Discussion on Problem of Standard Deviation of Concrete Strength

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Discussion on Problem of Standard Deviation of Concrete Strength

Author(s): Dai Zhenchao

Publication: Materials Journal

Volume: 117

Issue: 1

Appears on pages(s): 25-35

Keywords: empirical equation of concrete strength; error transmission; linear relationship; normal distribution; χ2 distribution

DOI: 10.14359/51718053

Date: 1/1/2020

Abstract:
This paper discusses the characteristics of the standard deviation of concrete specimen strength and the relationship between the standard deviation of concrete strength and the average value of strength. It is revealed that strength standard deviation of a small number of specimens is highly uncertain and can neither represent nor be used to predict the actual strength standard deviation of concrete. The results of theoretical calculation and practical measurement show that the standard deviation of strength increases with the increase of the average strength, which is close to linear relationship, but when the strength equals zero, the standard deviation of strength still exists.

Related References:

1. ACI Committee 214, “Guide to Evaluation of Strength Test Results of Concrete (ACI 214R-11),” American Concrete Institute, Farmington Hills, MI, 2011, 16 pp.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

3. Li, T., Mathematical Processing of Experiments, Science Press, China, 1980, pp. 86-90.

4. Zheng, S.; Wu, L.; Tao, Z.; and Wang, J., Probability Theory and Mathematical Statistics, Shanghai Science and Technology Press, China, 1961, 88 pp.

5. Philleo, R. E., “Increasing the Usefulness of ACI 214: Use of Standard Deviation and a Technique for Small Sample,” Concrete International, V. 4, No. 9, Sept. 1981, pp. 71-74.

6. Wang, S., Concrete Quality Control Translation Collection, China Industry Press, China, 1965, 126 pp.

7. ACI Committee 214, “Methods for Assessing the Results of Concrete Compression Tests on Site,” American Concrete Institute, Farmington Hills, MI, 1965.

8. ACI Committee 214, “Recommended Practice for Evaluation of Strength Test Results of Concrete (ACI 214-77),” American Concrete Institute, Farmington Hills, MI, 1977, 14 pp.

9. Shiyan, F., Error Theory and Experimental Data Processing, Science Press, China, 1964, 49 pp.

10. Xu, H., “Strength Analysis and Guaranteed Strength Design of Dam Concrete in China,” Special Research Report on Dam Concrete Construction Quality Control (No. 9), Danjiangkou Engineering Bureau, China, 1962.

11. Danjiangkou Engineering Bureau, “Statistical Report on Quality Index of Concrete Construction Material for Danjiangkou Project in Hanjiang,” China, 1970.

12. Gao, J., “Statistical Analysis of Concrete Testing and Production Quality,” Exchange of Construction Technology Experience of the Eighth Engineering Bureau of the Ministry of Water Resources and Electric Power, China, 1984, pp. 38-51.

13. The 8th Engineering Bureau of the Ministry of Water Resources and Electric Power, Wujiangdu Construction Technology, Water Resources and Electric Power Press, China, 1987, 221 pp.

14. Chenghua, D., “Relationship between Deviation and Mean Value of Sleeper Concrete Compressive Strength,” Journal of Concrete and Reinforced Concrete, V. 4, 1983, pp. 27-29.

15. Ruesch, H., “Quality Control of Concrete,” Materialprufing, V. 6, No. 11, Nov. 1964, pp. 387-394.


ALSO AVAILABLE IN:

Electronic Materials Journal