Experimental Study on Damaged Prestressed Concrete Beams Using External Post-Tensioned Tendons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Damaged Prestressed Concrete Beams Using External Post-Tensioned Tendons

Author(s): Weichen Xue, Yuan Tan, and Fei Peng

Publication: Structural Journal

Volume: 117

Issue: 1

Appears on pages(s): 159-168

Keywords: carbon fiber-reinforced polymer (CFRP); external post-tensioning; initial damage; prestressed concrete beams; steel strands; strengthening

DOI: 10.14359/51718019

Date: 1/1/2020

Abstract:
This paper focused on flexural behavior of damaged partially prestressed concrete beams strengthened with external post-tensioned tendons. A total of six strengthened beams and two unstrengthened beams, serving as control specimens, were tested to failure. The test parameters were prestressing tendon types (steel and carbon fiber-reinforced polymer [CFRP]) and initial damage levels (undamaged, in-service damage, and over-loaded damage). The test results revealed that strengthening the beams with external tendons could successfully improve serviceability and ultimate flexural capacity with good deformability. Additionally, the initial damage had slight effect on ultimate capacity and ductility, but it did affect the cracking and deflection behavior. The ductility of the strengthened beams using external CFRP tendons was comparable to those using steel strands. Finally, the experimental results were compared to theoretical predictions obtained from several design approaches, indicating that the flexural capacity of the strengthened beams with initial damage can be analyzed in the same way as those without initial damage, whereas the effect of initial damage should be considered in calculating the deflection of the beams with overloaded initial damage.

Related References:

AASHTO, 2017, “LRFD Bridge Design Specifications,” eighth edition, American Association of State Highway and Transportation Officials, Washington, DC, 1781 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2004, “Prestressing Concrete Structures with FRP Tendons (ACI 440.4R-04),” American Concrete Institute, Farmington Hills, MI, 35 pp.

ACI Committee 440, 2012, “Guide Test Methods for Fiber-Reinforced Polymers (FRPs) for Reinforcing or Strengthening Concrete Structures (ACI 440.3R-12),” American Concrete Institute, Farmington Hills, MI, 23 pp.

ASCE, 2017, “2017 Report Card for America’s Infrastructure,” American Society of Civil Engineers, www.infrastructurereportcard.org.

Au, F. T. K., and Du, J. S., 2008, “Deformability of Concrete Beams with Unbonded FRP Tendons,” Engineering Structures, V. 30, No. 12, pp. 3764-3770. doi: 10.1016/j.engstruct.2008.07.003

Bennitz, A.; Schmidt, J. W.; Nilimaa, J.; Taljsten, B.; Goltermann, P.; and Ravn, D. L., 2012, “Reinforced Concrete T-beams Externally Prestressed with Unbonded Carbon Fiber-Reinforced Polymer Tendons,” ACI Structural Journal, V. 109, No. 4, July-Aug., pp. 521-530. doi: 10.14359/51683871

Burningham, C. A.; Pantelides, C. P.; and Reaveley, L. D., 2014, “Repair of Prestressed Concrete Beams with Damaged Steel Tendons Using Post-Tensioned Carbon Fiber-Reinforced Polymer Rods,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr., pp. 387-396. doi: 10.14359/51686529

Burningham, C. A.; Pantelides, C. P.; and Reaveley, L. D., 2015, “Repair of Reinforced Concrete Deep Beams Using Post-Tensioned CFRP Rods,” Composite Structures, V. 125, July, pp. 256-265. doi: 10.1016/j.compstruct.2015.01.054

CAN/CSA S6-14, 2014, “Canadian Highway Bridge Design Code (CHBDC),” Canadian Standards Association, Rexdale, ON, Canada, 894 pp.

Elrefai, A.; West, J. S.; and Soudki, K. A., 2008, “Effect of Over-Loading on Fatigue Performance of Reinforced Concrete Beams Strengthened with Externally Post-tensioned Carbon-Fibre-Reinforced Polymer Tendons,” Canadian Journal of Civil Engineering, V. 35, No. 11, Nov., pp. 1294-1307. doi: 10.1139/L08-070

GB 50010, 2010, “Code for Design of Concrete Structures (GB 50010-2010),” China Architecture & Building Press, Beijing, China, 425 pp.

