Prediction of Self-Healing Potential of Cementitious Materials Incorporating Crystalline Admixture by Isothermal Calorimetry

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prediction of Self-Healing Potential of Cementitious Materials Incorporating Crystalline Admixture by Isothermal Calorimetry

Author(s): Byoungsun Park and Young Cheol Choi

Publication: IJCSM

Volume: 13

Issue:

Appears on pages(s):

Keywords: self-healing potential, isothermal calorimetry, further hydration, water flow test, cementitious materials

DOI: 10.1186/s40069-019-0349-9

Date: 7/31/2019

Abstract:
Crack formation is an inherent property of concrete structures; however, these materials also have the ability to heal cracks autogenously. External water penetrates the inside of concrete through the cracks, and unreacted cement particles present on the crack surface are rehydrated. Cracks are healed by hydration products owing to further hydra-tion. Ground-granulated blast-furnace slag (GGBFS) and fly ash (FA) have slower reactions with water than cement. Because of this late reactivity, there is a high possibility of being present in an unreacted state inside the matrix. This study investigated the self-healing potential of supplementary cementitious materials (SCMs) such as GGBFS, FA, and calcium sulfur aluminate (CSA) expansion agents. For this purpose, isothermal calorimetry and water flow tests were performed. Experimental results showed that the self-healing potential of GGBFS and CSA expansion agent was higher than that of OPC and FA is decreased.