Impact of Materials, Proportioning, and Curing on Ultra- High-Performance Concrete Properties

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Impact of Materials, Proportioning, and Curing on Ultra- High-Performance Concrete Properties

Author(s): A. S. Carey, I. L. Howard, D. A. Scott, R. D. Moser, J. Shannon, and A. Knizley

Publication: Materials Journal

Volume: 117

Issue: 1

Appears on pages(s): 213-222

Keywords: compressive strength; optimization; ultra-high-performance concrete; varying proportions

DOI: 10.14359/51719076

Date: 1/1/2020

Abstract:
This paper evaluated constituent proportions on mechanical and thermal properties of ultra-high-performance concrete. This paper assessed how fine aggregates and fibers at varying proportions enhance cement paste and can improve its mechanical properties to a desired compressive strength, elastic modulus, or tensile strength. Approximately 400 specimens were tested for mechanical properties within four curing regimes and 22 different mixtures. These experiments aimed to add to the body of knowledge found during literature review. Past efforts found in literature have drawn conclusions by varying one ingredient at a time, whereas the current effort systematically varied multiple ingredients. Results showed compressive strength to be due to synergistic relationships between cement paste, fine aggregates, and steel fibers where absence of any ingredient reduced strength. Tensile strength and elastic modulus were dominated by a single ingredient.

Related References:

1. ACI Committee 239, “Ultra-High Performance Concrete: An Emerging Technology Report (ACI 239R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 22 pp.

2. Roth, M. J., “Flexural and Tensile Properties of Thin, Very High-Strength, Fiber-Reinforced Concrete Panels,” (ERDC/GSL TR-08-24), U.S. Army Engineer Research and Development Center, Geotechnical and Structures Laboratory, Vicksburg, MS, 2008.

3. Pyo, S.; Kim, H. Y.; and Lee, B. Y., “Effects of Coarser Fine Aggregate on Tensile Properties of Ultra-High Performance Concrete,” Cement and Concrete Composites, V. 84, 2017, pp. 28-35. doi: 10.1016/j.cemconcomp.2017.08.014

4. Yoo, D. Y.; Banthia, N.; and Yoon, Y. S., “Predicting the Flexural Behavior of Ultra-High Performance Fiber-Reinforced Concrete,” Cement and Concrete Composites, V. 74, 2016, pp. 71-87. doi: 10.1016/j.cemconcomp.2016.09.005

5. Yoo, D. Y.; Banthia, N.; Lee, J. Y.; and Yoon, Y. S., “Effect of Fiber Geometric Property on Rate Dependent Flexural Behavior of Ultra-High-­Performance Cementitious Composite,” Cement and Concrete Composites, V. 86, 2018, pp. 57-71. doi: 10.1016/j.cemconcomp.2017.11.002

6. Scott, D.; Long, W.; Moser, R.; Green, B.; O’Daniel, J.; and Williams, B., “Impact of Steel Fiber Size and Shape on the Mechanical Properties of Ultra-High Performance Concrete,” (ERDC/GSL TR-15-22), U.S. Army Engineer Research and Development Center, Geotechnical and Structures Laboratory, Vicksburg, MS, 2015.

7. Feng, J.; Sun, W. W.; Wang, X. M.; and Shi, X. Y., “Mechanical Analyses of Hooked Fiber Pullout Performance in Ultra-High-­Performance Concrete,” Construction and Building Materials, V. 69, 2014, pp. 403-410. doi: 10.1016/j.conbuildmat.2014.07.049

8. Wille, K., and Naaman, A. E., “Pullout Behavior of High-Strength Steel Fibers Embedded in Ultra-High-Performance Concrete,” ACI Materials Journal, V. 109, No. 4, July-Aug. 2012, pp. 479-488.

9. Chandler, M. Q.; Peters, J. F.; and Pelessone, D., “Modeling Nanomechanical Behavior of Calcium-Silicate-Hydrate,” (ERDC/GSL TR-12-30), U.S. Army Engineer Research and Development Center, Geotechnical and Structures Laboratory, Vicksburg, MS, 2012.

10. Ghafari, E.; Costa, H.; and Júlio, E., “Statistical Mixture Design Approach to Eco-Efficient UHPC,” Cement and Concrete Composites, V. 55, 2015, pp. 17-25. doi: 10.1016/j.cemconcomp.2014.07.016

11. Tayeh, B. A.; Abu Bakar, B. H.; Megat Johari, M. A.; and Voo, Y. L., “Mechanical and Permeability Properties of the Interface between Normal Concrete Substrate and Ultra High Performance Fiber Concrete Overlay,” Construction and Building Materials, V. 36, 2012, pp. 538-548. doi: 10.1016/j.conbuildmat.2012.06.013

12. Alkaysi, M.; El-Tawil, S.; Liu, Z.; and Hansen, W., “Effects of Silica Powder and Cement Type on Durability of Ultra-High-Performance Concrete (UHPC),” Cement and Concrete Composites, V. 66, 2016, pp. 47-56. doi: 10.1016/j.cemconcomp.2015.11.005

13. Berry, M.; Snidarich, R.; and Wood, C., “Development of Non-­Proprietary Ultra-High-Performance Concrete,” Report FHWA/MT-17-010/8237-001, Montana Department of Transportation, Helena, MT, 2017.

