A Seawall Constructed with GFRP Bars as Structural Reinforcing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Seawall Constructed with GFRP Bars as Structural Reinforcing

Author(s): Christian C. Steputat, Steven Nolan, Lowry Denty, Paul A. Kaminski, and Antonio Nanni

Publication: Concrete International

Volume: 41

Issue: 9

Appears on pages(s): 26-30

Keywords: pile, cage, cap, installation

DOI: 10.14359/51720157

Date: 9/1/2019

Abstract:
In 2016, the seaside community of Flagler Beach, FL, was severely impacted by Hurricane Matthew. To help mitigate the effects of future storms, a concrete secant-pile seawall is being constructed east of State Road A1A. The seawall comprises glass-fiber-reinforced polymer (GFRP) reinforcing bars in its 1847 secant piles and continuous cap. The noncorrosive GFRP bars are expected to provide minimal maintenance and repair costs over the life cycle of the seawall

Related References:

1. FDOT Structures Manual, Florida Department of Transportation, Tallahassee, FL, Jan. 2018.

2. 2018 FDOT Design Manual, Florida Department of Transportation, Tallahassee, FL, Jan. 2018, www.fdot.gov/roadway/fdm/2018fdm.shtm.

3. AASHTO LRFD Bridge Design Specification, 8th Edition, American Association of State Highway and Transportation Officials, Washington, DC, 2017, 438 pp.

4. FDOT Standard Specifications for Road and Bridge Construction, Florida Department of Transportation, Tallahassee, FL, July 2018, 1213 pp.

5. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 83 pp.

6. ISO/IEC 17025:2017, “General Requirements for the Competence of Testing and Calibration Laboratories,” International Organization for Standardization (ISO), Geneva, Switzerland, 2017, 30 pp.

7. ASTM E2160-04(2018), “Standard Test Method for Heat of Reaction of Thermally Reactive Materials by Differential Scanning Calorimetry,” ASTM International, West Conshohocken, PA, 2004 (Reapproved 2018), 5 pp.

8. ASTM D3418-15, “Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

9. ASTM D2584-18, “Standard Test Method for Ignition Loss of Cured Reinforced Resins,” ASTM International, West Conshohocken, PA, 2018, 3 pp.

10. ASTM D570-98(2018), “Standard Test Method for Water Absorption of Plastics,” ASTM International, West Conshohocken, PA, 1998 (Reapproved 2018), 4 pp.

11. ASTM D792-13, “Standard Test Methods for Density and Specific Gravity (Relative Density) of Plastics by Displacement,” ASTM International, West Conshohocken, PA, 2013, 6 pp.

12. ASTM D7205/D7205M-06(2016), “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 2006 (Reapproved 2016), 13 pp.