Ghallab, A., and Beeby, A. W., 2002, “Ultimate Strength of Externally Strengthened Prestressed Beams,” Proceedings of the Institution of Civil Engineers, Structures and Buildings, V. 152, No. 4, Nov., pp. 395-406. doi: 10.1680/stbu.2002.152.4.395

Ghallab, A., and Beeby, A. W., 2005, “Factors Affecting the External Prestressing Stress in Externally Strengthened Prestressed Concrete Beams,” Cement and Concrete Composites, V. 27, No. 9-10, Oct.-Nov., pp. 945-957. doi: 10.1016/j.cemconcomp.2005.05.003

Grace, N.; Bebawy, M.; and Kasabasic, M., 2015, “Evaluation and Analysis of Decked Bulb T Beam Bridge,” Report No. RC-1620, Lawrence Technological University, Southfield, MI, 217 pp.

Grace, N. F., and Abdel-Sayed, G., 1998, “Behavior of Externally Draped CFRP Tendons in Prestressed Concrete Bridges,” PCI Journal, V. 43, No. 5, Sept.-Oct., pp. 88-101. doi: 10.15554/pcij.09011998.88.101

Harajli, M. H., 1993, “Strengthening of Concrete Beams by External Prestressing,” PCI Journal, V. 38, No. 6, pp. 76-88. doi: 10.15554/pcij.11011993.76.88

Jaeger, L.; Mufti, A.; and Tadros, G., 1997, “The Concept of the Overall Performance Factor in Rectangular-Section Reinforced Concrete Beams,” Proceedings of the 3rd International Symposium on Non-Metallic (FRP) Reinforcement for Concrete Structures, Japan Concrete Institute, Tokyo, Japan, pp. 551-558.

JTG D62, 2004, “Code for Design of Highway Reinforced Concrete and Prestressed Concrete Bridges and Culverts (JTG D62-2004),” China Communication Press, Beijing, China, 231 pp.

Karbhari, V. M., 1998, “Use of Composite Materials in Civil Infrastructure in Japan,” International Technology Research Institute, Word Technology Division, Baltimore, MD.

Kwon, S. J.; Yang, K. H.; and Mun, J. H., 2018, “Flexural Tests on Externally Post-tensioned Lightweight Concrete Beams,” Engineering Structures, V. 164, June, pp. 128-140. doi: 10.1016/j.engstruct.2018.02.064

MacGregor, R. J. G., 1989, “Strength and Ductility of Externally Post-Tensioned Segmental Box Girders,” PhD dissertation, University of Texas at Austin, Austin, TX, 368 pp.

Naaman, A. E., and Alkhairi, F. M., 1991, “Stress at Ultimate in Unbonded Post-Tensioning Tendons: Part 2—Proposed Methodology,” ACI Structural Journal, V. 88, No. 6, Nov.-Dec., pp. 683-692. doi: 10.14359/1288

Naaman, A. E.; Burns, N. H.; French, C.; Gamble, W. L.; and Mattock, A. H., 2002, “Stresses in Unbonded Prestressing Tendons at Ultimate: Recommendation,” ACI Structural Journal, V. 99, No. 4, July-Aug., pp. 518-529. doi: 10.14359/12121

NACE International, 2012, “Corrosion Costs and Preventive Strategies in the United States,” Publication No. FHWA-RD-01-156, National Association for Corrosion Engineers, Houston, TX, http://www.nace.org.

Peng, F., and Xue, W., 2018, “Analytical Approach for Flexural Capacity of FRP Prestressed Concrete T-beams with Non-Prestressed Steel Bars,” Journal of Composites for Construction, ASCE, V. 22, No. 6, Nov.-Dec., p. 04018063 doi: 10.1061/(ASCE)CC.1943-5614.0000903

Peng, F.; Xue, W.; and Tan, Y., 2018, “Design Approach for Flexural Capacity of Prestressed Concrete Beams with External Tendons,” Journal of Structural Engineering, ASCE, V. 144, No. 12, p. 04018215 doi: 10.1061/(ASCE)ST.1943-541X.0002208

Rabbat, B., and Sowlat, K., 1987, “Testing of Segmental Concrete Girders with External Tendons,” PCI Journal, V. 32, No. 2, pp. 86-107. doi: 10.15554/pcij.03011987.86.107

Tan, K. H., and Ng, C. K., 1997, “Effects of Deviators and Tendon Configuration on Behavior of Externally Prestressed Beams,” ACI Structural Journal, V. 94, No. 1, Jan.-Feb., pp. 13-22.

Wang, X.; Shi, J.; Wu, G.; Yang, L.; and Wu, Z., 2015, “Effectiveness of Basalt FRP Tendons for Strengthening of RC Beams through the External Prestressing Technique,” Engineering Structures, V. 101, Oct., pp. 34-44. doi: 10.1016/j.engstruct.2015.06.052


ALSO AVAILABLE IN:

Electronic Structural Journal