, Strength and Corrosion Level,” Cement and Concrete Research, V. 42, No. 5, pp. 643-655. doi: 10.1016/j.cemconres.2012.01.003

Yalciner, H.; Kumbasaroglu, A.; Ertuc, İ.; and Turan, A. İ., 2018, “Confinement Effect of Geo-Grid and Conventional Shear Reinforcement Bars Subjected to Corrosion,” Structures, V. 13, pp. 139-152. doi: 10.1016/j.istruc.2017.12.004

Yalciner, H.; Sensoy, S.; and Eren, O., 2015, “Seismic Performance Assessment of a Corroded 50-Year-Old Reinforced Concrete Building,” Journal of Structural Engineering, ASCE, V. 141, No. 12, pp. 1-11. doi: 10.1061/(ASCE)ST.1943-541X.0001263

Yang, S. Y.; Song, X. B.; Jia, H. X.; Chen, X.; and Liu, X. L., 2016, “Experimental Research on Hysteretic Behaviors of Corroded Reinforced Concrete Columns with Different Maximum Amounts of Corrosion of Rebar,” Construction and Building Materials, V. 121, pp. 319-327. doi: 10.1016/j.conbuildmat.2016.06.002

Zhang, R.; Castel, A.; and Francois, R., 2010, “Concrete Cover Cracking with Reinforcement Corrosion of RC Beam During Chloride-Induced Corrosion Process,” Cement and Concrete Research, V. 40, No. 3, pp. 415-425. doi: 10.1016/j.cemconres.2009.09.026