Title: Design Approach for Compressive Arch Action in Reinforced Concrete Beams

Author(s): Shao-Bo Kang and Shan Wang

Publication: Structural Journal

Volume: 117

Issue: 1

Appears on pages(s): 197-206

Keywords: axial stiffness; compressive arch action; design approach; reinforced concrete beams; rotational stiffness

DOI: 10.14359/51718071

Date: 1/1/2020

Abstract:
This paper addresses a direct design approach for compressive arch action in reinforced concrete beams. Equilibrium and compatibility of the beam are established on a plastic hinge mechanism. The effects of axial and rotational stiffnesses are considered explicitly in the approach by correlating the strains of compressive reinforcement and the bending moments with the axial compressive strain of beams. The expression for the axial compressive strain is obtained by solving a quadratic equation and used to calculate the neutral axis depths at the beam ends. Vertical load and the associated axial compression force can be quantified from flexural theory. The calculated load capacity and the peak axial compression force are in reasonably good agreement with test data. The effects of axial and rotational stiffnesses on compressive arch action are investigated through the design approach.

Related References:

1. Park, R., and Gamble, W. L., Reinforced Concrete Slabs, John Wiley & Sons, Inc., New York, NY, 2000.

2. Lew, H. S.; Bao, Y.; Pujol, S.; and Sozen, M. A., “Experimental Study of Reinforced Concrete Assemblies under Column Removal Scenarios,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 881-892. doi: 10.14359/51686739

3. Yi, W. J.; He, Q. F.; Xiao, Y.; and Kunnath, S. K., “Experimental Study on Progressive Collapse-Resistant Behavior of Reinforced Concrete Frame Structures,” ACI Structural Journal, V. 105, No. 4, July-Aug. 2008, pp. 433-439.

4. Su, Y.; Tian, Y.; and Song, X., “Progressive Collapse Resistance of Axially-Restrained Frame Beams,” ACI Structural Journal, V. 106, No. 5, Sept.-Oct. 2009, pp. 600-607.

5. Guice, L. K., and Rhomberg, E. J., “Membrane Action in Partially Restrained Slabs,” ACI Structural Journal, V. 85, No. 4, July-Aug. 1988, pp. 365-373.

6. Park, R., “The Ultimate Strength and Long-Term Behaviour of Uniformly Loaded, Two-Way Concrete Slabs with Partial Lateral Restraint at All Edges,” Magazine of Concrete Research, V. 16, No. 48, 1964, pp. 139-152. doi: 10.1680/macr.1964.16.48.139

7. Yu, J., and Tan, K. H., “Analytical Model for the Capacity of Compressive Arch Action of Reinforced Concrete Subassemblages,” Magazine of Concrete Research, V. 66, No. 3, 2014, pp. 109-126. doi: 10.1680/macr.13.00217

8. Park, R., “The Lateral Stiffness and Strength Required to Ensure Membrane Action at the Ultimate Load of a Reinforced Concrete Slab and Beam Floor,” Magazine of Concrete Research, V. 16, No. 40, 1965, pp. 139-152.

9. Lu, X.; Lin, K.; Li, C.; and Li, Y., “New Analytical Calculation Models for Compressive Arch Action in Reinforced Concrete Structures,” Engineering Structures, V. 168, 2018, pp. 721-735. doi: 10.1016/j.engstruct.2018.04.097

10. Kang, S.-B., and Tan, K. H., “Analytical Model for Compressive Arch Action in Horizontally-Restrained Beam-Column Subassemblages,” ACI Structural Journal, V. 113, No. 4, July-Aug. 2016, pp. 813-826. doi: 10.14359/51688629

11. Kang, S.-B., and Tan, K. H., “Analytical Study on Reinforced Concrete Frames Subject to Compressive Arch Action,” Engineering Structures, V. 141, 2017, pp. 373-385. doi: 10.1016/j.engstruct.2017.03.039

12. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington, MI, 2011, 473 pp.

13. Yu, J., and Tan, K. H., “Experimental and Numerical Investigation on Progressive Collapse Resistance of Reinforced Concrete Beam-Column Subassemblages,” Engineering Structures, V. 55, 2013, pp. 90-106. doi: 10.1016/j.engstruct.2011.08.040

14. Kang, S.-B.; Tan, K. H.; and Yang, E.-H., “Progressive Collapse Resistance of Precast Beam-Column Subassemblages with Engineered Cementitious Composites,” Engineering Structures, V. 98, 2015, pp. 186-200. doi: 10.1016/j.engstruct.2015.04.034

15. FarhangVesali, N.; Valipour, H.; Samali, B.; and Foster, S., “Development of Arching Action in Longitudinally-Restrained Reinforced Concrete Beams,” Construction and Building Materials, V. 47, 2013, pp. 7-19. doi: 10.1016/j.conbuildmat.2013.04.050

16. Yu, J., and Tan, K. H., “Structural Behavior of Reinforced Concrete Frames Subjected to Progressive Collapse,” ACI Structural Journal, V. 114, No. 1, Jan. 2017, pp. 63-74. doi: 10.14359/51689424

17. Yu, J., and Tan, K. H., “Structural Behavior of RC Beam-Column Subassemblages under a Middle Column Removal Scenario,” Journal of Structural Engineering, ASCE, V. 139, No. 2, 2013, pp. 233-250. doi: 10.1061/(ASCE)ST.1943-541X.0000658

18. Kang, S.-B., and Tan, K. H., “Progressive Collapse Resistance of Precast Concrete Frames with Discontinuous Reinforcement in the Joint,” Journal of Structural Engineering, ASCE, V. 143, No. 9, 2017, p. 04017090 doi: 10.1061/(ASCE)ST.1943-541X.0001828

19. Kang, S.-B., and Tan, K. H., “Robustness Assessment of Exterior Precast Concrete Frames under Column Removal Scenarios,” Journal of Structural Engineering, ASCE, V. 142, No. 12, 2016, p. 04016131 doi: 10.1061/(ASCE)ST.1943-541X.0001616


ALSO AVAILABLE IN:

Electronic Structural Journal