Shear Strength of Dry and Epoxy Joints for Ultra-High-Performance Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Dry and Epoxy Joints for Ultra-High-Performance Fiber-Reinforced Concrete

Author(s): Balamurugan A. Gopal, Farzad Hejazi, Milad Hafezolghorani, and Yen Lei Voo

Publication: Structural Journal

Volume: 117

Issue: 1

Appears on pages(s): 279-288

Keywords: bridges; dry; epoxy; joint; precast; shear keys; shear strength; ultra-high-performance fiber-reinforced concrete (UHPFRC)

DOI: 10.14359/51718078

Date: 1/1/2020

Abstract:
Joints between precast segmental bridge girders (PSBGs) represent the locations of discontinuity through which compression and shear forces are transmitted. Therefore, knowledge of the joint behavior to accurately predict the response of PSBGs is essential. The aim of this research is to investigate the shear behavior, shear capacity, and shear-transfer mechanisms of the ultra-high-performance fiber-reinforced concrete (UHPFRC) keyed dry and epoxy joints. For this purpose, a series of full-scale UHPFRC keyed joint specimens were manufactured and tested with three variable parameters—namely, number of shear keys, confining stress, and the type of joint (dry or epoxy). The observations from experimental tests showed that the capacity of the UHPFRC keyed joints increased with increasing confining pressure applied across the joint, number of shear keys, and the epoxy layers applied on joints. Furthermore, a new design shear model for UHPFRC precast segmental bridges was developed and validated with experimental data.

Related References:

1. Buyukozturk, O.; Bakhoum, M. M.; and Beattie, S. M., “Shear Behavior of Joints in Precast Concrete Segmental Bridges,” Journal of Structural Engineering, ASCE, V. 116, No. 12, 1990, pp. 3380-3401.

2. Zhou, X.; Mickleborough, N.; and Li, Z., “Shear Strength of Joints in Precast Concrete Segmental Bridges,” ACI Structural Journal, V. 102, No. 1, Jan.-Feb. 2005, p. 3.

3. Rombach, G. A., and Specker, A., “Segmentbrücken,” Beton-Kalender, Teil 1, Verlag Ernst und Sohn, Berlin, Germany, 2004, pp. 177-211.

4. Voo, Y. L.; Foster, S. J.; and Voo, C. C., “Ultrahigh-Performance Concrete Segmental Bridge Technology: Toward Sustainable Bridge Construction,” Journal of Bridge Engineering, V. 20, No. 8, 2014, p. B5014001.

5. Bu, Z. Y., and Wu, W. Y., “Inter Shear Transfer of Unbonded Prestressing Precast Segmental Bridge Column Dry Joints,” Engineering Structures, V. 154, June 2018, pp. 52-65.

6. Issa, M. A., and Abdalla, H. A., “Structural Behavior of Single Key Joints in Precast Concrete Segmental Bridges,” Journal of Bridge Engineering, V. 12, No. 3, 2007, pp. 315-324.

7. Rombach, G., “Dry Joint Behavior of Hollow Box Girder Segmental Bridges,” FIP Symposium, Segmental Construction in Concrete, New Delhi, India, 2004.

8. Turmo, J.; Ramos, G.; and Aparicio, A. C., “Shear Strength of Dry Joints of Concrete Panels with and Without Steel Fibers: Application to Precast Segmental Bridges,” Engineering Structures, V. 28, No. 1, 2006, pp. 23-33.

9. Alcalde, M.; Cifuentes, H.; and Medina, F., “Influence of the Number of Keys on the Shear Strength of Post-Tensioned Dry Joints,” Materiales de Construcción, V. 63, No. 310, 2013, pp. 297-307.

10. Hu, Z. N., and Xie, Y. L., “Mechanical and Failure Characteristics of Shear Keys on Immersed Tunnel Segment Joints under Differential Settlements,” Procedia Engineering, V. 166, 2016, pp. 373-378.

11. Shamass, R.; Zhou, X.; and Wu, Z., “Numerical Analysis of Shear-Off Failure of Keyed Epoxied Joints in Precast Concrete Segmental Bridges,” Journal of Bridge Engineering, V. 22, No. 1, 2016, p. 4016108.

12. Han, Q.; Zhou, Y.; and Ou, Y., “Seismic Behavior of Reinforced Concrete Sacrificial Exterior Shear Keys of Highway Bridges,” Engineering Structures, V. 139, 2017, pp. 59-70.

13. Tawadrous, R., and Morcous, G., “Interface Shear Resistance of Clustered Shear Connectors for Precast Concrete Bridge Deck Systems,” Engineering Structures, V. 160, No. 1, 2018, pp. 195-211.

14. Jang, H. O.; Lee, H. S.; and Cho, K., “Experimental Study on Shear Performance of Plain Construction Joints Integrated with Ultra-High Performance Concrete (UHPC),” Construction and Building Materials, V. 152, 2017, pp. 16-23.

15. Voo, Y. L.; Foster, S. J.; and Gilbert, R. I., “Shear Strength of Fiber Reinforced Reactive Powder Concrete Prestressed Girders without Stirrups,” Journal of Advanced Concrete Technology, V. 4, No. 1, 2006, pp. 123-132.

16. Voo, Y. L., and Foster, S. J., “Characteristics of Ultra-High Performance ‘Ductile’ Concrete and Its Impact on Sustainable Construction,” IES Journal Part A: Civil and Structural Engineering, V. 3, No. 3, 2010, pp. 168-187.

17. Buttignol, T. E. T.; Sousa, J. L. A. O.; and Bittencourt, T. N., “Ultra High-Performance Fiber-Reinforced Concrete (UHPFRC): A Review of Material Properties and Design Procedures,” Revista IBRACON de Estruturas e Materiais, V. 10, No. 4, 2017, pp. 957-971.

18. El-Tawil, S.; Tai, Y.; and Belcher, J. A., “Field Application of Nonproprietary Ultra-High-Performance Concrete,” Concrete International, V. 40, No. 1, Jan. 2018, pp. 36-42.

19. AASHTO, “Guide Specifications for the Design and Construction of Segmental Concrete Bridges,” second edition, Washington, DC, 1999, pp. 3-118.

20. NF P 18-470, “Concrete-Ultra-High Performance Fiber-Reinforced Concrete-Specifications, Performance, Production and Conformity,” 2016.

21. ASTM C882/C882M-05, “Bond Strength of Epoxy-Resin Systems Used With Concrete By Slant Shear,” ASTM International, West Conshohocken, PA, 2005.


ALSO AVAILABLE IN:

Electronic Structural Journal