14. Liu, Z.; Chen, W.; Wenhua, Z.; Yunsheng, Z.; and Lv, H., “Complete Stress-Strain Behavior of Ecological Ultra-High Performance Cementitious Composite under Uniaxial Compression,” ACI Materials Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 783-794. doi: 10.14359/51689899

15. Wipf, T.; Sritharan, S.; Abu-Hawash, A.; Phares, B.; and Bierwagen, D., “Iowa’s Ultra-High Performance Concrete Implementation,” Iowa Department of Transportation, Ames, IA, Apr. 2011.

16. Weldon, B. D.; Jáuregui, D. V.; Newtson, C. M.; Taylor, C. W.; Montoya, K. F.; Allena, S.; Muro, J.; Talahat, M.; Lyell, E.; and Visage, E. T., “Feasibility Analysis of Ultra High Performance Concrete for Prestressed Bridge Applications—Phase I and II,” Report NM09MSC-01, New Mexico Department of Transportation, Santa Fe, NM, 2012.

17. Graybeal, B. A., “Material Property Characterization of Ultra-High Performance Concrete,” Report FHWA-HRT-06-103, Federal Highway Administration, Washington, DC, 2006.

18. Ahlborn, T. M.; Peuse, E. J.; and Misson, D. L., “Ultra-High-Performance-Concrete for Michigan Bridges Material Performance—Phase I,” Research Report RC-1525, Michigan Department of Transportation, Lansing, MI, 2008.

19. Tia, M.; Ferraro, C.; Lawrence, A.; Smith, S.; and Ochiai, E., “Development of Design Parameters for Mass Concrete Using Finite Element Analysis,” Report 000548 63, Florida Department of Transportation, Tallahassee, FL, 2010.

20. Meddah, M. S.; Zitouni, S.; and Belâabes, S., “Effect of Content and Particle Size Distribution of Course Aggregate on the Compressive Strength of Concrete,” Construction and Building Materials, V. 24, No. 4, 2010, pp. 505-512. doi: 10.1016/j.conbuildmat.2009.10.009

21. Oner, A., and Akyuz, S., “An Experimental Study on Optimum Usage of GGBS for the Compressive Strength of Concrete,” Cement and Concrete Composites, V. 29, No. 6, 2007, pp. 505-514. doi: 10.1016/j.cemconcomp.2007.01.001

22. Tikalsky, P. J.; Carrasquillo, P. M.; and Carrasquillo, R. L., “Strength and Durability Considerations Affecting Mix Proportioning of Concrete Containing Fly Ash,” ACI Materials Journal, V. 85, No. 6, Nov.-Dec. 1987, pp. 505-511.

23. Richard, P., and Cheyrezy, M., “Composition of Reactive Powder Concretes,” Cement and Concrete Research, V. 25, No. 7, 1995, pp. 1501-1511. doi: 10.1016/0008-8846(95)00144-2

24. Juenger, M. C. G., and Siddique, R., “Recent Advances in Understanding the Role of Supplementary Cementitious Materials in Concrete,” Cement and Concrete Research, V. 78, 2015, pp. 71-80. doi: 10.1016/j.cemconres.2015.03.018

25. Williams, E. M.; Graham, S. S.; Reed, P. A.; and Rushing, T. S., “Laboratory Characterization of Cor-Tuf Concrete With and Without Steel Fibers (ERDC/GSL TR-09-22),” U.S. Army Engineer Research and Development Center, Geotechnical and Structures Laboratory, Vicksburg, MS, 2009.

26. Talebinejad, I.; Bassam, S. A.; Iranmanesh, A.; and Shekarchizadeh, M., “Optimizing Mix Proportions of Normal Weight Reactive Powder Concrete with Strengths of 200-350 MPa,” Proceedings of the International Symposium on Ultra High Performance Concrete, Kassel, Germany, 2004, pp. 133-141.

27. Park, J. J.; Kang, S. T.; Koh, K. T.; and Kim, S. W., “Influence of the Ingredients on the Compressive Strength of UHPC as a Fundamental Study on Optimize the Mixing Proportion,” Proceedings of the International Symposium on Ultra High Performance Concrete, Kassel, Germany, 2004, pp. 105-112.

28. Ibrahim, M. A.; Farhat, M.; Issa, M. A.; and Hasse, J. A., “Effect of Material Constituents on Mechanical and Fracture Mechanics Properties of Ultra-High-Performance Concrete,” ACI Materials Journal, V. 114, No. 3, May-June 2016, pp. 453-465.

