Thermomechanical-Coupled Distress for Reinforced Concrete Beams Strengthened with Carbon Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thermomechanical-Coupled Distress for Reinforced Concrete Beams Strengthened with Carbon Fiber-Reinforced Polymer

Author(s): Yail J. Kim and Ibrahim Bumadian

Publication: Structural Journal

Volume: 117

Issue: 4

Appears on pages(s): 49-59

Keywords: carbon fiber-reinforced polymer (CFRP); degradation; performance; retrofit; strengthening; thermomechanical

DOI: 10.14359/51718016

Date: 7/1/2020

Abstract:
This paper presents detrimental synergies resulting from mechanical distress coupled with elevated temperatures on the behavior of reinforced concrete beams strengthened with carbon fiber-reinforced polymer (CFRP) sheets. Thermal loadings ranging from 20 to 170°C (68 to 338°F) are associated with various mechanical loading configurations for 18 beams—monotonic, incremental cyclic, and anomalous cyclic. Of interest are the flexural responses, failure modes, and energy development of the strengthened beams subjected to the coupled loadings. The capacity of the beams decreases with an increase in temperature, whereas their individual performance is controlled by the mechanical loading schemes. A threshold temperature is noticed, which classifies the response domains of the cyclically loaded beams. The implications of the monotonic and cyclic loadings become similar above the threshold temperature due to the deteriorated CFRP-concrete interface. The failure modes of the beams are dominated by the thermal loading, rather than the mechanical loadings. Regarding the energy development of the test beams, the influence of the incremental cyclic loading is pronounced relative to its anomalous counterpart. The degree of energy dissipation tends to stabilize as long as the anomalous excitation does not exceed the magnitude of the sinusoidal cyclic loading. To characterize the performance of the strengthened beams under the thermomechanical-coupled loadings, an analytical approach is proposed.

Related References:

1. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 2017, 112 pp.

2. Hu, W., Polymer Physics: A Molecular Approach, Springer, New York, NY, 2013.

3. Kodur, V. K. R., and Yu, B., “Rational Approach for Evaluating Fire Resistance of FRP-Strengthened Concrete Beams,” Journal of Composites for Construction, ASCE, V. 20, No. 6, 2016, p. 04016041 doi: 10.1061/(ASCE)CC.1943-5614.0000697

4. Foster, S. K., and Bisby, L. A., “Fire Survivability of Externally Bonded FRP Strengthening Systems,” Journal of Composites for Construction, ASCE, V. 12, No. 5, 2008, pp. 553-561. doi: 10.1061/(ASCE)1090-0268(2008)12:5(553)

5. Leone, M.; Matthys, S.; and Aiello, M. A., “Effect of Elevated Service Temperature on Bond Between FRP EBR Systems and Concrete,” Composites. Part B, Engineering, V. 40, No. 1, 2009, pp. 85-93. doi: 10.1016/j.compositesb.2008.06.004

6. Hashemi, S., and Al-Mahaidi, R., “Flexural Performance of CFRP Textile-Retrofitted RC Beams Using Cement-Based Adhesives at High Temperature,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 791-797. doi: 10.1016/j.conbuildmat.2011.09.015

7. Miyano, Y.; McMurray, M. K.; Enyama, J.; and Nakada, M.,“Loading Rate and Temperature Dependence on Flexural Fatigue Behavior of a Satin Woven CFRP Laminate,” Journal of Composite Materials, V. 28, No. 13, 1994, pp. 1250-1260. doi: 10.1177/002199839402801305

8. Coronado, P.; Arguelles, A.; Vina, J.; Mollon, V.; and Vina, I., “Influence of Temperature on a Carbon-Fibre Epoxy Composite Subjected to Static and Fatigue Loading Under Mode-I Delamination,” International Journal of Solids and Structures, V. 49, No. 21, 2012, pp. 2934-2940. doi: 10.1016/j.ijsolstr.2012.05.018

9. Montesano, J.; Selezneva, M.; Fawaz, Z.; Poon, C.; and Behdinan, K., “Elevated Temperature Off-Axis Fatigue Behavior of an Eight-Harness Satin Woven Carbon-Fiber/Bismaleimide Laminate,” Composites. Part A, Applied Science and Manufacturing, V. 43, No. 9, 2012, pp. 1454-1466. doi: 10.1016/j.compositesa.2012.04.016

10. March, M. L., and Stringer, S. J., “Performance-Based Seismic Bridge Design (NCHRP Synthesis 440),” Transportation Research Board, Washington, DC, 2013,126 pp.

11. Williams, B. K., “Fire Performance of FRP-Strengthened Reinforced Concrete Flexural Members,” PhD thesis, Queen’s University, Kingston, ON, Canada, 2004, 389 pp.

12. ASTM C39/C39M-16a, “Standard Practice for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2016, 7 pp.

13. Li, H.; Jacob, K. J.; and Wong, C. P., “An Improvement of Thermal Conductivity of Underfill Materials for Flip-Chip Packages,” IEEE Transactions on Advanced Packaging, V. 26, No. 1, 2003, pp. 25-32. doi: 10.1109/TADVP.2003.811546

14. Park, S.-J., and Jin, F.-L., “Thermal Stabilities and Dynamic Mechanical Properties of Sulfone-Containing Epoxy Resin Cured with Anhydride,” Polymer Degradation & Stability, V. 86, No. 3, 2004, pp. 515-520. doi: 10.1016/j.polymdegradstab.2004.06.003

15. FEMA 461, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” Federal Emergency Management Agency, Washington, DC, 2007.

16. Sabelli, R.; Mahin, S.; and Chang, C., “Seismic Demands on Steel Braced Frame Buildings with Buckling Restrained Braces,” Engineering Structures, V. 25, No. 5, 2003, pp. 655-666. doi: 10.1016/S0141-0296(02)00175-X

17. Brachmann, I.; Browning, J.; and Matamoros, A., “Drift-Dependent Confinement Requirements for Reinforced Concrete Columns Under Cyclic Loading,” ACI Structural Journal, V. 101, No. 5, Sept.-Oct. 2004, pp. 669-677.

18. Akay, M., “Aspects of Dynamic Mechanical Analysis in Polymeric Composites,” Composites Science and Technology, V. 47, No. 4, 1993, pp. 419-423. doi: 10.1016/0266-3538(93)90010-E

19. ASCE 41-17, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2017.

20. Neville, A. M., Properties of Concrete, fourth edition, Pearson, Essex, UK, 1995.


ALSO AVAILABLE IN:

Electronic Structural Journal