Title: In-Drum Measurement Systems

Author(s): Denis Beaupré

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2019

Abstract:
This presentation reviews the current capabilities of automated measurement systems for ready mix concrete trucks. It discusses methods of slump evaluation in addition to a wide array of other parameters such as drum speed, detection of mixing end, water addition, temperature, volume, slump flow, German DIN flow and rheological properties. It also presents a discussion on the synergy of such expanded system when used in conjunction with global positioning system and wireless transmission to central database.