29. Alsalman, A.; Dang, C. N.; and M. Hale, W. M., “Development of Ultra-High Performance Concrete with Locally Available Materials,” Construction and Building Materials, V. 133, 2017, pp. 135-145. doi: 10.1016/j.conbuildmat.2016.12.040

30. Yazıcı, H., “The Effect of Curing Conditions on Compressive Strength of Ultra-High Strength Concrete with High Volume Mineral Admixtures,” Building and Environment, V. 42, No. 5, 2007, pp. 2083-2089. doi: 10.1016/j.buildenv.2006.03.013

31. Ma, J.; Orgass, M.; Dehn, F.; Schmidt, D.; and Tue, N. V., “Comparative Investigations on Ultra-High Performance Concrete with and without Coarse Aggregates,” Proceedings of the International Symposium on Ultra High Performance Concrete, Kassel, Germany, 2004, pp. 205-212.

32. Li, P. P.; Yu, Q. L.; and Brouwers, H. J. H., “Effect of Coarse Basalt Aggregates on the Properties of Ultra-High Performance Concrete (UHPC),” Construction and Building Materials, V. 170, 2018, pp. 649-659. doi: 10.1016/j.conbuildmat.2018.03.109

33. Yoo, D. Y.; Lee, J. H.; and Yoon, Y. S., “Effect of Fiber Content on Mechanical and Fracture Properties of Ultra-High Performance Fiber Reinforced Cementitious Composites,” Composite Structures, V. 106, 2013, pp. 742-753. doi: 10.1016/j.compstruct.2013.07.033

34. Howard, I. L.; Carey, A.; Burcham, M.; Scott, D. A.; Shannon, J. D.; Moser, R. D.; and Horstemeyer, M. F., “Constituent Properties of Cor-Tuf Ultra-High Performance Concrete Considering Aggregate and Paste Effects.” (ERDC/GSL TR-18-31), U.S. Army Corps of Engineers Engineer Research and Development Center, Vicksburg, MS, 2018.

35. Green, B. H.; Moser, R. D.; Scott, D. A.; and Long, W. R., “Ultra-High Performance Concrete History and Usage by the Corps of Engineers,” Advances in Civil Engineering Materials, V. 4, No. 2, 2015, pp. 132-143.

36. Grabowski, E., and Gillott, J. E., “Effect of Replacement of Silica Flour with Silica Fume on Engineering Properties of Oilwell Cements at Normal and Elevated Temperatures and Pressures,” Cement and Concrete Research, V. 19, No. 3, 1989, pp. 333-344. doi: 10.1016/0008-8846(89)90023-9

37. Ranade, R.; Li, V. C.; Stults, M. D.; Heard, W. F.; and Rushing, T. S., “Composite Properties of High-Strength, High-Ductility Concrete,” ACI Materials Journal, V. 110, No. 4, July-Aug. 2015, pp. 413-422.

38. Cost, V. T.; Howard, I. L.; and Shannon, J., “Improving Concrete Sustainability and Performance with Use of Portland-Limestone Cement Synergies,” Transportation Research Record: Journal of the Transportation Research Board, V. 2342, No. 1, 2013, pp. 26-34. doi: 10.3141/2342-04

39. Shannon, J.; Howard, I. L.; and Tim Cost, V., “Potential of Portland-Limestone Cement to Improve Performance of Concrete Made With High Slag Cement and Fly Ash Replacement Rates,” Journal of Testing and Evaluation, V. 45, No. 3, 2017, pp. 872-889. doi: 10.1520/JTE20150306

40. Hansen, B. S.; Shannon, J.; and Howard, I. L., “Improved Understanding of Concrete Compressive Strength Utilizing Cement Paste Testing,” Advances in Civil Engineering Materials, V. 8, No. 1, 2019, pp. 267-284. doi: 10.1520/ACEM20180134

41. ACI Committee 363, “Report on High Strength Concrete: (ACI 363R-10),” American Concrete Institute, Farmington Hills, MI, 2013, 65 pp.

42. Graybeal, B., and Davis, M., “Cylinder or Cube: Strength Testing of 80 to 200 MPa (11.6 to 29 ksi) Ultra-High-Performance Fiber-Reinforced Concrete,” ACI Materials Journal, V. 105, No. 6, Nov.-Dec. 2008, pp. 603-609.

43. ASTM C192/C192M-16, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2016, 8 pp.

44. Sullivan, W. G.; Howard, I. L.; Cost, T.; and Shannon, J., “Early Age Thermal Measurements of Soil-Cement Mixtures for Quality Control during Paving,” Journal of Testing and Evaluation, V. 46, No. 5, 2018, pp. 1957-1971. doi: 10.1520/JTE20170104

45. ASTM C39/C39M-03, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2003, 15 pp.

46. ASTM C469/C469M-14, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014, 5 pp.

47. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary (ACI 318R-11),” American Concrete Institute, Farmington Hills, MI, 503 pp.

48. ASTM C496/C496M-11, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2011, 5 pp.

49. Allard, T. E.; Priddy, M. W.; Howard, I. L.; and Shannon, J., “Isothermal Strength Development Models of Ultra-High Performance Concrete,” ACI Materials Journal, V. 117, No. 1, Jan. 2020, pp. 175-186. doi: 10.14359/51719075


ALSO AVAILABLE IN:

Electronic Materials Journal